Interlaminar fracture toughness properties of hybrid glass fiber-reinforced composite interlayered with carbon nanotube using electrospray deposition

Fatin Nur Amirah Mohd Sabri, Muhammad Razlan Zakaria, Hazizan Md Akil, Mohd Shukur Zainol Abidin, Aslina Anjang Ab Rahman, Mohd Firdaus Omar

Nanotechnology Reviews· Volume 10· Issue 1

Abstract

Abstract The electrospray deposition (ESD) method was used to deposit carbon nanotubes (CNTs) onto the surface of glass fiber (GF). The morphology of the hybrid CNTs-GF was analyzed using a field emission scanning electron microscope, and the images indicated that the CNTs were uniformly and homogenously deposited onto the GF’s surface. Laminated composite based on GF and hybrid CNTs-GF were then fabricated via vacuum-assisted resin transfer molding. The mode I interlaminar fracture toughness was measured using the double cantilever beam test method. The hybrid CNTs-GF showed a 34% increase in fracture toughness relative to the control sample. The mechanism of interlaminar fracture toughness enhancement was elucidated via fractography, where fiber bridging, adhesive and cohesive failures, hackles, and coarse matrix surface were observed along the crack pathways.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Carbon Nanotubes in Composites · Diamond and Carbon-based Materials Research · Tribology and Wear Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials and Mineral Resources Engineering, Engineering Campus, Universiti Sains Malaysia , 14300 Nibong Tebal , Pulau Pinang , Malaysia

School of Aerospace Engineering, Engineering Campus, Universiti Sains Malaysia , 14300 Nibong Tebal , Pulau Pinang , Malaysia

Faculty of Chemical Engineering Technology, Universiti Malaysia Perlis (UniMAP) , Perlis , Malaysia

References (39)

Show source-provided references
1. Fan Z, Santare MH, Advani SG. Interlaminar shear strength of glass fiber reinforced epoxy composites enhanced with multi-walled carbon nanotubes. Compos A Appl Sci Manuf. 2008;39(3):540–54.10.1016/j.compositesa.2007.11.013 ↗
2. Mirjalili V, Ramachandramoorthy R, Hubert P. Enhancement of fracture toughness of carbon fiber laminated composites using multi wall carbon nanotubes. Carbon. 2014;79(1):413–23. 10.1016/j.carbon.2014.07.084.10.1016/j.carbon.2014.07.084 ↗
3. Blake SP, Berube KA, Lopez-Anido RA. Interlaminar fracture toughness of woven E-glass fabric composites. J Composite Mater. 2012;46(13):1583–92.10.1177/0021998311421221 ↗
4. Wang B, Gao H. Fibre reinforced polymer composites. Cham: Springer; 2021. p. 15–43.10.1007/978-3-030-71438-3_2 ↗
5. Eskizeybek V, Avci A, Gülce A. The Mode I interlaminar fracture toughness of chemically carbon nanotube grafted glass fabric/epoxy multi-scale composite structures. Compos A. 2014;63:94–102.10.1016/j.compositesa.2014.04.013 ↗
6. Shindo Y, Takeda T, Narita F, Saito N, Watanabe S, Sanada K. Delamination growth mechanisms in woven glass fiber reinforced polymer composites under Mode II fatigue loading at cryogenic temperatures. Compos Sci Technol. 2009;69(11–12):1904–11. 10.1016/j.compscitech.2009.04.010.10.1016/j.compscitech.2009.04.010 ↗
7. Nasuha N, Azmi AI, Tan CL. A review on mode-I interlaminar fracture toughness of fibre reinforced composites. J Physics Conf Ser. 2017;908(1):012024.10.1088/1742-6596/908/1/012024 ↗
8. Cui K, Zhang Y, Fu T, Wang J, Zhang X. Toughening mechanism of mullite matrix composites: a review. Coatings. 2020;10:7672.10.3390/coatings10070672 ↗
9. Aghamohammadi H, Eslami-Farsani R, Tcharkhtchi A. The effect of multi-walled carbon nanotubes on the mechanical behavior of basalt fibers metal laminates: an experimental study. Int J Adhes Adhesives. 2020;98:102538. 10.1016/j.ijadhadh.2019.102538.10.1016/j.ijadhadh.2019.102538 ↗
10. Fanteria D, Lazzeri L, Panettieri E, Mariani U, Rigamonti M. Experimental characterization of the interlaminar fracture toughness of a woven and a unidirectional carbon/epoxy composite. Compos Sci Technol. 2017;142:20–9. 10.1016/j.compscitech.2017.01.028.10.1016/j.compscitech.2017.01.028 ↗
11. Shrivastava R, Singh KK. Interlaminar fracture toughness characterization of laminated composites: a review. Polym Rev. 2019;7(6):1020–45. 10.1080/15583724.2019.1677708.
12. Borowski E, Soliman E, Kandil UF, Taha MR. Interlaminar fracture toughness of CFRP laminates incorporating multi-walled carbon nanotubes. Polymers. 2015;7(6):1020–45.10.3390/polym7061020 ↗
13. Barathi Dassan EG, Anjang Ab Rahman A, Abidin MSZ, Akil HM. Carbon nanotube-reinforced polymer composite for electromagnetic interference application: a review. Nanotechnol Rev. 2020;9(1):768–88.10.1515/ntrev-2020-0064 ↗
14. Chaudhry MS, Czekanski A, Zhu ZH. Characterization of carbon nanotube enhanced interlaminar fracture toughness of woven carbon fiber reinforced polymer composites. Int J Mech Sci. 2017;131–132:480–9.10.1016/j.ijmecsci.2017.06.016 ↗
15. Khan SU, Kim J. Impact and delamination failure of multiscale carbon nanotube-fiber reinforced. Polym Composites: A Rev. 2011;12(2):115–33.10.5139/IJASS.2011.12.2.115 ↗
16. Srivastava AK, Kumar D. Postbuckling behavior of functionally graded CNT-reinforced nanocomposite plate with interphase effect. Nonlinear Eng. 2019;8(1):496–512.10.1515/nleng-2017-0133 ↗
17. Kośla K, Olejnik M, Olszewska K. Preparation and properties of composite materials containing graphene structures and their applicability in personal protective equipment: a review. Rev Adv Mater Sci. 2020;59(1):215–42.10.1515/rams-2020-0025 ↗
18. Kharissova VasilievnaO, Kharisov BI. In solubilization and dispersion of carbon nanotubes. Cham, Switzerland AG: Springer; 2017. p. 33–148.10.1007/978-3-319-62950-6_3 ↗
19. Hashim H, Salleh MS, Omar MZ. Homogenous dispersion and interfacial bonding of carbon nanotube reinforced with aluminum matrix composite: a review. Rev Adv Mater Sci. 2019;58(1):295–303.10.1515/rams-2019-0035 ↗
20. Zhang H, Kuwata M, Bilotti E, Peijs T. Integrated damage sensing in fibre-reinforced composites with extremely low carbon nanotube loadings. J Nanomaterials. 2015;2015(3):1–7.10.1155/2015/785834 ↗
21. Zakaria MR, Akil HM, Omar MF, Abdullah MMAB, Rahman AAA, Othman MBH. Improving flexural and dielectric properties of carbon fiber epoxy composite laminates reinforced with carbon nanotubes interlayer using electrospray deposition. Nanotechnol Rev. 2020;9(1):1170–82.10.1515/ntrev-2020-0090 ↗
22. An Q, Rider AN, Thostenson ET. Hierarchical composite structures prepared by electrophoretic deposition of carbon nanotubes onto glass fibers. ACS Appl Mater Interfaces. 2013;5(6):2022–32.10.1021/am3028734 ↗
23. Demircan Ö, Çolak P, Kadıoğlu K, Günaydın E. Flexural properties of glass fiber/epoxy/MWCNT composites. Res Eng Struct Mater. 2019;5(2):91–8.
24. Haghbin A, Liaghat G, Hadavinia H, Arabi AM, Pol MH. Enhancement of the electrical conductivity and interlaminar shear strength of CNT/GFRP hierarchical composite using an electrophoretic deposition technique. Materials. 2017;10(10):1120.10.3390/ma10101120 ↗
25. Rodriguez AJ, Guzman ME, Lim CS, Minaie B. Mechanical properties of carbon nanofiber/fiber-reinforced hierarchical polymer composites manufactured with multiscale-reinforcement fabrics. Carbon. 2011;49(3):937–48. 10.1016/j.carbon.2010.10.057.10.1016/j.carbon.2010.10.057 ↗
26. Li Q, Church JS, Naebe M, Fox BL. A systematic investigation into a novel method for preparing carbon fibre–carbon nanotube hybrid structures. Compos A Appl Sci Manuf. 2016;90:174–85. 10.1016/j.compositesa.2016.05.004.10.1016/j.compositesa.2016.05.004 ↗
27. Zakaria MR, Md Akil H, Omar MF, Abdul Kudus MH, Mohd Sabri FNA, Abdullah MMAB. Enhancement of mechanical and thermal properties of carbon fiber epoxy composite laminates reinforced with carbon nanotubes interlayer using electrospray deposition. Compos C Open Access. 2020;3:100075.10.1016/j.jcomc.2020.100075 ↗
28. Vieille B, Casado VM, Bouvet C. About the impact behavior of woven-ply carbon fiber-reinforced thermoplastic- and thermosetting-composites: a comparative study. Compos Struct. 2013;101:9–21. 10.1016/j.compstruct.2013.01.025.10.1016/j.compstruct.2013.01.025 ↗
29. Mansour R. Mode I. Interlaminar fracture properties of oxide and non-oxide ceramic matrix composites [Internet]; 2017 [cited 2020 Nov 25]. Available from: http://rave.ohiolink.edu/etdc/view? acc_num=akron1494248628194216
30. Khan R. Fiber bridging in composite laminates: a literature review. Compos Struct. 2019;229:111418.10.1016/j.compstruct.2019.111418 ↗
31. Pinto MA, Chalivendra VB, Kim YK, Lewis AF. Effect of surface treatment and Z-axis reinforcement on the interlaminar fracture of jute/epoxy laminated composites. Eng Fract Mech. 2013;114:104–14.10.1016/j.engfracmech.2013.10.015 ↗
32. Perrin F, Bureau MN, Denault J, Dickson JI. Mode I interlaminar crack propagation in continuous glass fiber/polypropylene composites: Temperature and molding condition dependence. Compos Sci Technol. 2003;63(5):597–607.10.1016/S0266-3538(02)00255-5 ↗
33. Zhang H, Liu Y, Kuwata M, Bilotti E, Peijs T. Improved fracture toughness and integrated damage sensing capability by spray coated CNTs on carbon fibre prepreg. Compos A. 2015;70:102–10. 10.1016/j.compositesa.2014.11.029.10.1016/j.compositesa.2014.11.029 ↗
34. Warrier A, Godara A, Rochez O, Mezzo L, Luizi F, Gorbatikh L, et al. The effect of adding carbon nanotubes to glass/epoxy composites in the fibre sizing and/or the matrix. Compos A Appl Sci Manuf. 2010;41(4):532–8. 10.1016/j.compositesa.2010.01.001.10.1016/j.compositesa.2010.01.001 ↗
35. Tsantzalis S, Karapappas P, Vavouliotis A, Tsotra P, Kostopoulos V, Tanimoto T, et al. On the improvement of toughness of CFRPs with resin doped with CNF and PZT particles. Compos A Appl Sci Manuf. 2007;38(4):1159–62.10.1016/j.compositesa.2006.04.016 ↗
36. Khosravi H, Eslami-Farsani R. Reinforcing effect of surface-modified multiwalled carbon nanotubes on flexural response of E-glass/epoxy isogrid-stiffened composite panels. Polym Compos. 2018;39:E677–86.10.1002/pc.24118 ↗
37. Keshavarz R, Aghamohammadi H, Eslami-Farsani R. The effect of graphene nanoplatelets on the flexural properties of fiber metal laminates under marine environmental conditions. Int J Adhes Adhesives. 2020;103:102709. 10.1016/j.ijadhadh.2020.102709.10.1016/j.ijadhadh.2020.102709 ↗
38. Blackman B, Kinloch A. Fracture tests on structural adhesive joints. European Structural Integrity Society. Kidlington, Oxford, UK: Elsevier; 2001. p. 225–67.10.1016/S1566-1369(01)80036-4 ↗
39. Bonhomme J, Argüelles A, Viña J, Viña I. Fractography and failure mechanisms in static mode I and mode II delamination testing of unidirectional carbon reinforced composites. Polym Test. 2009;28(6):612–7.10.1016/j.polymertesting.2009.05.003 ↗