Abstract
High-temperature oxidation and elemental diffusion significantly affect the microstructure and mechanical properties of Cr-coated zircaloys under accident conditions, leading to cracking modes different from those of samples with fresh coatings. To clarify the intrinsic mechanisms, in situ three-point bending tests were performed and finite element models were built for the Cr-coated Zr-4 alloys oxidized and vacuum-annealed at 1000 °C. In the case of vacuum-annealed Cr coatings, although numerous microcracks were initiated in the brittle ZrCr 2 diffusion layer under external loading, they could hardly propagate through the Cr coating. Recrystallization and grain growth under the annealing conditions led to significant improvement in the ductility of the Cr coating and its deformation compatibility with the substrate, resulting in the best crack resistance of the coating. In the case of oxidized Cr coatings, oxygen penetrated the Cr coating on the substrate, causing a β-Zr to α-Zr(O) phase transformation beneath the interface at the high annealing temperature. Under external loading, driven by large stresses, the brittle layers of Cr 2O 3, ZrCr 2, and α-Zr(O) were susceptible to microcracking, and some cracks penetrated the Cr coating. However, the crack resistance of the oxidized Cr coating was better than that of the as-deposited coating.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Nuclear reactor physics and engineering
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. High temperature steam oxidation of chromium-coated zirconium-based alloys: kinetics and process10.1016/j.corsci.2020.108537 ↗
2. Accident tolerant fuel cladding development: Promise, status, and challenges10.1016/j.jnucmat.2017.12.043 ↗
3. Protective coatings on zirconium-based alloys as accident-tolerant fuel (ATF) claddings10.1515/corrrev-2017-0010 ↗
4. Accident tolerant fuels for LWRs: a perspective10.1016/j.jnucmat.2013.12.005 ↗
5. Adhesion property and high-temperature oxidation behavior of Cr-coated Zircaloy-4 cladding tube prepared by 3D laser coating10.1016/j.jnucmat.2015.06.030 ↗
6. Semi-integral LOCA test of cold-spray chromium coated zircaloy-4 accident tolerant fuel cladding10.1016/j.jnucmat.2021.152940 ↗
7. Oxidation kinetics of Cr-coated zirconium alloy: effect of coating thickness and microstructure10.1016/j.corsci.2020.108883 ↗
8. Early studies on Cr-Coated Zircaloy-4 as enhanced accident tolerant nuclear fuel claddings for light water reactors10.1016/j.jnucmat.2019.02.018 ↗
9. Protection of zirconium by alumina-and chromia-forming iron alloys under high-temperature steam exposure10.1016/j.jnucmat.2013.03.006 ↗
10. Study of the oxidation behavior of CrN coating on Zr alloy in air10.1016/j.jnucmat.2019.01.006 ↗
11. SiC coating as hydrogen permeation reduction and oxidation resistance for nuclear fuel cladding10.1080/00223131.2015.1020901 ↗
12. Reactivity of Zircaloy-4 with Ti3SiC2 and Ti2AlC in the 1100–1300° C temperature range10.1016/j.jnucmat.2015.02.006 ↗
13. Cold spray deposition of Ti2AlC coatings for improved nuclear fuel cladding10.1016/j.jnucmat.2015.06.028 ↗
14. Characterization of Al2O3/ZrO2 composite coatings deposited on Zr-2.5Nb alloy by plasma electrolytic oxidation10.1016/j.apsusc.2018.04.207 ↗
15. Oxidation resistance improvement of Zr-4 alloy in 1000° C steam environment using ZrO2/FeCrAl bilayer coating10.1016/j.surfcoat.2018.05.005 ↗
16. Vacuum-arc chromium-based coatings for protection of zirconium alloys from the high-temperature oxidation in air10.1016/j.jnucmat.2015.06.016 ↗
17. Microstructure, corrosion resistance and oxidation behavior of Cr-coatings on Zircaloy-4 prepared by vacuum arc plasma deposition10.1016/j.corsci.2019.06.029 ↗
18. High-temperature oxidation of thick Cr coating prepared by arc deposition for accident tolerant fuel claddings10.1016/j.jnucmat.2019.01.039 ↗
19. High temperature oxidation and microstructural evolution of cold spray chromium coatings on Zircaloy-4 in steam environments10.1016/j.jnucmat.2019.151737 ↗
20. Development of cold spray chromium coatings for improved accident tolerant zirconium-alloy cladding10.1016/j.jnucmat.2019.03.039 ↗
21. Evaluation of equivalent cladding reacted parameters of Cr-coated claddings oxidized in steam at 1200 °C in relation with oxygen diffusion/partitioning and post-quench ductility10.1016/j.jnucmat.2020.152106 ↗
22. Experimental investigation of cold-spray chromium cladding
23. Degradation and failure phenomena of accident tolerant fuel concepts
24. Enhanced plasticity of the oxide scales by in-situ formed Cr2O3/Cr heterostructures for Cr-based coatings on Zr alloy in 1200°C steam
25. High temperature Cr-Zr interaction of two types of Cr-coated Zr alloys in inert gas environment10.1016/j.jnucmat.2021.152806 ↗
26. In-situ study on the tensile behavior of Cr-coated zircaloy for accident tolerant fuel claddings10.1016/j.surfcoat.2020.125747 ↗
27. Positive or negative role of preoxidation in the crack arresting of Cr coating for accident tolerant fuel cladding10.1016/j.corsci.2021.109870 ↗
28. Effects of oxidation and inter-diffusion on the fracture mechanisms of Cr-coated Zry-4 alloys: an in situ three-point bending study10.1016/j.matdes.2021.110168 ↗
29. Effect of a pre-oxide on the high temperature steam oxidation of Zircaloy-4 and M5Framatome alloys10.1016/j.jnucmat.2019.03.023 ↗
30. Numerical analyses of the residual stress and top coat cracking behavior in thermal barrier coatings under cyclic thermal loading10.1016/j.engfracmech.2018.04.031 ↗
31. A.M. Huntz, B. Pieraggi. Oxydation des matériaux métalliques, Lavoisier, Paris, 2003.
32. Stress release in α-Cr2O3 oxide thin films formed on Ni30-Cr and Fe47-Cr alloys10.1016/j.jallcom.2017.05.137 ↗
33. Mechanical and thermomechanical properties of commercially pure chromium and chromium alloys10.1016/S0022-3115(01)00745-0 ↗
34. Elastic moduli of the C15 Laves-phase materials TaV2, TaV2H(D)x and ZrCr210.1080/13642810008205755 ↗
35. An elastic–plastic shear lag model for fracture of layered coatings10.1016/S0040-6090(02)01124-0 ↗