journal article·2023-10

Nanograin formation mechanism under fatigue loadings in additively manufactured Ti-6Al-4V alloy

Weiqian Chi, Wenjing Wang, Lei Wu, Guihua Duan, Chengqi Sun

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Surface Treatment and Residual Stress

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Additive manufacturing of structural materials10.1016/j.mser.2020.100596 ↗
2. Progress and perspectives in laser additive manufacturing of key aeroengine materials10.1016/j.ijmachtools.2021.103804 ↗
3. Ultrasonic fatigue of laser beam powder bed fused metals: a state-of-the-art review10.1016/j.engfailanal.2021.106015 ↗
4. Fatigue of additive manufactured Ti-6Al-4V, Part II: The relationship between microstructure, material cyclic properties, and component performance10.1016/j.ijfatigue.2019.105363 ↗
5. Characteristic and mechanism of crack initiation and early growth of an additively manufactured Ti-6Al-4V in very high cycle fatigue regime10.1016/j.ijmecsci.2021.106591 ↗
6. Investigation of the mechanisms by which hot isostatic pressing improves the fatigue performance of powder bed fused Ti-6Al-4V10.1016/j.ijfatigue.2018.10.015 ↗
7. Significance of hot isostatic pressing (HIP) on multiaxial deformation and fatigue behaviors of additive manufactured Ti-6Al-4V including build orientation and surface roughness effects10.1016/j.ijfatigue.2018.07.035 ↗
8. Effects of post-processing on cyclic fatigue response of a titanium alloy additively manufactured by electron beam melting10.1016/j.msea.2016.10.059 ↗
9. The nature and the mechanism of crack initiation and early growth for very-high-cycle fatigue of metallic materials - an overview10.1016/j.tafmec.2017.05.002 ↗
10. Interior initiation and early growth of very high cycle fatigue crack in an additively manufactured Ti-alloy10.1016/j.ijfatigue.2022.106862 ↗
11. Slip and fatigue crack formation processes in an α/β titanium alloy in relation to crystallographic texture on different scales10.1016/j.actamat.2008.04.036 ↗
12. The effects of crystallographic orientation on fatigue crack initiation behavior in Ti-6Al-4V10.1016/j.ijfatigue.2018.07.039 ↗
13. Multi-dimensional study of the effect of early slip activity on fatigue crack initiation in a near-a titanium alloy10.1016/j.actamat.2022.117967 ↗
14. Nanograin formation in dimple ridges due to local severe-plastic-deformation during ductile fracture10.1016/j.scriptamat.2020.113631 ↗
15. Formation mechanism of the distinctive granular fracture surface in subsurface fracture of Ti6Al4V alloy10.1016/j.mtla.2021.101312 ↗
16. Mechanism of subsurface microstructural fatigue crack initiation during high and very-high cycle fatigue of advanced bainitic steels10.1016/j.jmst.2021.08.060 ↗
17. Fatigue life and mechanistic modeling of interior micro-defect induced cracking in high cycle and very high cycle regimes10.1016/j.actamat.2018.07.036 ↗
18. Nanograin formation and cracking mechanism in Ti alloys under very high cycle fatigue loading10.1016/j.ijfatigue.2022.107331 ↗
19. Role of deformation twinning in fatigue of CrCoNi medium-entropy alloy at room temperature10.1016/j.scriptamat.2021.113985 ↗
20. Influence of grain size and grain boundary misorientation on the fatigue crack initiation mechanisms of textured AZ31 Mg alloy10.1016/j.scriptamat.2021.114304 ↗
21. Defect induced cracking and modeling of fatigue strength for an additively manufactured Ti-6Al-4V alloy in very high cycle fatigue regime10.1016/j.tafmec.2022.103380 ↗
22. A method for predicting the effects of specimen geometry and loading condition on fatigue strength10.3390/met8100811 ↗
23. Fatigue damage in copper polycrystals subjected to ultrahigh-cycle fatigue below the PSB threshold10.1016/j.ijfatigue.2009.04.004 ↗
24. Evolution of twinning and shear bands in magnesium alloys during rolling at room and cryogenic temperature10.1016/j.matdes.2020.108793 ↗
25. Deformation twinning activity and twin structure development of pure titanium at cryogenic temperature10.1016/j.msea.2018.09.091 ↗
26. Mechanism of artificial surface defect induced cracking for very high cycle fatigue of Ti alloys10.1016/j.engfracmech.2022.108721 ↗
27. Dislocation interactions with grain boundaries10.1016/j.cossms.2014.05.004 ↗
28. Twin nucleation by slip transfer across grain boundaries in commercial purity titanium10.1007/s11661-009-0097-6 ↗
29. A systematic study of hcp crystal orientation and morphology effects in polycrystal deformation and fatigue
30. Microstructure and texture evolution in a post-dynamic recrystallized titanium during annealing, monotonic and cyclic loading10.1007/s11661-020-06071-x ↗
31. An investigation of surface nanocrystallization mechanism in Fe induced by surface mechanical attrition treatment10.1016/S1359-6454(02)00310-5 ↗
32. Nanostructure formation mechanism of α-titanium using SMAT10.1016/j.actamat.2004.05.023 ↗
33. Dynamic continuous recrystallization characteristics in two stage deformation of Mg–3Al–1Zn alloy sheet10.1016/S0921-5093(02)00096-5 ↗
34. Analysis of deformation mechanisms operating under fatigue and dwell-fatigue loadings in an α/β titanium alloy10.1016/j.ijfatigue.2019.105341 ↗
35. The evolution of local stress during deformation twinning in a Mg-Gd-Y-Zn alloy10.1016/j.actamat.2021.117452 ↗
36. Concurrent operation of 〈c + a〉 slip and twinning under cyclic loading of Ti-6Al-4V10.1016/j.scriptamat.2018.07.033 ↗
37. Structural characterization of the 112¯2 twin boundary and the corresponding stress accommodation mechanisms in pure titanium10.1016/j.jmst.2020.07.030 ↗
38. Interface structures and twinning mechanisms of twins in hexagonal metals10.1080/21663831.2017.1336496 ↗
39. Serrated and stepped-like twin boundary of nano-sized extension twin in a deformed magnesium alloy10.1016/j.matlet.2018.11.008 ↗
40. Deformation twinning in hexagonal materials10.1557/mrs.2016.64 ↗
41. The dislocation-twin interaction and evolution of twin boundary in AZ31 Mg alloy10.1016/j.actamat.2017.05.034 ↗
42. Direct observation of dual-step twinning nucleation in hexagonal close-packed crystals10.1038/s41467-020-16351-0 ↗
43. Two types of basal stacking faults within 101¯2 twin in deformed magnesium alloy10.1016/j.matlet.2016.09.019 ↗
44. Slip, twinning, and fracture in hexagonal close-packed metals10.1007/BF02648537 ↗
45. On the mechanistic basis of deformation at the microscale in hexagonal close-packed metals
46. Deformation twinning in h.c.p. metals and alloys10.1080/01418619108213931 ↗
47. Williams DB, Barry C. Carter. Transmission electron microscopy: a textbook for materials science; 2009.10.1007/978-0-387-76501-3 ↗
48. Experimental observations of the mechanisms associated with the high hardening and low strain to failure of magnesium10.1016/j.mtla.2019.100504 ↗
49. Loading direction dependence of asymmetric response of pyramidal slip in rolled AZ31 magnesium alloy
50. An in situ transmission electron microscopy study of interface growth during martensitic transformation in an Fe–Ni–Mn alloy10.1016/j.actamat.2011.02.003 ↗
51. High cycle and very high cycle fatigue of TC17 titanium alloy: stress ratio effect and fatigue strength modeling10.1016/j.ijfatigue.2022.107299 ↗
52. High-temperature failure mechanism and defect sensitivity of TC17 titanium alloy in high cycle fatigue10.1016/j.jmst.2022.01.010 ↗
53. Effects of specimen geometry and surface defect on high and very high cycle fatigue of TC17 alloy10.1016/j.engfracmech.2022.108940 ↗
54. The mechanism of internal fatigue-crack initiation and early growth in a titanium alloy with lamellar and equiaxed microstructure10.1016/j.msea.2020.140110 ↗
55. Crack initiation mechanism and fatigue life of titanium alloy Ti–6Al–2Sn–2Zr–3Mo-X: Effects of stress ratio and loading frequency10.1016/j.msea.2020.140265 ↗
56. Effect of grain size on the very high cycle fatigue behavior and notch sensitivity of titanium10.1016/j.tafmec.2019.102362 ↗
57. Mechanism of fatigue crack initiation and propagation in the very high cycle fatigue regime of high-strength steels10.1016/j.scriptamat.2012.07.049 ↗
58. The formation of discontinuous gradient regimes during crack initiation in high strength steels under very high cycle fatigue10.1016/j.ijfatigue.2019.03.026 ↗
59. A general scenario of fish-eye crack initiation on the life of high-strength steels in the very high-cycle fatigue regime10.1111/ffe.13104 ↗
60. Fatigue limit and crack growth in ultra-fine grain metals produced by severe plastic deformation10.1007/s10853-006-0973-z ↗