Synthesis, structure, and physical properties of boron-doped diamond
Source abstract
Abstract
Microcrystalline boron-doped diamond powders consisting of octahedrally faceted crystals have been synthesized in the C-H-B system at a pressure of 8 GPa and temperatures above 2000 K. The presence of boron has been shown to reduce the parameters of diamond synthesis compared to the binary system C-H (naphthalene). One possible reason for the reduction in synthesis parameters is the formation of less perfect graphite in the boron system in an intermediate step of diamond synthesis. At B/(C + B) ratios of about 5–10 at % in the C-H-B (naphthalene + boron) system, superconducting diamond microcrystals have been synthesized.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Diamond and Carbon-based Materials Research · Boron and Carbon Nanomaterials Research · High-pressure geophysics and materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Vishnevskii, A.S., Gontar’, A.G., Torishnii, V.I., and Shul’zhenko, A.A., Electrical Conductivity of Heavily Doped p-Type Diamond, Fiz. Tekh. Poluprovodn. (Leningrad), 1981, vol. 15, no. 2, pp. 1145–1149.
2. Takano, Y., Nagao, M., Kobayashi, K., et al., Superconductivity in CVD Diamond Thin Film Well-above Liquid Helium Temperature, Appl. Phys. Lett., 2004, vol. 85, pp. 2851–2853.10.1063/1.1802389 ↗
3. Bustarret, E., Kacmarcik, J., Marcenat, C., et al., Dependence of Superconducting Transition Temperature on the Doping Level in Single-Crystalline Diamond Films, Phys. Rev. Lett., 2004, vol. 93, pp. 237 005 1–4.10.1103/PhysRevLett.93.237005 ↗
4. Ekimov, E.A., Sidorov, V.A., Bauer, E.D., et al., Superconductivity in Diamond, Nature, 2004, vol. 428, pp. 542–545.10.1038/nature02449 ↗
5. Dubrovinskaia, N., Eska, G., Sheshin, G.A., et al., Superconductivity in Polycrystalline Boron-Doped Diamond Synthesized at 20 GPa and 2700 K, J. Appl. Phys., 2006, vol. 99, pp. 0339031–7.10.1063/1.2166645 ↗
6. Irifune, T., Kurio, A., Sakamoto, S., et al., Ultrahard Polycrystalline Diamond from Graphite, Nature, 2003, vol. 421, pp. 599–600.10.1038/421599b ↗
7. Voronov, O.A. and Rakhmanina, A.V., Cubic Cell Parameter of Boron-Doped Diamond, Neorg. Mater., 1993, vol. 29, no. 5, pp. 623–626 [Inorg. Mater. (Engl. Transl.), vol. 29, no. 5, pp. 533–535].
8. Khvostantsev, L.G., Vereshchagin, L.F., and Novikov, A.P., Device of Toroid Type for High Pressure Generation, High Temp.-High Pressures, 1977, vol. 9, pp. 637–639.
9. Ekimov, E.A., Sadykov, R.A., Gierlotka, S., et al., High-Pressure Cell for High-Temperature Experiments in a Toroid Chamber, Prib. Tekh. Eksp., 2004, no. 3, pp. 157–159.
10. Ekimov, E.A., Sidorov, V.A., Mel’nik, N.N., et al., Synthesis of Polycrystalline Diamond in the Boron Carbide-Graphite and Boron-Graphite Systems under High Pressure and Temperature, J. Mater. Sci., 2004, vol. 39, pp. 4957–4960.10.1023/B:JMSC.0000035345.99616.24 ↗
11. Aleksandrov, I.V., Goncharov, A.F., Zisman, A.N., and Stishov, S.M., Diamond at High Pressures: Raman Scattering, Equation of State, and High-Pressure Scale, Zh. Eksp. Teor. Fiz., 1987, vol. 93, pp. 680–691.
12. Novikov, N.V., Fizicheskie svoistva almaza: Spravochnik (Physical Properties of Diamond: A Handbook), Kiev: Naukova Dumka, 1987.
13. Voronov, O.A. and Rakhmanina, A.V., Kinetics of Diamond Carbonization under Pressure, Neorg. Mater., 1992, vol. 28, no. 7, pp. 1408–1413.
14. Hishiyama, Y., Irumano, H., and Kaburagi, Y., Structure, Raman Scattering, and Transport Properties of Boron-Doped Graphite, Phys. Rev. B: Condens. Matter Mater. Phys., 2001, vol. 63, pp. 2454061 1–11.10.1103/PhysRevB.63.245406 ↗
15. Wentorf, R.H., Some Studies of Diamond Growth Rates, J. Phys. Chem., 1971, vol. 75, pp. 1833–1837.10.1021/j100681a013 ↗