Acid functionalization of carbon nanofibers
Source abstract
Abstract
We have studied the effects of temperature (70–100°C), process duration (1–4 h), and the ratio of the acid mixture (concentrated HNO 3 and H 2 SO 4 in the volume ratio 1: 3) volume to carbon nanofiber weight (70: 1 to 133: 1 ml/g) on the yield of functionalization products and their dispersibility in water. The results indicate that, with increasing temperature and process duration, the yield of functionalization products decreases, and their concentration (“solubility”) in the aqueous dispersion increases: from 1.2–1.3 to 11.0 mg/ml when the yield decreases from 71–89 to 30%. We present the first measurements of the gas volume evolved during functionalization and show that it increases with increasing temperature and process duration, reaching 500–600 ml/g carbon under the most severe conditions. The major component of the reaction gases is CO 2 (over 50 vol %).
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Carbon Nanotubes in Composites · Graphene research and applications · Nanopore and Nanochannel Transport Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Klein, K.L., Melechko, A.V., McKnight, T.E., et al., Surface Characterization and Functionalization of Carbon Nanofibers, J. Appl. Phys., 2008, vol. 103, paper 061301.10.1063/1.2840049 ↗
2. Liu, J., Rinzler, A.G., Dai, H., et al., Fullerene Pipes, Science, 1998, vol. 280, pp. 1253–1256.10.1126/science.280.5367.1253 ↗
3. Chen, J., Hamon, M.A., Hu, H., et al., Solution Properties of Single-Walled Carbon Nanotubes, Science, 1998, vol. 282, pp. 95–98.10.1126/science.282.5386.95 ↗
4. Lee, G.-W., Kim, J., Yoon, J., et al., Structural Characterization of Carboxylated Multi-Walled Carbon Nanotubes, Thin Solid Films, 2008, vol. 516, pp. 5781–5784.10.1016/j.tsf.2007.10.071 ↗
5. Nguyen Tran Hung, Anoshkin, I.V., Dement’ev, A.P., et al., Functionalization and Solubilization of Thin Multiwalled Carbon Nanotubes, Neorg. Mater., 2008, vol. 44, no. 3, pp. 270–274 [Inorg. Mater. (Engl. Transl.), vol. 44, no. 3, pp. 219–223].
6. Nguyen Tran Hung, Anoshkin, I.V., Dement’ev, A.P., et al., Functionalization and Solubilization of Carbon Nanofibers, Usp. Khim. Khim. Tekhnol., 2007, vol. 21, no. 8, pp. 82–86.
7. Park, K.C., Hayashi, T., Tomiyasu, H., et al., Progressive and Invasive Functionalization of Carbon Nanotube Sidewalls by Diluted Nitric Acid under Supercritical Conditions, J. Mater. Chem., 2005, vol. 15, pp. 407–411.10.1039/b411221k ↗
8. Yu, H., Jin, Y., Peng, F., et al., Kinetically Controlled Side-Wall Functionalization of Carbon Nanotubes by Nitric Acid Oxidation, J. Phys. Chem. C., 2008, vol. 112, pp. 6758–6763.10.1021/jp711975a ↗
9. Wang, Y., Iqbal, Z., and Mitra, S., Rapidly Functionalized, Water-Dispersed Carbon Nanotubes at High Concentration, J. Am. Chem. Soc., 2006, vol. 128, pp. 95–99.10.1021/ja053003q ↗
10. Kuznetsova, A., Popova, I., Yates, J.T., et al., Oxygen-Containing Functional Groups on Single-Wall Carbon Nanotubes: NEXAFS and Vibrational Spectroscopic Studies, J. Am. Chem. Soc., 2001, vol. 123, pp. 10699–10704.10.1021/ja011021b ↗
11. Rakov, E.G., Blinov, S.N., Ivanov, I.G., et al., A Continuous Process for Carbon Nanofiber Fabrication, Zh. Prikl. Khim. (S.-Peterburg), 2004, vol. 77, no. 2, pp. 193–196.
12. Salzmann, C.G., Llewellyn, S.A., Tobias, G., et al., The Role of Carboxylated Carbonaceous Fragments in the Functionalization and Spectroscopy of Single-Walled Carbon-Nanotube Material, Adv. Mater., 2007, vol. 19, pp. 883–887.10.1002/adma.200601310 ↗
13. Marshall, M.W., Popa-Nita, S., and Shapter, J.G., Measurement of Functionalised Carbon Nanotube Carboxylic Acid Groups Using a Simple Chemical Process, Carbon, 2006, vol. 44, pp. 1137–1141.10.1016/j.carbon.2005.11.010 ↗
14. Rosca, I.D., Watari, F., Uo, M., and Akasaka, T., Oxidation of Multiwalled Carbon Nanotubes by Nitric Acid, Carbon, 2005, vol. 43, pp. 3124–3131.10.1016/j.carbon.2005.06.019 ↗