Transport properties of amorphous CuO-Bi 2 O 3 semiconducting pellets

W. J. Gawande, S. V. Pakade, S. P. Yawale, D. K. Burghate, S. G. Motke

Open full text

Abstract

The results of measurement of dc-electrical conductivity and activation energy have been reported for four different composition of CuO-Bi 2 O 3 glass powder pellets pressed at 50°C in the temperature range of 300 - 493 K. A plot of - log a versus 1/T shows two different regions of conduction suggesting two types of conduction mechanisms switching from one type to another occurring at knee temperature. The dc-conductivity increases with increase in temperature of the sample and also with increase of mol% of CuO. Activation energy calculated for both regions (LTR and HTR) is below 1 eV, thus the electrical conduction is electronic. Activation energy decreases with increase of mol% of CuO. Non-adiabatic hopping conduction was observed in the sample. A plot of dielectric constant versus log of frequency shows zig-zag nature. Dielectric constant decreases with increase in mol% of CuO.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electrical and Thermal Properties of Materials · Transition Metal Oxide Nanomaterials · Glass properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.