Microstructural influences on fatigue threshold behavior and fracture toughness of an additively manufactured γ-titanium aluminide
Source abstract
Abstract
The fracture and fatigue behavior of an additively manufactured γ-TiAl alloy (BMBF3) produced by selective electron beam melting and further subjected to two different heat treatment conditions was investigated. As one of the heat-treatments led to a pronounced layer structure, the experiments were also performed with different specimen orientations to account for possible anisotropy effects. In order to characterize the frequently found peculiarities of the local fracture process in this material class, such as shear ligament bridging, static and cyclic R-curves were recorded. In addition, also fatigue crack growth curves were measured. The results were critically compared with the properties of a selected heat treatment condition of an established TNM alloy manufactured by a conventional processing route. The investigations show that large α2/γ-colonies lead to high fracture toughness, but have almost no positive effect on the long-crack fatigue threshold. On the other hand, duplex microstructures with small α2/γ-colonies and thick lamellae favor high long-crack thresholds, but low fracture toughness. Microstructures with high fractions of globular γ-phase exhibited both, low fracture toughness and low long-crack fatigue threshold values. In comparison to the established TNM reference alloy, the additively manufactured counterparts can compete especially when the evolving anisotropy of the properties is taken into account for component design.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Intermetallics and Advanced Alloy Properties · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Advances in gammalloy materials–processes–application technology: Successes, dilemmas, and future10.1007/s11837-018-2747-x ↗
2. Intermetallic β-solidifying γ-TiAl based alloys − from fundamental research to application10.1002/adem.201600735 ↗
3. Schloffer · 2013
4. Additive manufacturing of metallic components by selective electron beam melting — a review10.1080/09506608.2016.1176289 ↗
5. Designing advanced intermetallic titanium aluminide alloys for additive manufacturing10.1016/j.intermet.2021.107109 ↗
6. Effect of stress ratio on fatigue crack growth in TiAl intermetallics at room and elevated temperatures10.1016/S0921-5093(00)00958-8 ↗
7. High-temperature fracture and fatigue resistance of a ductile β-TiNb reinforced γ-TiAl intermetallic composite10.1016/S1359-6454(98)00115-3 ↗
8. High-temperature fatigue-crack growth behavior in a two-phase (γ + α2) TiAl intermetallic alloy10.1016/0956-716X(95)00208-D ↗
9. On the fatigue behavior of γ-based titanium aluminides: role of small cracks10.1016/S1359-6454(98)00409-1 ↗
10. Evolution of fatigue crack growth and fracture behavior in gamma titanium aluminide Ti-43.5Al-4Nb-1Mo-0.1B (TNM) forgings10.1016/j.ijfatigue.2018.01.026 ↗
11. Processing 4th generation titanium aluminides via electron beam based additive manufacturing – characterization of microstructure and mechanical properties10.1016/j.mtla.2020.100902 ↗
12. In-situ aluminum control for titanium aluminide via electron beam powder bed fusion to realize a dual microstructure
13. The cyclic R-curve – determination, problems, limitations and application10.1016/j.engfracmech.2017.09.032 ↗
14. The influence of irregularities in the crack shape on the crack extension measurement by means of the direct-current-potential-drop method10.1520/JTE12039J ↗
15. How electron beam melting tailors the Al-sensitive microstructure and mechanical response of a novel process-adapted γ-TiAl based alloy10.1016/j.matdes.2021.110187 ↗
16. Fracture of convoluted and lamellar α2 + γ TiAl alloys10.1016/j.intermet.2011.11.001 ↗
17. Fracture and R-curve behavior of an intermetallic β-stabilized TiAl alloy with different nearly lamellar microstructures10.1016/j.intermet.2014.04.005 ↗
18. Colony boundary resistance to crack propagation in lamellar Ti-46Al10.1016/S1359-6454(02)00559-1 ↗
19. Slightly curved or kinked cracks10.1007/BF00012619 ↗
20. In situ fracture observations of distinct interface types within a fully lamellar intermetallic TiAl alloy10.1557/s43578-020-00088-z ↗
21. Crack propagation resistance of TiAl alloys10.1557/s43577-022-00387-2 ↗
22. Fatigue and fracture behavior of a fine-grained lamellar TiAl alloy10.1007/s11661-997-0084-8 ↗
23. Fatigue crack closure: a review of the physical phenomena10.1111/ffe.12578 ↗