Abstract

The effect of yttrium (Y) on the glass-forming ability (GFA), mechanical properties and corrosion of (Cu 50Zr 43Al 7) 100-xY x ( x = 0, 2 and 4, in at. %) alloys was investigated. The GFA of Cu 50Zr 43Al 7 alloy was improved by the addition of Y, with a GFA of 15 mm in diameter being obtained for (Cu 50Zr 43Al 7) 98Y 2 . In uniaxial compression, the bulk metallic glasses (BMGs) exhibited a limited plastic strain of less than 1%, however compressive fracture strength and Young`s modulus of 1787–2006 MPa and 101–122 GPa were achieved, respectively. Fracture surfaces and shear bands were studied via scanning electron microscopy. The corrosion behavior of BMGs was analyzed by potentiodynamic polarization experiments and electrochemical impedance spectroscopy (EIS) in acidic chloride (1 M HCl) and neutral chloride (0.6 M NaCl) environments. As a result of the Y addition, the corrosion resistance of the base BMG was improved.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Electromagnetic wave absorption materials · Electrodeposition and Electroless Coatings

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. Stabilization of metallic supercooled liquid and bulk amorphous alloys10.1016/S1359-6454(99)00300-6 ↗
2. Mechanical behavior of amorphous alloys10.1016/j.actamat.2007.01.052 ↗
3. Effect of additional elements on the corrosion behavior of a Cu–Zr–Ti bulk metallic glass10.1016/j.msea.2003.10.034 ↗
4. Recent development and application products of bulk glassy alloys10.1016/j.actamat.2010.11.027 ↗
5. Improving the plasticity of bulk metallic glasses via pre-compression below the yield stress10.1016/j.msea.2014.02.065 ↗
6. High-strength Cu-based bulk glassy alloys in Cu–Zr–Ti and Cu–Hf–Ti ternary systems10.1016/S1359-6454(01)00181-1 ↗
7. Effects of a minor addition of Si and/or Sn on formation and mechanical properties of Cu–Zr–Ti bulk metallic glass
8. Effect of Ge addition on mechanical properties and fracture behavior of Cu–Zr–Al bulk metallic glass10.1016/j.jallcom.2009.05.023 ↗
9. Effect of Si addition on glass-forming ability and mechanical properties of Cu–Zr–Al bulk metallic glass10.1016/j.msea.2010.07.067 ↗
10. Roles of minor rare-earth elements addition in formation and properties of Cu–Zr–Al bulk metallic glasses10.1016/j.jallcom.2015.01.036 ↗
11. Microstructure and mechanical properties of a Cu-Zr based bulk metallic glass containing atomic scale chemical heterogeneities10.1016/j.msea.2018.05.082 ↗
12. Mechanical properties and crystallization kinetics of Er-containing Cu–Zr–Al bulk metallic glasses with excellent glass forming ability10.1016/j.vacuum.2020.109223 ↗
13. Effective role of minor silicon addition on crystallization kinetics of Cu50Zr43Al7 bulk metallic glass10.1007/s00339-021-04394-z ↗
14. Deformation behavior of Zr33Hf8Ti6Cu32Ni10Co5Al6 high-entropy bulk metallic glass and Cu47Zr47Al6 low-entropy bulk metallic glass at room and high temperatures10.1016/j.msea.2021.142499 ↗
15. Suryanarayana · 2017
16. Effects of Y addition on structural and mechanical properties of CuZrAl bulk metallic glass10.1016/S1003-6326(11)61254-5 ↗
17. Influence of yttrium addition on the glass forming ability in Cu–Zr–Al alloys10.1016/j.msea.2006.09.177 ↗
18. Thermal and mechanical properties of Cu-based Cu-Zr-Ti-Y bulk glassy alloys10.2320/matertrans.42.2042 ↗
19. Formation of bulk metallic glasses from Cu-Zr based alloys with yttrium addition10.1016/S1875-5372(14)60124-7 ↗
20. Unusual glass-forming ability of bulk amorphous alloys based on ordinary metal copper10.1103/PhysRevLett.92.245504 ↗
21. Ti microalloying effect on corrosion resistance and thermal stability of CuZr-based bulk metallic glasses10.1016/j.jallcom.2009.03.022 ↗
22. Corrosion behavior and glass-forming ability of Cu–Zr–Al–Nb alloys10.1016/j.jnoncrysol.2007.05.119 ↗
23. Thermodynamic and structural basis for electrochemical response of Cu–Zr based metallic glass10.1016/j.jallcom.2015.03.255 ↗
24. Corrosion behavior and in vitro biocompatibility of Zr–Al–Co–Ag bulk metallic glasses: an experimental case study10.1016/j.jnoncrysol.2012.04.022 ↗
25. Influence of minor addition of in on corrosion resistance of Cu-based bulk metallic glasses in 3.5% NaCl solution10.1016/S1875-5372(14)60047-3 ↗
26. Thermodynamic and kinetic interpretation of the glass-forming ability of Y-containing Cu-Zr-Al bulk metallic glasses10.1016/j.jnoncrysol.2021.121266 ↗
27. Atomic level structure in multicomponent bulk metallic glass10.1103/PhysRevLett.102.245501 ↗
28. Atomic-level structure and structure–property relationship in metallic glasses10.1016/j.pmatsci.2010.12.002 ↗
29. Effects of additional elements (M) on the thermal stability and structure of (Zr52.2Cu39.1Al8.7)100−xMx (M = Ag, Be, Gd, x = 8, 7, 2) amorphous alloys10.1007/s10853-009-3523-7 ↗
30. Superior glass-forming ability of CuZr alloys from minor additions10.1557/jmr.2006.0212 ↗
31. The atomic-scale mechanism for the enhanced glass-forming-ability of a Cu-Zr based bulk metallic glass with minor element additions10.1038/srep04648 ↗
32. Networked interpenetrating connections of icosahedra: effects on shear transformations in metallic glass10.1016/j.actamat.2010.09.020 ↗
33. Cephradine as corrosion inhibitor for copper in 0.9% NaCl solution10.1016/j.molstruc.2018.01.031 ↗
34. Three indazole derivatives as corrosion inhibitors of copper in a neutral chloride solution10.1016/j.corsci.2017.07.012 ↗
35. Inhibition effect of 4-amino-antipyrine on the corrosion of copper in 3wt.% NaCl solution10.1016/j.corsci.2011.12.009 ↗
36. Intramolecular synergistic effect of glutamic acid, cysteine and glycine against copper corrosion in hydrochloric acid solution10.1016/j.tsf.2011.07.009 ↗
37. Electrochemical and surface studies of some Porphines as corrosion inhibitor for J55 steel in sweet corrosion environment10.1016/j.apsusc.2015.10.129 ↗
38. Performances of alkaloid extract from Rauvolfia macrophylla Stapf toward corrosion inhibition of C38 steel in acidic media10.1021/acsomega.9b01076 ↗
39. Evaluation of inhibitive action of some quaternary N-heterocyclic compounds on the corrosion of Al–Cu alloy in hydrochloric acid10.1016/j.matchemphys.2008.09.065 ↗
40. Enhanced corrosion resistance of mild steel in 1M HCl solution by trace amount of 2-phenyl-benzothiazole derivatives: experimental, quantum chemical calculations and molecular dynamics (MD) simulation studies10.1016/j.corsci.2016.11.002 ↗
41. Identification of diverse 1,2,3-triazole-connected benzyl glycoside-serine/threonine conjugates as potent corrosion inhibitors for mild steel in HCl10.1016/j.corsci.2012.07.001 ↗
42. The inhibition of low carbon steel corrosion in hydrochloric acid solutions by succinic acid: Part I. Weight loss, polarization, EIS, PZC, EDX and SEM studies10.1016/j.electacta.2006.10.019 ↗
43. Establishment of equivalent circuits from electrochemical impedance spectroscopy study of corrosion inhibition of steel by pyrazine in sulphuric acidic solution10.1016/j.apsusc.2005.06.035 ↗
44. Corrosion behavior of TiZrHfBeCu (Ni) high-entropy bulk metallic glasses in 3.5 wt.% NaCl10.1038/s41529-022-00287-5 ↗
45. Effects of Si additions on the glass-forming ability and corrosion resistance of Cu49Zr45Al6 bulk metallic glass10.5006/0919 ↗
46. Effects of niobium on thermal stability and corrosion behavior of glassy Cu–Zr–Al–Nb alloys10.1016/j.jpcs.2005.11.012 ↗
47. Corrosion behavior and glass-forming ability of Cu–Zr–Al–Nb alloys10.1016/j.jnoncrysol.2007.05.119 ↗
48. Corrosion behavior of Cu 60 Zr 30 Ti 10 metallic glass in the Cl–containing solution
49. Pitting corrosion of zirconium-based bulk glass-matrix composites10.1016/j.msea.2005.09.062 ↗
50. Comparison of the corrosion of bulk amorphous steel with conventional steel10.1016/j.corsci.2009.09.016 ↗
51. Atomic-scale Nb heterogeneity induced icosahedral short-range ordering in metallic glasses10.1016/j.jmst.2021.08.046 ↗
52. Atomic-scale icosahedral short-range ordering in a rejuvenated Zr-based bulk metallic glass upon deep cryogenic treatment10.1016/j.msea.2022.143565 ↗
53. Corrosion resistance of Cu–Zr–Al–Y and Zr–Cu–Ni–Al–Nb bulk metallic glasses10.1016/j.jallcom.2006.08.112 ↗
54. Glass-forming ability and corrosion resistance of ZrCuAlCo bulk metallic glass10.1016/j.jmst.2015.12.012 ↗
55. Improving plasticity of the Zr46Cu46Al8 bulk metallic glass via thermal rejuvenation10.1016/j.scib.2018.04.021 ↗
56. In situ observation of pitting corrosion of the Zr50Cu40Al10 bulk metallic glass10.1016/j.intermet.2008.12.011 ↗
57. Effects of partial crystallization on compression and fatigue behavior of Zr-based bulk metallic glasses10.1557/jmr.2007.0059 ↗
58. Formation and corrosion behavior of mechanically-alloyed Cu–Zr–Ti bulk metallic glasses10.3390/met7040148 ↗
59. Effect of the substitution of Ag and Ni for Cu on the glass forming ability and plasticity of Cu60Zr30Ti10 alloy10.1016/j.scriptamat.2006.01.023 ↗
60. Effect of Hf substitution Cu on glass-forming ability, mechanical properties and corrosion resistance of Ni-free Zr–Ti–Cu–Al bulk metallic glasses10.1016/j.jallcom.2019.07.240 ↗
61. A novel Ni-free Zr-based bulk metallic glass with high glass forming ability, corrosion resistance and thermal stability10.1186/s10033-020-00482-y ↗
62. High glass-forming ability and unusual deformation behavior of new Zr-Cu-Fe-Al bulk metallic glasses10.4028/www.scientific.net/MSF.654-656.1042 ↗
63. Improved mechanical properties and pitting corrosion resistance of Zr65Cu17.5Fe10Al7.5 bulk metallic glass by isothermal annealing10.1016/j.jnoncrysol.2016.08.014 ↗
64. Mechanical and corrosion properties of Ti-Ni-Cu-Zr metallic glass matrix composites10.1016/j.jallcom.2017.08.120 ↗