Oxidation behavior of sulfidation processed TiAl–2 at.% X (X=V, Fe, Co, Cu, Nb, Mo, Ag and W) alloys at 1173 K in air
Source abstract
Abstract
Abstract The oxidation behavior of sulfidation processed TiAl–2 at.% X (X=V, Fe, Co, Cu, Nb, Mo, Ag, and W) alloys was investigated at 1173 K in air for up to 630 ks under a heat-cycle condition between 1173 K and room temperature. Oxidation behavior was classified into two groups: group A with alloys containing Fe, Nb, Mo and W, and group B containing V, Co, Cu and Ag. The TiAl binary alloy belonged to group B. During the sulfidation processing, the alloying elements in group A formed aluminides on the TiAl 3 layer, while the group B alloys formed a TiAl 3 (TiAl 2 included) layer including a small amount of the third element. The cross-sectional microstructures for group A show the sequence; oxide scale/TiAlX/TiAl 2 /alloy substrate, and for group B oxide scale/Ti 3 Al/alloy substrate. The alloys in group A (except Nb containing alloy) showed some scale exfoliation at the initial stage of oxidation, but only very little exfoliation after long oxidation times, whereas alloys in group B showed little exfoliation at the first several cycles, and then tended to exfoliate significantly, resulting in very rapid oxidation. The TiAlX/TiAl 2 layers formed by the reaction between the X-aluminide and TiAl 3 improve the oxidation properties of the group A alloys.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · High-Temperature Coating Behaviors · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Suzuki · Mater Trans JIM · 1991 · 32 · 101710.2320/matertrans1989.32.1017 ↗
2. Taniguchi · C, Matsumoto Y, Shibata T, Materials Science and Engineering A · 2000 · 277 · 22910.1016/S0921-5093(99)00542-0 ↗
3. Brady · P, Smialek J.L, Terepka F. Scripta Metall Mater. · 1995 · 32 · 165910.1016/0956-716X(95)00251-P ↗
4. Schumacher · Mater. Corros · 1999 · 50 · 16210.1002/(SICI)1521-4176(199903)50:3<162::AID-MACO162>3.0.CO;2-O ↗
5. Lei · K, Zhu X.P, Han S.Q, Wang D.Y, Wang F.G, Wang F. Materials Chemistry and Physics · 2000 · 65 · 249
6. Xhou · Surface and Coatings Technology · 2000 · 127 · 220
7. Katsman · Surface and Coating Technology · 2000 · 127 · 22010.1016/S0257-8972(00)00555-7 ↗
8. Shida · Oxid Met · 1996 · 45 · 19710.1007/BF01046826 ↗
9. McKee · W, Huang S.C.. Corros Sci. · 1992 · 33 · 189910.1016/0010-938X(92)90192-6 ↗
10. Rahmel · Mater Corros · 1995 · 46 · 27110.1002/maco.19950460503 ↗
11. Yoshioka · Zairyo-to-Kankyo · 1996 · 45 · 71210.3323/jcorr1991.45.712 ↗
12. Yoshioka · Corros Eng. · 1996 · 45 · 74910.3323/jcorr1991.45.712 ↗
13. Yoshioka · Zairyo-to-Kankyo · 1999 · 48 · 21410.3323/jcorr1991.48.214 ↗
14. Yoshioka · Zairyo-to-Kankyo · 1999 · 48 · 22010.3323/jcorr1991.48.220 ↗
15. Binary Alloy Phase Diagram, ASM vol.1, p. 175.
16. Van Loo · Act Metallurgica · 1973 · 21 · 7310.1016/0001-6160(73)90221-6 ↗
17. Sprengel · Intermetallics · 1996 · 4 · 18510.1016/0966-9795(94)00033-6 ↗
18. Narita · Intermetallics · 2000 · 8 · 37110.1016/S0966-9795(99)00117-X ↗
19. Izumi · Intermetallics · 2000 · 8 · 89110.1016/S0966-9795(00)00028-5 ↗
20. Schutze-Niederau · Oxid Met · 1999 · 52 · 22510.1023/A:1018839511102 ↗
21. Perkins · A, Chiang K.T. Scripta Met · 1987 · 21 · 150510.1016/0036-9748(87)90291-2 ↗
22. Brady M.P, Brindiey W.J, Smialek J.L, Locci I. E. JOM November 1996: 46.10.1007/BF03223244 ↗
23. Zheng · Scripta Metall Mater. · 1995 · 33 · 4710.1016/0956-716X(95)00155-O ↗
24. Cheng · Scripta Materialia · 1996 · 34 · 70710.1016/1359-6462(95)00552-8 ↗
25. Fujimoto · J of JIM · 2000 · 64 · 502
26. Yoshihara · Abstract of the Japan Institute of Metals · 1999 · 125 · 507