Liquid-Assisted Interaction of Iridium with Silicon Carbide Ceramics
Source abstract
Abstract
Abstract— Liquid-assisted processes that occur in iridium–silicon carbide diffusion couples have been studied in the temperature range 1500–1800°C at different heat treatment times. We have examined the microstructure and determined the elemental and phase compositions of the diffusion zone forming above eutectic temperatures and/or the melting points of individual reaction products: iridium silicides. The microstructure of the diffusion zone forming under liquid formation conditions has been shown to differ from that forming under the conditions of solid-state reaction between iridium and silicon carbide. At temperatures above 1700°C, the silicon content of the Ir–Si melt exceeds 50 mol %, which leads to crystallization of the Ir3Si4 and Ir3Si5 phases during cooling. The carbon resulting from reaction between iridium and SiC undergoes graphitization with increasing heat treatment temperature and time.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Nuclear materials and radiation effects · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Kim, Y.-W. and Malik, R., SiC ceramics, structure, processing and properties, Encyclopedia of Materials: Technical Ceramics and Glasses, Pomeroy, M., Ed., Oxford: Elsevier, 2021, pp. 150–164. https://doi.org/10.1016/B978-0-12-818542-1.00022-910.1016/B978-0-12-818542-1.00022-9 ↗
2. DiCarlo, J.A., Yun, H., Morscher, G.N., and Bhatt, R.T., SiC/SiC composites for 1200°C and above, Handbook of Ceramic Composites, Bansal, N.P., Ed., New York: Springer, 2005, pp. 77–98. https://doi.org/10.1007/0-387-23986-3_410.1007/0-387-23986-3_4 ↗
3. Wu, W. and Chen, Z., Iridium coating: processes, properties and application, part I, Johnson Matthey Technol. Rev., 2017, vol. 61, no. 1, pp. 16–28. https://doi.org/10.1595/205651317X69360610.1595/205651317X693606 ↗
4. Jin, X., Fan, X., Lu, C., and Wang, T., Advances in oxidation and ablation resistance of high and ultra-high temperature ceramics modified or coated carbon/carbon composites, J. Eur. Ceram. Soc., 2018, vol. 38, no. 1, pp. 1–28. https://doi.org/10.1016/j.jeurceramsoc.2017.08.01310.1016/j.jeurceramsoc.2017.08.013 ↗
5. Jehn, H., Volker, R., and Ismail, M.I., Iridium losses during oxidation, Platinum Met. Rev., 1978, vol. 22, no. 3, pp. 92–97.10.1595/003214078X2239297 ↗
6. Wimber, R.T., Hills, S.W., Wahl, N.K., and Tempero, C.R., Kinetics of evaporation/oxidation of iridium, Metall. Trans. A, 1977, vol. 8, no. 1, pp. 193–199. https://doi.org/10.1007/BF0267728110.1007/BF02677281 ↗
7. Wimber, R.T. and Kraus, H.G., Oxidation of iridium, Metall. Trans. A, 1974, vol. 5, no. 7, pp. 1565–1571. https://doi.org/10.1007/BF0264632710.1007/BF02646327 ↗
8. Criscione, J.M., Volk, H.F., and Smith, A.W., Protection of graphite from oxidation at 2100 deg C, AIAA J., 1966, vol. 4, no. 10, pp. 1791–1797. https://doi.org/10.2514/3.377910.2514/3.3779 ↗
9. Sun, L., Wang, B., and Wang, Y., A Schottky-junction-based platinum nanoclusters@silicon carbide nanosheet as long-term stable hydrogen sensors, Appl. Surf. Sci., 2019, vol. 473, pp. 641–648. https://doi.org/10.1016/j.apsusc.2018.12.19310.1016/j.apsusc.2018.12.193 ↗
10. Kerimov, E.A., Study of photodetectors with Schottky barriers based on the IrSi–Si contact, Russ. Microelectron., 2023, vol. 52, no. 1, pp. 32–34. https://doi.org/10.1134/S106373972203004010.1134/S1063739722030040 ↗
11. Hill, P.J., Cornish, L.A., and Witcomb, M.J., Constitution and hardnesses of the Al–Ir system, J. Alloys Compd., 1998, vol. 280, nos. 1–2, pp. 240–250. https://doi.org/10.1016/S0925-8388(98)00748-810.1016/S0925-8388(98)00748-8 ↗
12. Katoh, Y. and Snead, L.L., Silicon carbide and its composites for nuclear applications – historical overview, J. Nucl. Mater., 2019, vol. 526, p. 151849. https://doi.org/10.1016/j.jnucmat.2019.15184910.1016/j.jnucmat.2019.151849 ↗
13. Yunfeng, H., Zhengxian, L., Jihong, D., and Chunliang, H., Solid state reaction of Ir with SiC and Ir with Y2O3, Rare Met. Mater. Eng., 2012, vol. 41, no. 7, pp. 1149–1152. https://doi.org/10.1016/S1875-5372(12)60059-910.1016/S1875-5372(12)60059-9 ↗
14. Golosov, M.A., Lozanov, V.V., Titov, A.T., and Baklanova, N.I., Toward understanding the reaction between silicon carbide and iridium in a broad temperature range, J. Am. Ceram. Soc., 2021, vol. 104, no. 12, pp. 6653–6669. https://doi.org/10.1111/jace.1797810.1111/jace.17978 ↗
15. Golosov, M., Lozanov, V., and Baklanova, N., The study of the iridium–silicon carbide reaction by Raman and IR spectroscopy, Mater. Today: Proc., 2020, vol. 25, pp. 352–355. https://doi.org/10.1016/j.matpr.2019.12.08810.1016/j.matpr.2019.12.088 ↗
16. Golosov, M.A., Utkin, A.V., Lozanov, V.V., Titov, A.T., and Baklanova, N.I., Microstructural patterning of the reaction zone formed by solid-state interaction between iridium and SiC ceramics, Materials, 2023, vol. 27, p. 101647. https://doi.org/10.1016/j.mtla.2022.10164710.1016/j.mtla.2022.101647 ↗
17. Camarano, A., Narciso, J., and Giuranno, D., Solid state reactions between SiC and Ir, J. Eur. Ceram. Soc., 2019, vol. 39, no. 14, pp. 3959–3970. https://doi.org/10.1016/j.jeurceramsoc.2019.06.00910.1016/j.jeurceramsoc.2019.06.009 ↗
18. Okamoto, H., Ir–Si (iridium–silicon), J. Phase Equilib. Diffus., 2007, vol. 28, no. 5, pp. 495–495. https://doi.org/10.1007/s11669-007-9151-510.1007/s11669-007-9151-5 ↗
19. Bhanumurthy, K. and Schmid-Fetzer, R., Interface reactions between silicon carbide and metals (Ni, Cr, Pd, Zr), Composites, 2001, vol. 32, nos. 3–4, pp. 569–574. https://doi.org/10.1016/S1359-835X(00)00049-X10.1016/S1359-835X(00)00049-X ↗
20. Chou, T.C., High temperature reactions between SiC and platinum, J. Mater. Sci., 1991, vol. 26, no. 5, pp. 1412–1420. https://doi.org/10.1007/BF0054448710.1007/BF00544487 ↗
21. Searcy, A.W. and Finnie, L.N., Stability of solid phases in the ternary systems of silicon and carbon with rhenium and the six platinum metals, J. Am. Ceram. Soc., 1962, vol. 45, no. 6, pp. 268–273. https://doi.org/10.1111/j.1151-2916.1962.tb11142.x10.1111/j.1151-2916.1962.tb11142.x ↗
22. Novakovic, R., Delsante, S., and Giuranno, D., Design of composites by infiltration process: a case study of liquid Ir–Si alloy/SiC systems, Materials, 2021, vol. 14, no. 20, p. 6024. https://doi.org/10.3390/ma1420602410.3390/ma14206024 ↗