Preparation of boron microcrystals via high-pressure, high-temperature pyrolysis of decaborane, B10H14
Source abstract
Abstract
Crystalline boron has been prepared via high-pressure, high-temperature pyrolysis of decaborane, B10H14. We obtained α-tetragonal boron crystals at a pressure of 8–9 GPa and temperatures in the range 1100–1600°C and β-rhombohedral boron intergrowths at 3 GPa and 1200°C.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Boron and Carbon Nanomaterials Research · High-pressure geophysics and materials · Boron Compounds in Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (13)
Show source-provided references
1. Nakamura, K., Preparation and Properties of Amorphous Boron Films Deposited by Pyrolysis of Decaborane in the Molecular Flow Region, J. Electrochem. Soc., 1984, vol. 131, no. 11, pp. 2691–2697.10.1149/1.2115385 ↗
2. Kamimura, K., Nagaoka, T., Shinomiya, T., et al., Preparation and Properties of Boron Thin Films, Thin Solid Films, 1999, vols. 343–344, pp. 342–344.10.1016/S0040-6090(98)01676-9 ↗
3. Kamimura, K., Yoshimura, T., Nagaoka, T., et al., Preparation and Thermoelectric Property of Boron Thin Film, J. Solid State Chem., 2000, vol. 154, no. 1, pp. 153–156.10.1006/jssc.2000.8827 ↗
4. Kodama, H., Oyaidzu, M., Sasaki, M., et al., Studies on Structural and Chemical Characterization for Boron Coating Films Deposited by PCVD, J. Nucl. Mater., 2004, vols. 329–333, pp. 889–893.10.1016/j.jnucmat.2004.04.277 ↗
5. Nakano, S., Hemley, R.J., Gregoryanz, E.A., et al., Pressure Induced Transformations of Molecular Boron Hydride, J. Phys.: Condens. Matter, 2002, vol. 14, no. 44, pp. 10 453–10 456.
6. Nakano, S, Hemley, R.J, Tschauner, O, and Mao, H.K, High-Pressure/High-Temperature Transformations of Boron Hydride, Proc. 8th NIRIM Int. Symp. Advanced Materials (ISAM 2001): Ultra-High Pressure Research-Novel Process for New Materials, Akaishi, M. et al., Eds., Tsukuba: Natl. Inst. Res. Inorganic Materials, 2001, pp. 49–50.
7. Becher, H.J. and Mattes, R., Tetragonal Boron-I and Its Derivatives, Boron and Refractory Borides, Matkovich, V.I., Ed., Berlin: Springer, 1977, pp. 107–114.10.1007/978-3-642-66620-9_9 ↗
8. Shirai, K., Masago, A., and Katayama-Yoshida, H., High-Pressure Properties and Phase Diagram of Boron, Phys. Status Solidi B, 2007, vol. 244, pp. 303–308.10.1002/pssb.200672589 ↗
9. Will, G. and Kossobutzki, K.H., X-Ray Diffraction Analysis of B50C2 and B50N2 Crystallizing in the “Tetragonal” Boron Lattice, J. Less-Common Met., 1976, vol. 47, pp. 33–38.10.1016/0022-5088(76)90070-9 ↗
10. Shirai, K., Electronic Structures and Mechanical Properties of Boron and Boron-Rich Crystals, J. Superhard Mater., 2010, vol. 32, pp. 336–345.10.3103/S1063457610050059 ↗
11. Hayami, W. and Otani, S., First-Principles Study of the Crystal and Electronic Structures of α-Tetragonal Boron, J. Solid State Chem., 2010, vol. 183, no. 7, pp. 1521–1528.10.1016/j.jssc.2010.04.036 ↗
12. Hayami, W. and Otani, S., The Role of Surface Energy in the Growth of Boron Crystals, J. Phys. Chem. C, 2007, vol. 111, pp. 688–692.10.1021/jp065680s ↗
13. Wang, S., Mao, W.L., and Autrey, T., Bonding in Boranes and Their Interaction with Molecular Hydrogen at Extreme Conditions, J. Chem. Phys., 2009, vol. 131, paper 144 508.10.1063/1.3244982 ↗