Abstract
Abstract High-performance tungsten molybdenum disilicide (MoxW1-xSi2) heating elements were prepared using a self-propagating high temperature synthesis process. The effect of post annealing on the degradation behavior of the alloy was experimentally investigated. Increasing the attrition milling time up to 20 min during powder preparation resulted in MoxW1-xSi2 heaters with the highest density, which increased the fracture strength compared to samples with shorter attrition times. Such samples were annealed and evaluated as heating elements using accelerated degradation tests and failure analysis in order to compare their structural characteristics and flexural strength with as-fabricated samples. The annealed MoxW1-xSi2 heater showed a relatively dense structure with few pores and no secondary phases, apart from a SiO2 layer. This favorable structure prevented bubble formation, which can result in fracturing of the heater, as revealed by evaluation at high temperatures with various heating rates. The flexural strength of the annealed specimen was 2.5-times higher than that of the as-fabricated specimen, which was attributed to removal of secondary phases during annealing. Failure time and surface load analyses were used to investigate the fracture mechanism of the MoxW1-xSi2 heaters in detail at 1790 °C by quantifying bubble formation and the presence of secondary phases.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. A comparative overview of molybdenum disilicide composites10.1016/0921-5093(92)90308-N ↗
2. Mechanical behavior of MoSi2 and MoSi2 composites10.1016/0921-5093(94)03246-7 ↗
3. Preparation and characterization of SiC/(Mo, W)Si2 composites from powders resulting from a SHS in a chemical oven10.1016/j.ijrmhm.2008.03.005 ↗
4. Emerging applications of intermetallics10.1016/S0966-9795(00)00077-7 ↗
5. Oxidation of MoSi2-based composites10.1016/0921-5093(92)90325-U ↗
6. Plastic deformation of MoSi2 and WSi2 single crystals and directionally solidified MoSi2-based alloys10.1016/0966-9795(96)00030-1 ↗
7. Synthesis of MoSi2/WSi2 nanocrystalline powder by mechanical-assistant combustion synthesis method10.1016/j.ijrmhm.2009.10.001 ↗
8. Feasibility of a composite of SiC whiskers in an MoSi2 Matrix10.1111/j.1151-2916.1985.tb10182.x ↗
9. ZrO2 and ZrO2-SiC particle reinforced MoSi2 matrix composites10.1016/0921-5093(92)90332-U ↗
10. Creep behavior of SiC whisker-reinforced Si3N4/BN fibrous monolithic ceramics10.1016/S0955-2219(00)00251-X ↗
11. Synthesis and kinetic study of (Mo,W)Si2-WSi2 nanocomposite by mechanical alloying10.1016/j.jallcom.2012.06.072 ↗
12. Growth kinetics of W5Si3 layer in WSi2/W system10.1016/j.surfcoat.2004.02.039 ↗
13. Combustion synthesis of MoSi2-WSi2 alloys10.1016/0921-5093(94)90904-0 ↗
14. Strain-rate dependence of the brittle-to-ductile transition temperature in tungsten10.1080/14786430701253197 ↗
15. (Mo,W)5Si3-(Mo,W)Si2 eutectics: properties and application in composite materials10.1023/A:1024535825077 ↗
16. Processing of molybdenum disilicide10.1007/BF00356804 ↗
17. Reaction synthesis of high-temperature silicides10.1016/0921-5093(94)03284-X ↗
18. An overview of powder processing of silicides and their composites10.1016/S0921-5093(98)01063-6 ↗
19. Combustion synthesis of MoSi2 and MoSi2-Mo5Si3 composites10.1016/j.jallcom.2006.08.033 ↗
20. Degradation mechanism of MoxW1-xSi2 heating elements fabricated by SHS process
21. Isothermal oxidation behaviour of Mo–Si–B and Mo –Si–B–Al alloys in the temperature range of 400-800°C10.1016/j.msea.2006.03.014 ↗
22. Microstructure and oxidation resistance of Mo-Si and Mo-Si-Al alloy coatings prepared by electro-thermal explosion ultrahigh speed spraying10.1016/j.msea.2009.04.026 ↗
23. An experimental study of bonding and crystal structure modifications in MoSi2 and MoSi2+xAl (x=10 to 40 at% Al) via auger parameter shifts and charge transfer calculations10.1016/S1359-6454(00)00383-9 ↗
24. Oxidation behaviour of particle reinforced MoSi2 composites at temperatures up to 1700°C Part II: initial screening of the oxidation behaviour of MoSi2 composites10.1002/maco.200403832 ↗
25. Effect of ball-milling time on the structural characteristics of biomedical porous Ti-Sn-Nb alloy10.1016/j.msec.2011.02.011 ↗
26. German · 1996
27. Effects of ball milling time on microstructure evolution and optical transparency of Nd:YAG ceramics10.1016/j.ceramint.2014.02.076 ↗
28. Nanoparticulate materials densification10.1016/S0965-9773(96)00046-3 ↗
29. Combustion synthesis of advanced materials: Part I. Reaction parameters10.1016/0079-6425(94)00011-5 ↗
30. Effects of ball milling time on the synthesis and consolidation of nanostructured WC-Co composites10.1016/j.ijrmhm.2009.05.006 ↗
31. Effect of ball milling on graphene reinforced Al6061 composite fabricated by semi-solid sintering10.1016/j.compositesb.2013.12.043 ↗
32. Mechanical behavior and interface design of MoSi2-based alloys and composites10.1016/0921-5093(92)90322-R ↗
33. A MoSi2/SiC oxidation protective coating for carbon/carbon composites10.1016/j.corsci.2010.11.024 ↗
34. Oxidation of MoSi2 and comparison with other silicide materials10.1016/0921-5093(92)90324-T ↗
35. “PEST” degradation in beryllides, silicides, aluminides, and related compounds10.1016/0022-3115(64)90142-4 ↗
36. Structure of scale on molybdenum disilicide
37. Characterization of thin film molybdenum silicide oxide10.1149/1.2129832 ↗
38. Oxidation behaviour of particle reinforced MoSi2 composites at temperatures up to 1700°C10.1002/maco.200403833 ↗
39. Materials for temperatures above 1500°C in oxidizing atmospheres Part II: experimental results on the oxidation of MoSi2 composites and coated SiC10.1002/1521-4176(200104)52:4<268::AID-MACO268>3.0.CO;2-C ↗
40. Oxidation of MoSi2-based composites10.1016/0921-5093(92)90325-U ↗
41. High temperature oxidation of ZrC-20% MoSi2 in air for future solar receivers10.1016/j.solmat.2011.03.028 ↗
42. Supersonic plasma sprayed MoSi2-ZrB2 antioxidation coating for SiC-C/C composites10.1179/1743294415Y.0000000098 ↗
43. Mechanism of MoSi2 pest during low temperature oxidation10.1557/JMR.1993.0214 ↗
44. The phenomena of rupture and flow in solids
45. Dependence of ceramic fracture properties on porosity10.1007/BF01159841 ↗
46. Properties of a pressureless-sintered ZrB2-MoSi2 ceramic composite10.1111/j.1551-2916.2006.00999.x ↗
47. Microstructure and mechanical properties of ZrB2-MoSi2 ceramic composites produced by different sintering techniques10.1016/j.msea.2006.06.112 ↗
48. Effects of MoSi2 additions on the properties of Hf- and Zr-B2 composites produced by pressureless sintering10.1016/j.scriptamat.2007.02.040 ↗
49. Fabrication and characterization of TiCw/MoSi2 and SiCw/MoSi2 composites10.1016/S0167-577X(01)00398-6 ↗
50. Creep behavior of MoSi2 and MoSi2 + SiC composite10.1023/B:JMSC.0000031499.17440.17 ↗
51. Fracture and mechanical properties of MoSi2 and MoSi2 + SiC