journal article·2007-05

Simulation of hot compression of Ti–Al alloy

Jin-song Huang, Lan Huang, Bin Liu, Yong-hong Zhang, Wei Zhang, Xiao-yu He, Yong Liu

Intermetallics· Volume 15· Issue 5-6
Publisher page

Abstract

Abstract Hot compressive experiments of Ti–45Al–7Nb–0.15B–0.4W (mole fraction, %) alloy canned by 45# carbon steel were conducted at 1050–1230 °C on Gleeble1500 hot simulator with nominal deformation of 30% and strain rate of 0.01 s−1. The displacement–loading curves were obtained, and the macrostructure and microstructure were observed. The results show that the hot compressive temperature of TiAl alloy must be higher than 1050 °C and lower than 1230 °C with 45# steel can, and its optimum temperature is 1180 °C. The highest actual deformation of TiAl alloy canned by 45# steel is 50% with nominal deformation of 30%. The grains after being hotly compressed are flattened and elongated.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Energetic Materials and Combustion

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Structural transformations activated during the formation of the lamellar microstructure of TiAl alloys10.1016/j.intermet.2004.12.009 ↗
2. Oxidation behavior of gamma alloys designed for high temperature applications10.1016/j.intermet.2004.12.007 ↗
3. Creep of nearly lamellar TiAl alloy containing W10.1016/j.scriptamat.2004.05.005 ↗
4. Inhomogeneous microstructure in highly alloyed cast TiAl-based alloys, caused by microsegregation10.1016/j.scriptamat.2005.01.024 ↗
5. Microstructures and properties of powder metallurgy TiAl alloys10.1016/S0921-5093(02)00639-1 ↗
6. Porosity and argon concentration in gas atomized γ-TiAl powder and hot isostatically pressed compacts10.1016/S0921-5093(98)00656-X ↗
7. The brittle–ductile transition in HIP consolidated near γ-TiAl+W and TiAl+Cr powder alloys10.1016/0921-5093(94)03214-9 ↗
8. Nitrogen-induced powder formation of titanium aluminides during mechanical alloying10.1016/S0966-9795(00)00002-9 ↗
9. Structural characterization and tensile properties of a high niobium containing gamma TiAl sheet obtained by powder metallurgical processing10.1016/j.intermet.2003.10.005 ↗
10. Effect of boron addition on tensile ductility in lamellar TiAl alloys10.1016/S0966-9795(02)00087-0 ↗
11. The mechanism of grain refinement in TiAl alloys by boron addition – an alternative hypothesis10.1016/S0966-9795(99)00063-1 ↗
12. Effects of B and W alloying additions on the formation and stability of lamellar structures in two-phase γ-TiAl10.1016/S0966-9795(96)00070-2 ↗
13. Deformation behavior of differently processed γ-titanium aluminides10.1016/S0921-5093(01)01552-0 ↗
14. Microstructure control and high temperature properties of TiAl base alloys10.1016/S0966-9795(98)00047-8 ↗
15. Physical aspects of hot-working gamma-based titanium aluminides10.1016/j.intermet.2004.02.042 ↗
16. Effect of canned forging on microstructure of high Nb-containing TiAl alloy
17. Pack rolling of Ti–Al based alloy
18. Canned forging process of TiAl based alloy