Abstract The present work focuses on developing a low-cost medium entropy alloy (MEA) with desirable mechanical properties according to the benchmark CoCrFeMnNi high entropy alloy (MEA). By adjusting the ratio of each component and adding silicon to the system, the Fe50Mn17.5Cr12.5Co10Ni5Si5 MEA with a single face-centered cubic (FCC) phase was developed. After homogenization, hot rolling, cold rolling, and annealing, fully recrystallized MEA specimens with grain sizes ranging from 10 μm to 149 μm were used for tensile tests. The microstructure of the elongated MEAs showed a ɛ-martensite transformation from the FCC phase to the hexagonal close-packed (HCP) phase, indicating the stacking fault energy (SFE) of the MEA was significantly reduced. The room-temperature deformed MEA showed improved mechanical properties in yield strength and tensile strength than the CoCrFeMnNi MEA. Meanwhile, the volume fraction of the HCP phase in cryogenic-deformed MEA is much larger than that in room-temperature deformed MEA; its yield strength was increased by two times, while the tensile strength exceeded the level of 1 GPa. Data availability The authors confirm that the data supporting the findings of this study are available within the article and its supplementary materials.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High Entropy Alloys Studies · High-Temperature Coating Behaviors · Additive Manufacturing Materials and Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. Nanostructured high-entropy alloys with multiple principal elements: novel alloy design concepts and outcomes10.1002/adem.200300567 ↗
2. Structural morphology and characterization of (AlCrMoTaTi)N coating deposited via magnetron sputtering10.1016/j.apsusc.2013.06.057 ↗
3. Anomalous decrease in X-ray diffraction intensities of Cu–Ni–Al–Co–Cr–Fe–Si alloy systems with multi-principal elements10.1016/j.matchemphys.2007.01.003 ↗
4. Processing, microstructure and mechanical properties of the CrMnFeCoNi high-entropy alloy10.1007/s11837-015-1589-z ↗
5. A critical review of high entropy alloys and related concepts10.1016/j.actamat.2016.08.081 ↗
6. High entropy alloys: a focused review of mechanical properties and deformation mechanisms10.1016/j.actamat.2019.12.015 ↗
7. High-entropy alloys: potential candidates for high-temperature applications - an overview
8. Hot deformation behavior of the high-entropy alloy CoCuFeMnNi10.1557/jmr.2018.500 ↗
9. The influences of temperature and microstructure on the tensile properties of a CoCrFeMnNi high-entropy alloy10.1016/j.actamat.2013.06.018 ↗
10. The effect of molybdenum on the corrosion behaviour of the high-entropy alloys Co1.5CrFeNi1.5Ti0.5Mox in aqueous environments10.1016/j.corsci.2010.04.004 ↗
11. Recovery, recrystallization, grain growth and phase stability of a family of FCC-structured multi-component equiatomic solid solution alloys10.1016/j.intermet.2013.10.024 ↗
12. The evolution of the deformation substructure in a Ni-Co-Cr equiatomic solid solution alloy10.1016/j.actamat.2017.04.033 ↗
13. Friction stress and Hall-Petch relationship in CoCrNi equi-atomic medium entropy alloy processed by severe plastic deformation and subsequent annealing10.1016/j.scriptamat.2017.02.042 ↗
14. The influence of manganese content on the stacking fault and austenite/ε-martensite interfacial energies in Fe-Mn-(Al-Si) steels investigated by experiment and theory10.1016/j.actamat.2014.01.001 ↗
15. Influence of deformation induced nanoscale twinning and FCC-HCP transformation on hardening and texture development in medium-entropy CrCoNi alloy10.1016/j.actamat.2018.07.028 ↗
16. Metastable high-entropy dual-phase alloys overcome the strength–ductility trade-off10.1038/nature17981 ↗
17. Cryogenic strength improvement by utilizing room-temperature deformation twinning in a partially recrystallized VCrMnFeCoNi high-entropy alloy10.1038/ncomms15719 ↗
18. Effects of grain size on body-centered-cubic martensitic transformation in metastable Fe46Co30Cr10Mn5Si7V2 high-entropy alloy10.1016/j.scriptamat.2020.11.005 ↗
19. Superior low-cycle fatigue properties of CoCrNi compared to CoCrFeMnNi10.1016/j.scriptamat.2020.113667 ↗
20. Temperature and load-ratio dependent fatigue-crack growth in the CrMnFeCoNi high-entropy alloy10.1016/j.jallcom.2019.04.234 ↗
21. Superior cryogenic tensile properties of ultrafine-grained CoCrNi medium-entropy alloy produced by high-pressure torsion and annealing10.1016/j.scriptamat.2019.01.016 ↗
22. Cryogenic-deformation-induced phase transformation in an FeCoCrNi high-entropy alloy10.1080/21663831.2018.1434250 ↗
23. Unraveling the discontinuous plastic flow of a Co-Cr-Fe-Ni-Mo multiprincipal-element alloy at deep cryogenic temperatures
24. Design of high-ductile medium entropy alloys for dental implants10.1016/j.msec.2020.110959 ↗
25. Revealing the deformation mechanisms of Cu–Al alloys with high strength and good ductility10.1016/j.actamat.2016.03.015 ↗
26. Factors affecting dynamic recrystallization of metals and alloys10.1179/mst.1987.3.5.329 ↗
27. Stacking fault energy of face-centered-cubic high entropy alloys10.1016/j.intermet.2017.10.004 ↗
28. The influence of stacking fault energy on the microstructural and strain-hardening evolution of Fe–Mn–Al–Si steels during tensile deformation10.1016/j.actamat.2015.08.030 ↗
29. A. Standard, E8/E8M, 2013a," Standard Test Methods for Tension Testing of Metallic Materials," ASTM International, West Conshohocken, PA, 2013, DOI: 〈10.1520/E0008_E0008M〉, (n.d.).
30. NanoAnalysis, Oxford AZtec User Manual, Oxford Instruments. (2013). 〈https://nano.oxinst.com/products/aztec/aztechkl〉.
31. Temperature dependencies of the elastic moduli and thermal expansion coefficient of an equiatomic, single-phase CoCrFeMnNi high-entropy alloy10.1016/j.jallcom.2014.11.061 ↗
32. The deformation and ageing of mild steel: III discussion of results10.1088/0370-1301/64/9/303 ↗
33. The cleavage strength of polycrystals
34. Optimizing the coupled effects of hall-petch and precipitation strengthening in a Al0.3CoCrFeNi high entropy alloy10.1016/j.matdes.2017.02.072 ↗
35. Microstructural evolution of a CoCrFeMnNi high-entropy alloy after swaging and annealing10.1016/j.jallcom.2015.05.129 ↗
36. Comparison of cryogenic deformation of the concentrated solid solutions CoCrFeMnNi, CoCrNi and CoNi10.1016/j.msea.2020.139290 ↗
37. Size effect, critical resolved shear stress, stacking fault energy, and solid solution strengthening in the CrMnFeCoNi high-entropy alloy10.1038/srep35863 ↗
38. The role of irradiation on deformation-induced martensitic phase transformations in face-centered cubic alloys10.1557/jmr.2020.80 ↗
39. Effect of elemental combination on friction stress and hall-petch relationship in face-centered cubic high / medium entropy alloys10.1016/j.actamat.2019.04.017 ↗
40. Dislocation theory of martensitic transformations
41. Screw dislocation driven martensitic nucleation: a step toward consilience of deformation scenario in fcc materials10.1016/j.actamat.2019.05.050 ↗
42. Correlations between the calculated stacking fault energy and the plasticity mechanisms in Fe–Mn–C alloys10.1016/j.msea.2004.01.059 ↗
43. Deformation behavior of HCP Ti-Al alloy single crystals10.1007/s11661-002-0153-y ↗
44. Deformation mechanisms in austenitic TRIP/TWIP steel as a function of temperature10.1007/s11661-014-2684-4 ↗
45. Shear and shuffling accomplishing polymorphic fcc γ → hcp ε → bct α martensitic phase transformation10.1016/j.actamat.2017.07.016 ↗
46. Martensitic transformation and mechanical behavior of a medium-entropy alloy10.1016/j.msea.2020.139371 ↗
47. Significant contribution of stacking faults to the strain hardening behavior of Cu-15%Al alloy with different grain sizes10.1038/srep16707 ↗
48. Mechanism of twinning induced plasticity in austenitic lightweight steel driven by compositional complexity10.1016/j.actamat.2021.116814 ↗
49. Tensile deformation behavior and deformation twinning of an equimolar CoCrFeMnNi high-entropy alloy10.1016/j.msea.2017.02.043 ↗
50. The effect of grain size and strain on the tensile flow stress of aluminium at room temperature10.1016/0001-6160(77)90171-7 ↗
51. Two-stage hall-petch relationship in Cu with recrystallized structure10.1016/j.jmst.2019.12.023 ↗
52. A novel ultrafine-grained Fe 22Mn 0.6C TWIP steel with superior strength and ductility10.1016/j.matchar.2016.12.026 ↗
53. Grain size dependence of mechanical, corrosion and tribological properties of high nitrogen stainless steels10.1023/A:1025181820252 ↗
54. Tensile properties of a nanocrystalline 316L austenitic stainless steel10.1016/j.scriptamat.2005.01.023 ↗
55. Ferrite effects in Fe-Mn-Al-C triplex steels10.1007/s11661-013-1990-6 ↗
56. Enhanced strength and ductility of bulk CoCrFeMnNi high entropy alloy having fully recrystallized ultrafine-grained structure10.1016/j.matdes.2017.07.054 ↗