Dissolution of ilmenite by roasting with LPG-pyrolysed products and subsequent leaching
Source abstract
Abstract
Illmenite has been leached with 6 g eq dm −3 hydrochloric and/or sulphuric acid after being roasted at (700 ± 15)°C; with LPG flow rate of 230 cm 3 min −1 for 75 min at a partial size of 63-125 μm. The maximum weight percentages of metals dissolved from the roasted mass are ∼85% titanium and 82.1% iron with 6 g eq dm −3 hydrochloric acid, whereas it is 52.3% titanium and 60.8% iron with 6 g eq dm −3 sulphuric acid system. The optimum leaching with hydrochloric acid solution requires a higher acid concentration than 6 g eq dm −3 , 110°C temperature, solid to liquid phase ratio (S/L) of 0.02 kg dm −3 and a pulp agitation speed of 350 rpm for 5 h. Identical concentration of sulphuric acid always gives poorer dissolution. Comparison of the X-ray powder diffraction patterns (XRD) of ilmenite and the roasted mass suggests certain chemical/physical changes occurring during treatment
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal Extraction and Bioleaching · Iron and Steelmaking Processes · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.