The effects of temperature and pressure on the hydrogen decrepitation and hydrogen desorption of Sm2TM17 sintered magnets
Source abstract
Abstract
This study investigated the impact of hydrogen pressure and processing temperature on the hydrogen decrepitation of Sm 2 TM 17 sintered magnets (where TM = Co, Fe, Cu and Zr). Sm and Co are ‘critical elements’, hence there is interest in recycling these materials from end-of-life applications such as surface mounted permanent magnet motors and actuators. Hydrogen Decrepitation (HD) is a potential recycling technology, but the effect of different processing parameters has yet to be fully explored. Three commercial grades of Sm 2 TM 17 sintered magnets with different compositions and microstructures were subjected to HD treatments over 72 h, at hydrogen pressures of 2 and 18 bar and temperatures between 25 and 300 °C. The resulting powders were characterised to assess their particle size and morphology, hydrogen content and degassing behaviour. Thermal activation temperatures of 100–150 °C allowed for significant decrepitation to be observed across all Sm 2 TM 17 compositions at both 2 and 18 bar pressures. Degassing analysis showed that all decrepitated powders examined released hydrogen in a single step, with peak hydrogen desorption occurring between 200 and 260 °C. At HD temperatures of 300 °C the reaction ceased as degassing took precedence over hydrogen absorption. Particle size analysis indicated that adjusting HD processing parameters altered powder size greatly, e.g. increasing temperature increased particle size whereas increasing pressure decreased particle size. The sample with the smallest cell size, greatest Cu and Zr and lowest Fe content absorbed the least amount of hydrogen. It also generated the coarsest powder and degassed at the lowest temperatures. This has been linked to this sample having less of the main interstitial hydride forming 2:17 rhombohedral phase found in the magnet nanostructure.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Magnetic Properties of Alloys · Magnetic and transport properties of perovskites and related materials · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Magnetic properties of the intermetallic compound Co3+xTi1-x10.1143/JPSJ.27.258 ↗
2. Recent progress in 2:17-type permanent magnets10.1007/BF02648616 ↗
3. New type rare earth cobalt magnets with an energy product of 30 MG·Oe10.1143/JJAP.16.671 ↗
4. The hard-magnetic properties of rare earth-transition metal alloys10.1109/TMAG.1972.1067368 ↗
5. Rare-earth magnets: properties, processing and applications
6. High temperature 2:17 magnets: relationship of magnetic properties to microstructure and processing10.1109/20.908808 ↗
7. The potential of hydrogen in permanent magnet production10.1016/0022-5088(87)90524-8 ↗
8. The use of hydrogen to separate and recycle neodymium-iron-boron-type magnets from electronic waste10.1016/j.jclepro.2015.05.033 ↗
9. Recycling of SmCo5 magnets by HD process10.1016/j.jmmm.2018.01.064 ↗
10. Hydrogen reaction with SmCo compounds: literature review10.1007/s40831-018-0195-z ↗
11. Interstitial intermetallics10.1016/0304-8853(95)00603-6 ↗
12. Hydrogen decrepitation of a 2/17 sintered magnet at room temperature10.1016/j.jallcom.2006.11.139 ↗
13. The Bethe-Slater curve revisited; new insights from electronic structure theory
14. Large scale recycling of industrial scrap Sm (Co, Fe, Cu, Zr)z magnets into valuable permanent magnets large scale recycling of industrial scrap Sm (Co, Fe, Cu, Zr)z magnets into valuable permanent magnets
15. Sulfuric acid leaching of Sm–Co alloy waste and separation of samarium from cobalt10.1016/j.hydromet.2017.09.014 ↗
16. Mechanism of phase transformation in 2:17 type SmCo magnets investigated by phase stabilization10.1016/j.scriptamat.2015.10.041 ↗
17. The hydrogenation behaviour of the phases Sm2Co17 and Pr2Co1710.1007/BF00585720 ↗
18. Hydrogen decrepitation as a method of powder preparation of a 2:17-type, Sm(Co, Cu, Fe, Zr)8.92 magnetic alloy10.1007/BF01026543 ↗
19. Study of Sm(Co,Fe,Cu,Zr)7.1 magnets produced using a combination of hydrogen decrepitation and ball milling10.1063/1.347847 ↗
20. Microstructure and magnetic properties of Sm (CobalFe0.28Cu0.06Zr0.02)7.84 magnet prepared by hydrogen decrepitation and mechanical crushing10.1109/TMAG.2017.2696495 ↗
21. Effect of hydrogen pressure on hydrogenation and pulverization behavior of Sm(CoFeCuZr)z ingot and strip casting flake10.1016/j.jallcom.2022.167427 ↗
22. Combination strategy for high-performance Sm(CoFeCuZr)z sintered permanent magnet: synergistic improvement of the preparation process10.1016/j.actamat.2023.118901 ↗
23. Chemical stability and hydrogen reaction behavior of SmCo 2:17-type permanent magnets10.1002/adem.202201934 ↗
24. Simple chemical etching of Sm2TM17 magnet alloys for metallography purposes10.1016/1044-5803(90)90058-R ↗
25. Modern Sm-Co permanent magnets10.1016/B978-0-323-88658-1.00001-7 ↗