Abstract

Selective laser melting (SLM) has provided an alternative to the conventional fabrication techniques for Ti-6Al-4V alloy parts because of its flexibility and ease in creating complex features. Therefore, this study investigated the effects of the process parameters and heat treatment on the microstructure and mechanical properties of Ti-6Al-4V fabricated using SLM. The influences of various process parameters on the relative density, tensile properties, impact toughness, and hardness of Ti-6Al-4V alloy parts were studied. By employing parameter optimization, a high-density high-strength Ti-6Al-4V alloy was fabricated by SLM. A relative density of 99.45%, a tensile strength of 1 188 MPa, and an elongation to failure of 9.5% were achieved for the SLM-fabricated Ti-6Al-4V alloy with optimized parameters. The effects of annealing and solution aging heat treatment on the mechanical properties, phase composition, and microstructure of the SLM-fabricated Ti-6Al-4V alloy were also studied. The ductility of the heat-treated Ti-6Al-4V alloy was improved. By applying a heat treatment at 850 °C for 2 h, followed by furnace cooling, the elongation to failure and impact toughness were found to be increased from 9.5% to 12.5%, and from 24.13 J/cm2 to 47.51 J/cm2, respectively.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. Cai J, Li F, Liu T et al (2011) Constitutive equations for elevated temperature flow stress of Ti-6Al-4V alloy considering the effect of strain. Mater Design 32:1144–115110.1016/j.matdes.2010.11.004 ↗
2. Leuders S, Thöne M, Riemer A et al (2013) On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance. Int J Fatigue 48:300–30710.1016/j.ijfatigue.2012.11.011 ↗
3. Ming W, Chen J, An Q et al (2019) Dynamic mechanical properties and machinability characteristics of selective laser melted and forged Ti6Al4V. J Mater Process Technol 271:284–29210.1016/j.jmatprotec.2019.04.015 ↗
4. Vandenbroucke B, Kruth JP (2007) Selective laser melting of biocompatible metals for rapid manufacturing of medical parts. Rapid Prototyping J 13:196–20310.1108/13552540710776142 ↗
5. Liu J, Sun Q, Zhou C et al (2019) Achieving Ti6Al4V alloys with both high strength and ductility via selective laser melting. Mat Sci Eng A 766:138319. https://doi.org/10.1016/j.msea.2019.13831910.1016/j.msea.2019.138319 ↗
6. Waqar S, Sun Q, Liu J et al (2020) Numerical investigation of thermal behavior and melt pool morphology in multi-track multi-layer selective laser melting of the 316L steel. Int J Adv Manuf Tech 112(3/4):879–895
7. Rao H, Giet S, Yang K et al (2016) The influence of processing parameters on aluminium alloy A357 manufactured by selective laser melting. Mater Design 109:334–34610.1016/j.matdes.2016.07.009 ↗
8. Gockel J, Sheridan L, Koerper B et al (2019) The influence of additive manufacturing processing parameters on surface roughness and fatigue life. Int J Fatigue 124:380–38810.1016/j.ijfatigue.2019.03.025 ↗
9. Wang Z, Xiao Z, Tse Y et al (2019) Optimization of processing parameters and establishment of a relationship between microstructure and mechanical properties of SLM titanium alloy. Opt Laser Technol 112:159–16710.1016/j.optlastec.2018.11.014 ↗
10. Kasperovich G, Haubrich J, Gussone J et al (2016) Correlation between porosity and processing parameters in TiAl6V4 produced by selective laser melting. Mater Design 105:160–17010.1016/j.matdes.2016.05.070 ↗
11. Wang X, Yu J, Liu J et al (2020) Effect of process parameters on the phase transformation behavior and tensile properties of NiTi shape memory alloys fabricated by selective laser melting. Addit Manuf 36:101545. https://doi.org/10.1016/j.addma.2020.10154510.1016/j.addma.2020.101545 ↗
12. Bidare P, Jiménez A, Hassanin H et al (2021) Porosity, cracks, and mechanical properties of additively manufactured tooling alloys: a review. Adv Manuf. https://doi.org/10.1007/s40436-021-00365-y10.1007/s40436-021-00365-y ↗
13. Pegues JW, Shao S, Shamsaei N et al (2020) Fatigue of additive manufactured Ti-6Al-4V, Part I: The effects of powder feedstock, manufacturing, and post-process conditions on the resulting microstructure and defects. Int J Fatigue 132:105358. https://doi.org/10.1016/j.ijfatigue.2019.10535810.1016/j.ijfatigue.2019.105358 ↗
14. Dilip JJS, Zhang S, Teng C et al (2017) Influence of processing parameters on the evolution of melt pool, porosity, and microstructures in Ti-6Al-4V alloy parts fabricated by selective laser melting. Prog Addit Manuf 2:157–16710.1007/s40964-017-0030-2 ↗
15. Cunningham R, Zhao C, Parab N et al (2019) Keyhole threshold and morphology in laser melting revealed by ultrahigh-speed X-ray imaging. Science 363:849–85210.1126/science.aav4687 ↗
16. Zhao C, Parab ND, Li X et al (2020) Critical instability at moving keyhole tip generates porosity in laser melting. Science 370:1080–108610.1126/science.abd1587 ↗
17. Pal S, Gubeljak N, Hudak R et al (2019) Tensile properties of selective laser melting products affected by building orientation and energy density. Mat Sci Eng A 743:637–64710.1016/j.msea.2018.11.130 ↗
18. Simonelli M, Tse YY, Tuck C (2014) Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti-6Al-4V. Mat Sci Eng A 616:1–1110.1016/j.msea.2014.07.086 ↗
19. Gupta MK, Singla AK, Ji H et al (2020) Impact of layer rotation on micro-structure, grain size, surface integrity and mechanical behaviour of SLM Al-Si-10Mg alloy. J Mater Res Technol 9:9506–952210.1016/j.jmrt.2020.06.090 ↗
20. Ma M, Wang Z, Zeng X (2015) Effect of energy input on microstructural evolution of direct laser fabricated IN718 alloy. Mater Charact 106:420–42710.1016/j.matchar.2015.06.027 ↗
21. Ali H, Ma L, Ghadbeigi H et al (2017) In-situ residual stress reduction, martensitic decomposition and mechanical properties enhancement through high temperature powder bed pre-heating of selective laser melted Ti6Al4V. Mat Sci Eng A 695:211–22010.1016/j.msea.2017.04.033 ↗
22. He B, Wu W, Zhang L et al (2018) Microstructural characteristic and mechanical property of Ti6Al4V alloy fabricated by selective laser melting. Vacuum 150:79–8310.1016/j.vacuum.2018.01.026 ↗
23. Leon A, Katarivas LG, Ron T et al (2020) The effect of strain rate on stress corrosion performance of Ti6Al4V alloy produced by additive manufacturing process. J Mater Res Technol 9:4097–410510.1016/j.jmrt.2020.02.035 ↗
24. Xu W, Sun S, Elambasseril J et al (2015) Ti-6Al-4V additively manufactured by selective laser melting with superior mechanical properties. JOM 67:668–67310.1007/s11837-015-1297-8 ↗
25. Waqar S, Liu J, Sun Q et al (2020) Effect of post-heat treatment cooling on microstructure and mechanical properties of selective laser melting manufactured austenitic 316L stainless steel. Rapid Prototyp J 26:1739–174910.1108/RPJ-12-2019-0320 ↗
26. Cabrini M, Lorenzi S, Pastore T et al (2016) Effect of heat treatment on corrosion resistance of DMLS AlSi10Mg alloy. Electrochim Acta 206:346–35510.1016/j.electacta.2016.04.157 ↗
27. Ju J, Li J, Yang C et al (2021) Evolution of the microstructure and optimization of the tensile properties of the Ti-6Al-4V alloy by selective laser melting and heat treatment. Mat Sci Eng A 802:140673. https://doi.org/10.1016/j.msea.2020.14067310.1016/j.msea.2020.140673 ↗
28. Frkan M, Konecna R, Nicoletto G et al (2019) Microstructure and fatigue performance of SLM-fabricated Ti6Al4V alloy after different stress-relief heat treatments. Transport Res Procedia 40:24–2910.1016/j.trpro.2019.07.005 ↗
29. Lu Y, Wu S, Gan Y et al (2016) Microstructure, mechanical property and metal release of As-SLM CoCrW alloy under different solution treatment conditions. J Mech Behav Biomed Mater 55:179–19010.1016/j.jmbbm.2015.10.019 ↗
30. Vrancken B, Thijs L, Kruth J et al (2012) Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties. J Alloy Compd 541:177–18510.1016/j.jallcom.2012.07.022 ↗
31. Liang Z, Sun Z, Zhang W et al (2019) The effect of heat treatment on microstructure evolution and tensile properties of selective laser melted Ti6Al4V alloy. J Alloy Compd 782:1041–104810.1016/j.jallcom.2018.12.051 ↗
32. DebRoy T, Wei HL, Zuback JS et al (2018) Additive manufacturing of metallic components: process, structure and properties. Prog Mater Sci 92:112–22410.1016/j.pmatsci.2017.10.001 ↗
33. Singla AK, Banerjee M, Sharma A et al (2021) Selective laser melting of Ti6Al4V alloy: process parameters, defects and post-treatments. J Manuf Process 64:161–18710.1016/j.jmapro.2021.01.009 ↗
34. Jin N, Yan Z, Wang Y et al (2021) Effects of heat treatment on microstructure and mechanical properties of selective laser melted Ti-6Al-4V lattice materials. Int J Mech Sci 190:10604210.1016/j.ijmecsci.2020.106042 ↗
35. Wu M, Lai P, Chen J (2016) Anisotropy in the impact toughness of selective laser melted Ti-6Al-4V alloy. Mat Sci Eng A 650:295–29910.1016/j.msea.2015.10.045 ↗
36. Wu M, Lai P (2016) The positive effect of hot isostatic pressing on improving the anisotropies of bending and impact properties in selective laser melted Ti-6Al-4V alloy. Mat Sci Eng A 658:429–43810.1016/j.msea.2016.02.023 ↗
37. Yan X, Yin S, Chen C et al (2018) Effect of heat treatment on the phase transformation and mechanical properties of Ti6Al4V fabricated by selective laser melting. J Alloy Compd 764:1056–107110.1016/j.jallcom.2018.06.076 ↗
38. Gong H, Rafi K, Gu H et al (2015) Influence of defects on mechanical properties of Ti-6Al-4V components produced by selective laser melting and electron beam melting. Mater Design 86:545–55410.1016/j.matdes.2015.07.147 ↗
39. Han L, Che S (2018) An overview of materials with triply periodic minimal surfaces and related geometry: from biological structures to self-assembled systems. Adv Mater 30:1705708. https://doi.org/10.1002/adma.20170570810.1002/adma.201705708 ↗
40. Heeling T, Cloots M, Wegener K (2017) Melt pool simulation for the evaluation of process parameters in selective laser melting. Addit Manuf 14:116–125
41. Tan P, Shen F, Li B et al (2019) A thermo-metallurgical-mechanical model for selective laser melting of Ti6Al4V. Mater Design 168:107642. https://doi.org/10.1016/j.matdes.2019.10764210.1016/j.matdes.2019.107642 ↗
42. Shipley H, McDonnell D, Culleton M et al (2018) Optimisation of process parameters to address fundamental challenges during selective laser melting of Ti-6Al-4V: a review. Int J Mach Tool Manu 128:1–2010.1016/j.ijmachtools.2018.01.003 ↗
43. Xu Y, Lu Y, Sundberg KL et al (2017) Effect of annealing treatments on the microstructure, mechanical properties and corrosion behavior of direct metal laser sintered Ti-6Al-4V. J Mater Eng Perform 26:2572–258210.1007/s11665-017-2710-y ↗
44. Toptan F, Alves AC, Carvalho Ó et al (2019) Corrosion and tribocorrosion behaviour of Ti6Al4V produced by selective laser melting and hot pressing in comparison with the commercial alloy. J Mater Process Tech 266:239–24510.1016/j.jmatprotec.2018.11.008 ↗
45. Sing SL, Yeong WY, Wiria FE (2016) Selective laser melting of titanium alloy with 50 wt% tantalum: microstructure and mechanical properties. J Alloy Compd 660:461–47010.1016/j.jallcom.2015.11.141 ↗
46. Liu YJ, Li SJ, Wang HL et al (2016) Microstructure, defects and mechanical behavior of beta-type titanium porous structures manufactured by electron beam melting and selective laser melting. Acta Mater 113:56–6710.1016/j.actamat.2016.04.029 ↗
47. Liu Y, Yang Y, Mai S et al (2015) Investigation into spatter behavior during selective laser melting of AISI 316L stainless steel powder. Mater Design 87:797–80610.1016/j.matdes.2015.08.086 ↗
48. Rabadia CD, Liu YJ, Cao GH et al (2018) High-strength β stabilized Ti-Nb-Fe-Cr alloys with large plasticity. Mat Sci Eng A 732:368–77710.1016/j.msea.2018.07.031 ↗
49. Liu C, Qin J, Feng Z et al (2018) Improving the microstructure and mechanical properties of Zr-Ti alloy by nickel addition. J Alloy Compd 737:405–41110.1016/j.jallcom.2017.12.046 ↗
50. Donnadieu P, Pohlmann C, Scudino S et al (2014) Deformation at ambient and high temperature of in situ Laves phases-ferrite composites. Sci Technol Adv Mater 15:34801. https://doi.org/10.1088/1468-6996/15/3/03480110.1088/1468-6996/15/3/034801 ↗
51. Waqar S, Guo K, Sun J (2021) FEM analysis of thermal and residual stress profile in selective laser melting of 316L stainless steel. J Manuf Process 66:81–10010.1016/j.jmapro.2021.03.040 ↗
52. Khorasani A, Gibson I, Awan US et al (2019) The effect of SLM process parameters on density, hardness, tensile strength and surface quality of Ti-6Al-4V. Addit Manuf 25:176–186
53. Zhan Y, Xu H, Du W et al (2021) Research on the influence of heat treatment on residual stress of TC4 alloy produced by laser additive manufacturing based on laser ultrasonic technique. Ultrasonics 115:106466. https://doi.org/10.1016/j.ultras.2021.10646610.1016/j.ultras.2021.106466 ↗
54. Yan X, Shi C, Liu T et al (2020) Effect of heat treatment on the corrosion resistance behavior of selective laser melted Ti6Al4V ELI. Surf Coat Tech 396:125955. https://doi.org/10.1016/j.surfcoat.2020.12595510.1016/j.surfcoat.2020.125955 ↗
55. Liu L, Ding Q, Zhong Y et al (2018) Dislocation network in additive manufactured steel breaks strength-ductility trade-off. Mater Today 21:354–36110.1016/j.mattod.2017.11.004 ↗