Abstract

The oxygen-ion conductivity of porous materials, the coarse-grained pyrochlore-like Sm 2 Ti 2 O 7 and fine-grained Sm 2 TiO 5 compounds, produced by mechanical activation of initial oxides is studied at 400–1000 °C. The Sm 2 TiO 5 samples contain ∼15 wt % of the nanosized pyrochlore-like Sm 2 TiO 5 phase in addition to the rhombic phase. As determined by impedance spectroscopy, the ionic conductivities of Sm 2 TiO 5 and Sm 2 Ti 2 O 7 at 1000°C are 1.3 × 10 −3 and 1.8 × 10 −4 S cm −1 , and the activation energies of the bulk and grainboundary conductivities of the materials are 1.04 and 1.24 eV for Sm 2 TiO 5 and 1.69 and 1.80 eV for Sm 2 Ti 2 O 7 .
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Nuclear materials and radiation effects · Radioactive element chemistry and processing · Electronic and Structural Properties of Oxides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Tuller, H.L., and Moon, P.K., Fast-Ion Conductors: Future Trends, Mater. Sci. Eng., 1988, vol. 1, pp. 171–191.10.1016/0921-5107(88)90018-9 ↗
2. Tuller, H.L., Ionic and Mixed Conductors: Materials Design and Optimization, in High Temperature Electrochemistry: Ceramics and Metals (Proc. 17-th Intern. Symp. on Materials Science, Riso, 1996), Poulsen, F.W. et al, Eds., Riso, Denmark: National Laboratory Roskilde, 1996, pp. 139–153.
3. Ivanov-Shits, A.K., and Murin, I.V., Ionika tverdogo tela (Solid State Ionics), vol. 1, St. Petersburg: St.-Peterb. Gos. Univ., 2000.
4. Minervini, L., Grimes, R.W., Tabira, Y., et al., The Oxygen Positional Parameter in Pyrochlores and its Dependence on Disorder, Philos. Mag. A, 2002, vol. 82, no. 1, pp. 123–135.10.1080/01418610208240001 ↗
5. Wuensch, B.J., Eberman, K.W., Heremans, C., et al., Connection between Oxygen-Ion Conductivity of Pyrochlore Fuel-Cell Materials and Structural Change with Composition and Temperature, Solid State Ionics, 2000, vol. 129, pp. 111–133.10.1016/S0167-2738(99)00320-3 ↗
6. Eberman, K.W., Wuensch, B.J., and Jorgensen, J.D., Order-Disorder Transformations Induced by Composition and Temperature Change in (SczYb1 − z)2Ti2O7 Pyrochlores, Prospective Fuel Cell Materials, Solid State Ionics, 2002, vol. 148, pp. 521–526.10.1016/S0167-2738(02)00099-1 ↗
7. Staneck, C.R., Minervini, L., and Grimes, R.W., Nonstoichiometry in A2B2O7 Pyrochlores, J. Am. Ceram. Soc., 2002, vol. 85, no. 11, pp. 2792–2798.10.1111/j.1151-2916.2002.tb00530.x ↗
8. Lyashenko, L.P., Kolbanev, I.V., and Shcherbakova, L.G., et al., Effect of a Nonequilibrium State on Phase Relations in the System TiO2-Sc2O3 (40–50 mol. % Sc2O3), Neorg. Mater., 2004, vol. 40, no. 8, pp. 955–962 [Inorg. Mater. (Engl. Transl.), vol. 40, no. 8, pp. 833–839].10.1023/B:INMA.0000037929.21412.0c ↗
9. Lyashenko, L.P., Shcherbakova, L.G., Kolbanev, I.V., et al., Mechanism of Structure Formation in Samarium and Holmium Titanates Prepared from Mechanically Activated Oxides, Neorg. Mater., 2007, vol. 43, no. 1, pp. 51–59 [Inorg. Mater. (Engl. Transl.), vol. 43, no. 1, pp. 46–54].10.1134/S0020168507010116 ↗
10. Okamota, M., Akimune, Y., Furuya, F., et al., Phase Transition and Electrical Conductivity of Scandia-Stabilized Zirconia Prepared By Spark Plasma Sintering Process, Solid State Ionics, 2005, vol. 176, nos. 7–8, pp. 675–680.10.1016/j.ssi.2004.10.022 ↗
11. Minervini L., Grimes R.W., Tabira Y. et al. The Oxygen Positional Parameter in Pyrochlores and its Dependence on Disoder // Philos. Mag. A. 2002. V. 82. № 1. P. 123–135.10.1080/01418610208240001 ↗
12. Etsell, T.H., and Flengas, S.N., Electrical Properties of Solid Oxide Electrolytes, Chem. Rev., 1970, vol. 70, no. 3, pp. 339–376.10.1021/cr60265a003 ↗
13. Powder Diffraction File, Swarthmore, Pa: Joint Committee on Powder Diffraction Standards, Card 22-1306.
14. Lyashenko, L.P., Nikonov, Yu.P., Raevskii, A.V., and Shcherbakova, L.G., The mechanism of Formation of Fluorite-Like Phases in TiO2-R2O3 (R = Y, Er, Sc) Systems, Materialovedenie, 1999, no. 1, pp. 29–33.
15. Xu, G., Zhang, Y., Liao, C., and Yan, C., Homogeneous Precipitation Synthesis and Electrical Properties of Scandia Stabilized Zirconia, Solid State Commun., 2002, vol. 121, no. 1, pp. 45–49.10.1016/S0038-1098(01)00444-6 ↗
16. Haering, C., Roosen, A., Schichl, H., and Schnoller, M., Degradation of the Electrical Conductivity in Stabilized Zirconia Systems, part 2: Scandia-Stabilized Zirconia, Solid State Ionics, 2005, vol. 176, nos. 3–4, pp. 261–268.10.1016/j.ssi.2004.07.039 ↗
17. Komissarova, L.N., Shatskii, V.N., Pushkina, G.Ya, et al., Khimiya redkikh elementov. Soedineniya redkosemel’nykh elementov. Karbonaty, oksalaty, nitraty, titanaty (Chemistry of Rare Elements. Rare-Earth Element Compounds: Carbonates, Oxalates, Nitrates, and Titanates), Moscow: Nauka, 1984.