journal article·2024-12

Effect of heat treatment on microstructure, mechanical properties and corrosion resistance of 7075 aluminum alloys fabricated by improved friction stir additive manufacturing

Ji Liu, Yugang Miao, Ruizhi Wu, Chao Wei, Yuyang Zhao, Yifan Wu, Qingwen Deng

Publisher page

Abstract

The use of an improved stirrng pin broadened the effective bonding area in the friction stir additive manufacturing (FSAM) of 7075 aluminum alloy. A systematic investigation was conducted to examine the effects of different heat treatment (T6, T73, and RRA) processes on the microstructure, tensile strength and corrosion resistance of as-fabricated (AS) specimen. The findings revealed that different heat treatments had minimal impact on the grain size, texture strength, and dislocation density. Variations in strength and corrosion resistance were primarily attributed to the size and distribution of precipitates. Following T6 heat treatment, the intragranular precipitates (IGPs) were smaller, with a higher proportion of η`, while the grain boundary precipitates (GBPs) were coarser η, continuously distributed along grain boundaries. Consequently, T6 specimen showed the highest tensile strength, reaching 568 MPa, but had lower corrosion resistance than AS specimen due to precipitate-induced disruption of the passive film. The T73 heat treatment resulted in significant coarsening of IGPs, with a substantial transformation of η` to η, thereby reducing the precipitation strengthening effect. The coarsening of GBPs led to their discontinuous distribution along grain boundaries, which significantly increased the corrosion resistance. After RRA heat treatment, IGPs consisted of numerous fine η`, while the coarser GBPs sporadically dispersed along grain boundaries. The strength of RRA specimen was only about 6 % lower than that of T6 specimen, but its corrosion resistance was significantly improved.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloys Composites Properties · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Multi-objective optimization of friction stir additively manufactured Al-7075 multi-layered laminates10.1016/j.jallcom.2024.174659 ↗
2. Improved interfacial strength in bimetallic additive manufacturing of aluminum bronze/steel by controlling interface melting10.1016/j.jmapro.2024.05.052 ↗
3. Big data, machine learning, and digital twin assisted additive manufacturing: a review10.1016/j.matdes.2024.113086 ↗
4. Characterization of microstructure and local mechanical properties of friction rolling additive manufactured Al–Li alloy under repeated thermal–mechanical cycles10.1016/j.matchar.2023.113169 ↗
5. A review of the wire arc additive manufacturing of metals: properties, defects and quality improvement10.1016/j.jmapro.2018.08.001 ↗
6. The influence of multi-scale second-phase particles on micro-crack initiation and propagation in Al–Zn–Mg–Cu alloy10.1016/j.vacuum.2024.113044 ↗
7. Review of recent trends and developments in aluminium 7075 alloy and its metal matrix composites (MMCs) for aircraft applications10.1016/j.rineng.2023.101372 ↗
8. Welding and additive manufacturing with nanoparticle-enhanced aluminum 7075 wire10.1016/j.jallcom.2020.154987 ↗
9. Enhanced high-temperature mechanical properties of laser-arc hybrid additive manufacturing of Al-Zn-Mg-Cu alloy via microstructure control10.1016/j.jmst.2023.05.071 ↗
10. Additive manufacturing ( 3D printing): a review of materials, methods, applications and challenges10.1016/j.compositesb.2018.02.012 ↗
11. Potentials and strategies of solid-state additive friction-stir manufacturing technology: a critical review10.1016/j.jmapro.2018.09.030 ↗
12. Experimental and numerical analysis of friction stir additive manufacturing of 2024 aluminium alloy
13. Microstructure evolution and mechanical properties of 2060 Al-Li alloy via friction stir additive manufacturing10.1016/j.jallcom.2022.168019 ↗
14. Microstructure evolution and mechanical properties of ultrafine-grained Al–Li alloy fabricated via friction stir additive manufacturing10.1016/j.matchar.2024.113760 ↗
15. Local microstructure evolution and mechanical performance of friction stir additive manufactured 2195 Al-Li alloy10.1016/j.matchar.2022.111818 ↗
16. Interfacial bonding features of friction stir additive manufactured build for 2195-T8 aluminum-lithium alloy10.1016/j.jmapro.2019.01.042 ↗
17. Friction stir additive manufacturing: route to high structural performance10.1007/s11837-014-1271-x ↗
18. Investigation on microstructural evolution and property variation along building direction in friction stir additive manufactured Al–Zn–Mg alloy10.1016/j.msea.2020.139035 ↗
19. Correlation of local microstructures and mechanical properties of Al–Zn–Mg–Cu alloy build fabricated via underwater friction stir additive manufacturing10.1016/j.msea.2020.140590 ↗
20. Lequeu P.H., Muzzolini R., Ehrstrom J.C., Bron F., Maziarz R. High-Performance friction stir welded structures using advanced alloys. Aeromat Conf., Seattle WA; 2006.
21. Baumann J.A. Production of Energy Efficient Preform Structures (PEEPS). 2012.
22. Review of recent trends in friction stir welding process of aluminum alloys and aluminum metal matrix composites10.1016/S1003-6326(21)65730-8 ↗
23. Microstructure and mechanical properties of aluminum-steel dissimilar metal welded using arc and friction stir hybrid welding10.1016/j.matdes.2022.111520 ↗
24. Combining pre-rolling with retrogression and re-aging treatment to balance strength and corrosion resistance of 7A99 Al alloy10.1016/S1003-6326(23)66307-1 ↗
25. Effect of heat treatment on strength, exfoliation corrosion and electrochemical behavior of 7085 aluminum alloy10.1016/j.matdes.2011.09.033 ↗
26. Study on the solid solution temperature of achieving ultra-high strength in wire-arc additive manufactured Al-Zn-Mg-Cu aluminum alloy10.1016/j.matchar.2023.112975 ↗
27. Microstructure, mechanical properties, aging behavior, and corrosion resistance of a laser powder bed fusion fabricated Al–Zn–Mg–Cu–Ta alloy10.1016/j.msea.2021.142364 ↗
28. Microstructures and properties of wire-arc additively manufactured ultra-high strength aluminum alloy under different heat treatments10.1016/j.jmrt.2023.03.100 ↗
29. Effect of heat treatment process on the micro machinability of 7075 aluminum alloy10.1016/j.vacuum.2022.111574 ↗
30. Wire-arc additive manufacturing of a novel high-performance Al-Zn-Mg-Cu alloy: processing, characterization and feasibility demonstration
31. A review on dissimilar laser welding of steel-copper, steel-aluminum, aluminum-copper, and steel-nickel for electric vehicle battery manufacturing10.1016/j.optlastec.2021.107595 ↗
32. Ultrafast microstructure modification by pulsed electron beam to enhance surface performance10.1016/j.surfcoat.2022.128226 ↗
33. Improved strength in nickel ‑ aluminum bronze / steel bimetallic component fabricated using arcing-wire arc additive manufacturing with alternating deposition strategy10.1016/j.jmapro.2024.01.027 ↗
34. Microstructural characterisation and hardness assessment of wire arc cladded Hastelloy C276 on creep resistant steel P9110.1016/j.jmrt.2022.06.129 ↗
35. Synergistic enhancement of mechanical performance in wire-arc directed energy deposited Al-Zn-Mg-Cu alloys through interlayer friction stir processing, concurrent forced cooling, and post-deposition heat treatment10.1016/j.jmapro.2024.05.059 ↗
36. Microstructure and properties research of Al-Zn-Mg-Cu alloy with high strength and high elongation fabricated by wire arc additive manufacturing10.1016/j.jmatprotec.2022.117665 ↗
37. Recent advances in ageing of 7xxx series aluminum alloys: a physical metallurgy perspective10.1016/j.jallcom.2018.11.286 ↗
38. Effect of heat treatment on microstructure and properties of additively manufactured aluminum bronze-steel bimetallic structures10.1016/j.matchar.2023.113462 ↗
39. Microstructure and mechanical properties of ultra-high strength Al-Zn-Mg-Cu-Sc aluminum alloy fabricated by wire + arc additive manufacturing10.1016/j.jmapro.2022.05.009 ↗
40. Corrosion behavior and mechanical properties of Al-Zn-Mg aluminum alloy weld10.1016/j.corsci.2017.05.007 ↗
41. A protective role of Cl− ion in corrosion of stainless steel10.1016/j.corsci.2023.111631 ↗
42. Zhang J., Liu L., Wang A., Wang J., Fang T., Niu L., et al. Electrochemical impedance behavior of implantable neural interface following the change of equivalent circuit element. 2022 12th Int Conf CYBER Technol Autom Control Intell Syst CYBER 2022 2022:952–7. https://doi.org/10.1109/CYBER55403.2022.9907100.10.1109/CYBER55403.2022.9907100 ↗
43. Effects of high temperature pre-precipitation on mechanical and corrosion behavior of an Al-Zn-Mg-Cu alloy10.1016/j.jallcom.2024.173738 ↗
44. Electrochemical corrosion behavior of Cu-20Fe-12Cr alloys with the different grain size in solutions containing chloride ions10.4028/www.scientific.net/AMR.457-458.655 ↗
45. The anisotropic corrosion behaviour of wire arc additive manufactured Ti-6Al-4V alloy in 3.5% NaCl solution10.1016/j.corsci.2018.03.047 ↗
46. Electrochemical behavior and corrosion mechanism of anodized 7B04 aluminum alloy in acid NaCl environments10.1016/j.jallcom.2021.161231 ↗
47. Enhancing the mechanical performance of Al–Zn–Mg alloy builds fabricated via underwater friction stir additive manufacturing and post-processing aging10.1016/j.jmst.2021.08.050 ↗
48. Influence of predeformation and ageing of an Al-Zn-Mg Alloy-II. Modeling of precipitation kinetics and yield stress10.1016/S1359-6454(98)00296-1 ↗
49. The effect of initial alloy temper on corrosion resistance for Al-Zn-Mg-Cu alloy10.1016/j.corsci.2022.110730 ↗
50. Effect of gradient grain structures on corrosion resistance of extruded Al–Zn–Mg–Cu alloy10.1016/j.jallcom.2020.154911 ↗