Abstract Ablation behavior of SiC nanowhisker toughened-SiC/ZrB2-SiC ultra-high temperature multilayer coatings was evaluated under supersonic flame at ∼2173 K for 120s. SiC nanowhisker toughened-SiC/ZrB2-SiC coatings were prepared on graphite substrate by two-step reactive melt infiltration (RMI) method. The ZrB2–SiC outer coating was prepared on the SiC coated graphite surface by in-situ and ex-situ methods. In ex-situ processing, ZrB2 powder was directly introduced into the powder mixture as a raw material. In in-situ processing, ZrB2 phase was formed in the coating by in-situ reaction between ZrO2 and B2O3. The linear and mass ablation rates for the in-situ ZrB2-SiC coating after 120s ablation under supersonic flame were 1.75 μm s−1 and 0.083 × 10−3 g cm−2 s−1 respectively. For the ex-situ ZrB2-SiC coating the linear and mass ablation rates were 1.5 μm s−1 and 0.064 × 10−3 g cm−2 s−1. The results showed that, the ablation resistance of in-situ ZrB2-SiC coating is very close to ex-situ ZrB2-SiC coating which can provide stable protection for the carbon substrate. Moreover, The SiC nanowhisker network structure in both in-situ ans ex-situ ZrB2-SiC coatings not only improved the toughness of the protective film by crack bridging, crack deflection and crack impedance, but also enhanced the bonding ability of protective film by the pinning and framework effects.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Energetic Materials and Combustion · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Ablation resistance of ZrC/SiC gradient coating for SiC-coated carbon/carbon composites prepared by supersonic plasma spraying10.1016/j.jeurceramsoc.2016.02.047 ↗
2. Effect of temperature gradient on the erosion behavior of SiC coating for carbon/carbon composites in a combustion environment10.1016/j.ceramint.2016.08.174 ↗
3. Thermal shock resistance and isothermal oxidation behavior of C/SiC-SiC nano functionally gradient coating on graphite produced via reactive melt infiltration (RMI)10.1016/j.matchemphys.2016.07.004 ↗
4. Effect of SiC/ZrC ratio on the mechanical and ablation properties of C/C–SiC–ZrC composites10.1016/j.corsci.2013.12.017 ↗
5. SiC nanoparticles toughened-SiC/MoSi2-SiC multilayer functionally graded oxidation protective coating for carbon materials at high temperatures10.1007/s11665-017-2725-4 ↗
6. Oxidation resistance and mechanical properties of HfC nanowire-toughened ultra-high temperature ceramic coating for SiC-coated C/C composites10.1016/j.apsusc.2015.11.097 ↗
7. TaB2–SiC–Si multiphase oxidation protective coating for SiC-coated carbon/carbon composites10.1016/j.jeurceramsoc.2013.06.028 ↗
8. Oxidation resistant graded multiphase coating for carbon/carbon composites10.1016/j.surfcoat.2013.06.105 ↗
9. Ablative property of ZrC SiC multilayer coating for PIP-C/SiC composites under oxy-acetylene torch10.1016/j.ceramint.2011.11.063 ↗
10. Oxidation protective ZrB2–SiC coatings with ferrocene addition on SiC coated graphite10.1016/j.ceramint.2015.10.072 ↗
11. A multilayer MoSi2–SiC–B coating to protect SiC-coated carbon/carbon composites against oxidation10.1016/j.vacuum.2012.04.045 ↗
12. Formation mechanism and oxidation behavior of MoSi2–SiC protective coating prepared by chemical vapor infiltration/reaction10.1016/S1003-6326(13)62702-8 ↗
13. Preparation of a nanostructured SiC-ZrO2 coating to improve the oxidation resistance of graphite10.1016/j.surfcoat.2016.08.093 ↗
14. Ablation resistance of ZrB2 SiC/SiC coating prepared by pack cementation for graphite10.1016/j.jallcom.2016.04.010 ↗
15. Effect of B4C, MoSi2, nano SiC and micro-sized SiC on pressureless sintering behavior, room-temperature mechanical properties and fracture behavior of Zr(Hf)B2-based composites10.1016/j.ceramint.2014.03.066 ↗
16. Preparation of oxidation protective ZrB2–SiC coating by in-situ reaction method on SiC-coated carbon/carbon composites10.1016/j.surfcoat.2014.03.017 ↗
17. ZrB 2–SiC gradient oxidation protective coating for carbon/carbon composites10.1016/j.ceramint.2013.12.055 ↗
18. In-situ synthesis of SiC-ZrB 2 coating by a novel pack cementation technique to protect graphite against oxidation10.1016/j.jallcom.2016.08.112 ↗
19. In-situ fabrication of ZrB2–SiC/SiC gradient coating on C/C composites10.1016/j.jallcom.2015.05.205 ↗
20. ZrB2–SiC oxidation protective coating on C/C composites prepared by vapor silicon infiltration process10.1111/j.1551-2916.2009.03481.x ↗
21. Microstructure and ablation performances of dual-matrix carbon/carbon composites10.1016/j.carbon.2006.01.017 ↗
22. Ablation behavior and mechanism of double-layer ZrB2-based ceramic coating for lightweight carbon-bonded carbon fiber composites under oxyacetylene flame at elevate temperature10.1016/j.jallcom.2017.01.242 ↗
23. Ablation resistance of HfB2-SiC coating prepared by in-situ reaction method for SiC coated C/C composites10.1016/j.ceramint.2017.06.052 ↗
24. Ablation and mechanical behavior of a sandwich-structured composite with an inner layer of Cf/SiC between two outer layers of C f/SiC–ZrB2–ZrC10.1016/j.corsci.2013.11.019 ↗
25. Ablation resistance of HfC coating reinforced by HfC nanowires in cyclic ablation environment10.1016/j.jeurceramsoc.2017.02.057 ↗
26. SiC/ZrB2–SiC–ZrC multilayer coating for carbon/carbon composites against ablation10.1016/j.surfcoat.2016.05.028 ↗
27. Laser ablation behaviors of SiC–ZrC coated carbon/carbon composites10.1016/j.surfcoat.2011.03.039 ↗
28. Reaction kinetics and ablation properties of C/C–ZrC composites fabricated by reactive melt infiltration10.1016/j.ceramint.2010.12.002 ↗
29. Ablative property and mechanism of C/C-ZrB2-ZrC-SiC composites reinforced by SiC networks under plasma flame10.1016/j.corsci.2016.02.015 ↗
30. Microstructure and ablation mechanism of C/C-ZrC-SiC composites in a plasma flame10.1016/j.ceramint.2017.04.089 ↗
31. Microstructure and ablation behavior of SiC coated C/C–SiC–ZrC composites prepared by a hybrid infiltration process10.1016/j.carbon.2013.08.014 ↗
32. Fabrication and ablation property of carbon/carbon composites with novel SiC–ZrB2 coating10.1016/S1003-6326(15)64012-2 ↗
33. C/SiC gradient oxidation protective coating on graphite by modified reactive melt infiltration method: effects of processing parameters on transition interface thickness and high-temperature anti-oxidation behavior10.1007/s11661-016-3813-z ↗
34. A SiC–Si–ZrB2 multiphase oxidation protective ceramic coating for SiC-coated carbon/carbon composites10.1016/j.ceramint.2011.10.047 ↗
35. Oxidation and ablation resistance of Fe2O3 modified ZrB2–SiC–Si coating for carbon/carbon composites10.1016/j.ceramint.2015.08.105 ↗
36. ZrB2/SiC as a protective coating for C/SiC composites: effect of high temperature oxidation on mechanical properties and anti-ablation property10.1016/j.compositesb.2012.07.007 ↗
37. Zircon formation from amorphous silica and tetragonal zirconia: kinetic study and modelling10.1016/S0167-2738(01)00676-2 ↗