Abstract
This manuscript examines development of noble corrosion-resistant Ti6Al4VxCryNi alloys by μ-plasma arc powder additive manufacturing (μ-PAPAM) process for chemical, shipbuilding, and aerospace industries. Inclusion of chromium and/or nickel to Ti6Al4V alloy decreased corrosion rate and corrosion current density and increased corrosion potential and polarisation resistance, implying increased corrosion resistance. The EIS findings indicated that the values of polarization resistance and layer thickness of oxides increased with the addition of chromium and/or nickel to Ti6Al4V alloy. Smaller size pits were observed on the corroded surfaces of developed Ti6Al4VxCryNi alloys due to the formation of relatively more stable layer of Cr 2O 3 and NiO enabled by the inclusion of chromium and/or nickel to Ti6Al4V alloy. It improved the surface finish of the developed alloys, indicating less damage by their corrosion and the appearance of small-size pits due to layer formation of Cr 2O 3 and NiO. As compared to Ti6Al4V alloy, Ti6Al4V5Cr alloy has maximum corrosion resistance followed by Ti6Al4V2.5Cr2.5Ni and Ti6Al4V5Ni alloy.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Metal and Thin Film Mechanics · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Microstructure characterization and tensile performance of a high-strength titanium alloy with in-situ precipitates of Ti5Si310.1016/j.jallcom.2023.171867 ↗
2. Investigation of electrochemical corrosion behaviour of additive manufactured Ti–6Al–4V alloy for medical implants in different electrolytes.10.1016/j.jallcom.2020.154620 ↗
3. The corrosion behaviour of Ti6Al4V fabricated by selective laser melting in the artificial saliva with different fluoride concentrations and pH values.10.1016/j.corsci.2020.109097 ↗
4. The corrosion resistance of dental Ti6Al4V with differing microstructures in oral environments10.1016/j.jmrt.2023.10.082 ↗
5. Mechano-electrochemical interaction of high-strength pipeline steels with Al-Ti deoxidization and Mg-Ca compound treatment10.1016/j.corsci.2023.111534 ↗
6. Microstructure and corrosion of CrFeMnV multi-principal element alloy10.1016/j.corsci.2023.111403 ↗
7. Controlling the corrosion resistance of multi-principal element alloys10.1016/j.scriptamat.2020.06.065 ↗
8. Electrochemical dissolution behaviour of Ti6Al4V alloy: Effect of microstructure and processing method.10.1016/j.jmatprotec.2022.117646 ↗
9. Heat treatment effects on the electrochemical behaviour of pore-free Ti6Al4V ELI fabricated by laser powder bed fusion in fluoride-containing chloride solution.10.1016/j.jallcom.2022.168439 ↗
10. Research on the surface characterization, corrosion and bioactivity of nano-featured tantalum coating on selective electron beam melted Ti6Al4V alloy10.1016/j.jallcom.2023.169351 ↗
11. Effects of laser shock peening on the hot corrosion behaviour of the selective laser melted Ti6Al4V titanium alloy10.1016/j.corsci.2021.109558 ↗
12. Corrosion, wear and in-vitro biocompatibility property of surface mechanical attrition treatment processed Ti-6Al-4V alloy10.1007/s11837-021-04970-x ↗
13. Corrosion behaviour of dual-phase Ti-6Al-4V alloys: A discussion on the impact of Fe content.10.1016/j.jallcom.2020.157708 ↗
14. Surface hardness and corrosion behaviour of laser surface alloyed Ti6Al4V with copper10.1016/j.surfcoat.2022.128663 ↗
15. Effect of Nb addition on mechanical properties and corrosion behaviour of Ti6Al4V alloy produced by selective laser melting10.1557/jmr.2019.415 ↗
16. Effect of scandium on microstructure and corrosion resistance of Ti64 alloy in NaCl solution
17. Laser surface alloying of titanium alloy with silver: Microstructure, hardness, and corrosion property10.1016/j.surfcoat.2023.129357 ↗
18. Effect of zirconium content on the microstructure and corrosion behaviour of Ti-6Al-4V-xZr alloys10.1016/j.corsci.2016.09.012 ↗
19. the effect of heat treatment on microstructure, microhardness, and pitting corrosion of Ti6Al4V produced by electron beam melting additive manufacturing process10.1007/s00170-022-08839-4 ↗
20. Effect of heat treatment on microstructure and corrosion behaviour of Ti6Al4V fabricated by laser beam powder bed fusion.10.1016/j.corsci.2022.110789 ↗
21. Electrochemical properties of the heat-treated Ti-6Al-4V alloy manufactured by direct energy deposition10.1016/j.jallcom.2021.163226 ↗
22. Evaluation of stellite coatings by µ-PTA powder, laser and PTA deposition processes10.1080/10426914.2017.1364764 ↗
23. Investigations on additive manufacturing of Ti–6Al–4V by micro plasma transferred arc powder deposition process10.1115/1.4040324 ↗
24. Development of Ti-Ta-Nb-Mo-Zr high entropy alloy by μ-plasma arc additive manufacturing process for knee implant applications and its biocompatibility evaluation10.1016/j.jmrt.2022.11.167 ↗
25. Corrosion susceptibility of passive films on 1060, 2024, and 5083 aluminum alloys: experimental study and first-principles calculations10.1149/1945-7111/accab8 ↗
26. Heat treatment of additively manufactured Ti-6Al-4V alloy: Microstructure and electrochemical properties10.1016/j.jallcom.2021.161602 ↗
27. Microstructural, mechanical, electrochemical, and biological studies of an electron beam melted Ti-6Al-4V alloy
28. Surface hardness and corrosion behaviour of laser surface alloyed Ti6Al4V with copper10.1016/j.surfcoat.2022.128663 ↗
29. The anisotropic corrosion behaviour of wire arc additive manufactured Ti-6Al-4V alloy in 3.5% NaCl solution10.1016/j.corsci.2018.03.047 ↗
30. Influence of Ru on structure and corrosion behaviour of passive film on Ti-6Al-4V alloy in oil and gas exploration conditions
31. Effect of thermal treatment and fluoride ions on the electrochemical corrosion behaviour of selective laser melted CoCrW alloy10.1016/j.jallcom.2017.09.318 ↗
32. Corrosion behaviour of pure Ti under a solid NaCl deposit in a wet oxygen flow at 600ºC10.3390/met6040072 ↗
33. Electrochemical performance, and corrosion mechanism of Cr–DLC coating on nitride Ti6Al4V alloy by magnetron sputtering.10.1016/j.diamond.2021.108398 ↗
34. Structure, mechanical properties and corrosion resistance of amorphous Ti-Cr-O coatings10.1016/j.surfcoat.2019.06.061 ↗
35. Immersion corrosion and electrochemical performances of laser cladded FeSiB, FeSiBCr and FeSiBCrMo coatings in 3.5 wt% NaCl solution.10.1016/j.surfcoat.2019.125229 ↗
36. Electrochemical behaviour of open-cellular structured Ti-6Al-4V alloy fabricated by electron beam melting in simulated physiological fluid: the significance of pore characteristics10.1016/j.jmst.2021.05.024 ↗
37. Titanium fabricated by selective laser melting: Microstructure, wear and corrosion behaviour in different orientations10.1108/RPJ-07-2021-0176 ↗
38. A review of passivity breakdown on metal surfaces: Influence of chloride-and sulfide-ion concentrations, temperature, and pH10.1007/s42247-021-00194-6 ↗