New insights into oxidation mechanism and kinetics of 9Cr–1Mo ferritic-martensitic steel in oxygen-saturated liquid lead-bismuth eutectic

Zhikun Zhou, Chenwen Tian, Juan Du, Xuhao Peng, Yunpeng Liu, Xiaofei Yu, Xue Mi, Zhuo Pu, Hai Xie, Magd Abdel Wahab, Ziguang Chen

Abstract

The evolution of oxide scales on a 9Cr-1Mo ferritic-martensitic steel (T91) in oxygen-saturated liquid LeadBismuth Eutectic (LBE) at 500 degrees C is investigated. While taken out at around 500 degrees C, the T91 steel, after corrosion, shows clean surface with little LBE adhesion due to the poor wettability induced by surface oxides. The results reveal the evolution of surface oxides from irregular strip shapes to regular crystalline grains, and stack-packed equiaxed crystals in the outer magnetite layer. Thermally-induced cracks are captured in the oxide scale on T91 steel after 1000 h exposure to LBE. A new oxidation mechanism is proposed, with consideration of the formation of the outer layer by metal dissolution/oxide precipitation, and a thin film of chromium oxide at the inner/outer layers interface. The dependency of temperature and oxygen concentration on the oxidation kinetics of T91 steel in LBE is discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Nuclear reactor physics and engineering · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (74)

Show source-provided references
1. Concept of an accelerator-driven advanced nuclear energy system10.3390/en10070944 ↗
2. GEN-IV LFR development: status & perspectives10.1016/j.pnucene.2018.02.005 ↗
3. C. Fazio, V. Sobolev, A. Aerts, S. Gavrilov, K. Lambrinou, P. Schuurmans, A. Gessi, P. Agostini, A. Ciampichetti, L. Martinelli, Handbook on lead-bismuth eutectic alloy and lead properties, materials compatibility, thermal-hydraulics and technologies-2015 Edition (No. NEA--7268), in, Organisation for Economic Co-Operation and Development, 2015.
4. Environmental degradation of structural materials in liquid lead- and lead-bismuth eutectic-cooled reactors10.1016/j.pmatsci.2022.100920 ↗
5. Materials for future nuclear energy systems10.1016/j.jnucmat.2019.151837 ↗
6. Ferritic-martensitic steels for fission and fusion applications10.1016/j.jnucmat.2019.05.058 ↗
7. W. Ren, Preliminary considerations of modified 9Cr-1Mo steel for Gen IV nuclear reactor application, in: ASME Pressure Vessels and Piping Division Conference, Chicago, 2008, pp. 753-766.10.1115/PVP2008-61004 ↗
8. Embrittlement of a martensitic steel by liquid lead10.1016/S1359-6462(00)00523-6 ↗
9. Liquid Pb–Bi embrittlement effects on the T91 steel after different heat treatments10.1016/j.jnucmat.2008.02.050 ↗
10. Investigation of liquid LBE embrittlement effects on irradiated ferritic/martensitic steels by slow-strain-rate tensile tests10.1016/j.jnucmat.2011.11.036 ↗
11. Investigating liquid-metal embrittlement of T91 steel by fracture toughness tests10.1016/j.jnucmat.2015.12.019 ↗
12. Liquid metal embrittlement sensitivity of the T91 steel in lead, in bismuth and in lead-bismuth eutectic10.1016/j.jnucmat.2020.152021 ↗
13. Initiation of LME crack in ferritic martensitic steel in liquid lead-bismuth10.1016/j.jnucmat.2018.09.033 ↗
14. Liquid lead–bismuth eutectic embrittlement effect on the tensile properties of T91 steel at 350°C10.1002/maco.202112530 ↗
15. Effects of pre-exposure and simulated corrosion “pits” on liquid metal embrittlement of T91 steel exposed to liquid lead-bismuth eutectic at 350 °C10.1016/j.jnucmat.2022.153641 ↗
16. Liquid metal embrittlement susceptibility of T91 steel by lead-bismuth10.1016/j.scriptamat.2005.02.027 ↗
17. Low cycle fatigue behavior of a modified 9Cr–1Mo ferritic–martensitic steel in lead–bismuth eutectic at 350 °C–Effects of oxygen concentration in the liquid metal and strain rate10.1016/j.corsci.2015.02.022 ↗
18. The role of oxide films in preventing liquid metal embrittlement of T91 steel exposed to liquid lead-bismuth eutectic10.1016/j.jnucmat.2018.07.018 ↗
19. On the mechanism of sulphide scale formation on iron10.1016/S0010-938X(65)80018-X ↗
20. Investigation on oxygen controlled liquid lead corrosion of surface treated steels10.1016/S0022-3115(99)00211-1 ↗
21. Oxidation mechanism of steels in liquid–lead alloys10.1007/s11085-005-4392-3 ↗
22. Oxidation mechanism of a Fe–9Cr–1Mo steel by liquid Pb–Bi eutectic alloy (Part I)10.1016/j.corsci.2008.06.050 ↗
23. Oxidation mechanism of an Fe–9Cr–1Mo steel by liquid Pb–Bi eutectic alloy at 470°C (Part II)10.1016/j.corsci.2008.06.051 ↗
24. Oxidation mechanism of T91 steel in liquid lead-bismuth eutectic: with consideration of internal oxidation10.1038/srep35268 ↗
25. A refined oxidation mechanism proposed for ferritic-martensitic steels exposed to oxygen-saturated liquid lead-bismuth eutectic at 400°C for 500h10.1016/j.jnucmat.2021.152852 ↗
26. Microstructure evolution of magnetite layer on CLAM steel exposed to lead-bismuth eutectic containing 10−6 wt% oxygen at 500 °C10.1016/j.jnucmat.2022.153579 ↗
27. Corrosion kinetics of steel T91 in flowing oxygen-containing lead–bismuth eutectic at 450°C10.1016/j.jnucmat.2011.11.014 ↗
28. Influence of temperature on the interaction mode of T91 and AISI 316L steels with Pb–Bi melt saturated by oxygen10.1016/j.corsci.2008.02.006 ↗
29. Oxidation behavior of ferritic/martensitic steels in stagnant liquid LBE saturated by oxygen at 600 °C10.1016/j.jnucmat.2014.11.018 ↗
30. Stress corrosion behavior of T91 steel in static lead–bismuth eutectic at 480 °C10.1016/j.jnucmat.2015.09.032 ↗
31. Transmission electron microscopy (TEM) on oxide layers formed on D9 stainless steel in lead bismuth eutectic (LBE)10.1016/j.corsci.2012.09.019 ↗
32. Effect of substrate grain size on the growth, texture and internal stresses of iron oxide scales forming at 450C10.1007/s11085-009-9162-1 ↗
33. Review of the high-temperature oxidation of iron and carbon steels in air or oxygen10.1023/A:1023685905159 ↗
34. Corrosion of 9Cr steel in CO2 at intermediate temperature I: mechanism of void-induced duplex oxide formation10.1007/s11085-011-9271-5 ↗
35. Corrosion behavior of heat-resistant steel T91 in high-temperature supercritical carbon dioxide with impurity O2, SO2 or H2S10.1016/j.supflu.2023.105936 ↗
36. Continuous and cyclic oxidation of T91 ferritic steel under steam10.1016/S0010-938X(03)00173-2 ↗
37. The mechanism of oxide film formation on austenitic stainless steels in high temperature water10.1016/S0010-938X(97)00140-6 ↗
38. The mechanism of high temperature aqueous corrosion of steel10.1016/0010-938X(89)90120-0 ↗
39. Corrosion characteristics and mechanisms of typical Ni-based corrosion-resistant alloys in sub- and supercritical water10.1016/j.supflu.2020.105138 ↗
40. Corrosion behavior of Alloy 690 in aerated supercritical water10.1016/j.corsci.2012.10.001 ↗
41. Characterization of oxide films grown on 316L stainless steel exposed to H2O2-containing supercritical water10.1016/j.supflu.2006.12.020 ↗
42. Comparison of solid metal–metal oxide reference electrodes for potentiometric oxygen sensors in liquid lead–bismuth eutectic operating at low temperature ranges10.1016/j.snb.2015.03.004 ↗
43. Liquid metal embrittlement susceptibility of a high-entropy alloy exposed to oxygen-depleted liquid lead-bismuth eutectic at 250 and 350 °C10.1016/j.jnucmat.2019.151859 ↗
44. Creep failure of a solution-annealed 15-15Ti steel exposed to stagnant lead-bismuth eutectic at 550 and 600 °C10.1016/j.msea.2020.140230 ↗
45. C. Schroer, J. Konys, Physical chemistry of corrosion and oxygen control in liquid lead and lead bismuth eutectic, in, Forschungszentrum Karlsruhe Karlsruhe, 2007.
46. Fiji: an open-source platform for biological-image analysis10.1038/nmeth.2019 ↗
47. M.D. Abràmoff, P.J. Magalhães, S.J. Ram, Image processing with ImageJ, Biophotonics international, 11 (2004) 36-42.
48. NIH Image to ImageJ: 25 years of image analysis10.1038/nmeth.2089 ↗
49. ImageJ2: ImageJ for the next generation of scientific image data10.1186/s12859-017-1934-z ↗
50. Long term corrosion on T91 and AISI1 316L steel in flowing lead alloy and corrosion protection barrier development: Experiments and models10.1016/j.jnucmat.2011.04.028 ↗
51. The mechanism of thermal oxide film formation on low Cr martensitic stainless steel and its behavior in fluoride-based pickling solution in conversion treatment10.1016/j.corsci.2020.109206 ↗
52. Influence of oxide scale on the wettability of LBE on T91 steel10.1016/j.fusengdes.2017.03.089 ↗
53. Characterization of oxide scales grown on 216L stainless steels in liquid lead–bismuth eutectic10.1016/j.corsci.2012.05.016 ↗
54. An essay on the cohesion of fluids
55. Calama, What do we need for a superhydrophobic surface? A review on the recent progress in the preparation of superhydrophobic surfaces10.1039/b602486f ↗
56. Superhydrophobic surfaces for corrosion protection: a review of recent progresses and future directions10.1007/s11998-015-9744-6 ↗
57. Hierarchical micro/nano structures for super-hydrophobic surfaces and super-lyophobic surface against liquid metal10.1186/s40486-014-0003-x ↗
58. Structure of surface oxides on martensitic steel under simultaneous ion irradiation and molten LBE corrosion10.1016/j.corsci.2021.109953 ↗
59. Classical and nonclassical nucleation and growth mechanisms for nanoparticle formation10.1146/annurev-physchem-082720-100947 ↗
60. Modelling of nanoparticles: approaches to morphology and evolution10.1088/0034-4885/73/8/086502 ↗
61. Crystallization mechanisms of acicular crystals10.1016/j.jcrysgro.2007.10.006 ↗
62. Diagnostic criteria for distinguishing between the dissolution-precipitation and the solid state mechanisms of passivation10.1016/S0010-938X(71)80003-3 ↗
63. Crystal nucleation and growth: supersaturation and crystal resilience determine stickability10.1021/acs.cgd.2c01459 ↗
64. Insights into the corrosion mechanism of a 12Cr F/M steel in oxygen-saturated liquid LBE10.1016/j.corsci.2023.111602 ↗
65. Graeve, Early stages of liquid-metal corrosion on pre-oxidized surfaces of austenitic stainless steel 316L exposed to static Pb-Bi eutectic at 400 °C10.1016/j.corsci.2023.111680 ↗
66. The distribution of cations in metal oxide and metal sulphide solid solutions formed during the oxidation of alloys10.1016/S0010-938X(69)80046-6 ↗
67. Corrosion characteristics of T91 steel in lead–bismuth eutectic with different oxygen concentrations at 500 °C10.1002/maco.202112505 ↗
68. Modelling of the oxide scale formation on Fe-Cr steel during exposure in liquid lead-bismuth eutectic in the 450–600C temperature range10.1002/maco.201005871 ↗
69. Corrosion behavior of T91 steel in liquid lead-bismuth eutectic at 550 °C: effects of exposure time and dissolved oxygen concentration10.1016/j.corsci.2022.110405 ↗
70. Cracking and exfoliation behavior of oxide scale on T91 steel under different tensile stresses in oxygen-controlled lead-bismuth eutectic at 550° C10.1016/j.corsci.2021.109324 ↗
71. Steel T91 subjected to static stress in lead-bismuth eutectic at 450–550 °C and low oxygen concentration10.1016/j.jnucmat.2018.09.056 ↗
72. Cracking and spalling of protective oxide layers10.1016/0921-5093(89)90731-4 ↗
73. Influence of temperature on the oxide spallation of T91 alloy superheater tubes in power plant10.1016/j.applthermaleng.2017.08.139 ↗
74. Early oxidation of Super304H stainless steel and its scales stability in supercritical water environments10.1016/j.ijhydene.2016.04.144 ↗