Design and characterization of nano and bimodal structured biodegradable Fe-Mn-Ag alloy with accelerated corrosion rate
Source abstract
Abstract
Highlights of the Study This study investigates the design and characterization of nano-, micro-, and bimodal-structured biodegradable Fe–Mn–Ag alloys with the aim of accelerating the corrosion rate of iron-based biodegradable metals while maintaining favorable mechanical performance. Fe–30Mn–Ag alloys were fabricated through mechanical alloying and spark plasma sintering (SPS), and the relationships between microstructure, corrosion behavior, and mechanical properties were systematically evaluated. Key findings: 🔹 Bimodal alloy fabrication: Bimodal Fe–Mn–Ag alloys were successfully produced using mechanical alloying followed by spark plasma sintering. 🔹 Distinct phase structures: The bimodal alloy exhibited a combination of austenitic γ-FeMn and ferritic α-Fe phases, whereas the nano- and macro-structured alloys were predominantly composed of γ-FeMn and α-Fe phases, respectively. 🔹 Effect of silver addition: Incorporating 1–3 wt.% Ag into the nanostructured Fe–30Mn alloy increased the corrosion rate from 0.24 mm/year to 0.33 and 0.58 mm/year for Fe–30Mn–1Ag and Fe–30Mn–3Ag, respectively. 🔹 Accelerated corrosion rate: The bimodal Fe–30Mn–1Ag alloy achieved a substantially higher corrosion rate of 0.88 mm/year, demonstrating the effectiveness of bimodal microstructural design for accelerating degradation. 🔹 High mechanical performance: The bimodal alloy exhibited a high strength of 722 MPa together with 38% ductility, providing mechanical performance comparable to stainless steel. 🔹 Shear properties: The combination of high- and low-microhardness phases resulted in a shear strength of 417 MPa and a shear strain of 0.66. 🔹 Structure–property relationship: The coexistence of nano- and microstructural features played an important role in simultaneously controlling corrosion behavior and mechanical performance. 🔹 Biodegradable alloy design: Bimodal structural engineering provides a novel strategy for designing Fe-based biodegradable alloys with accelerated corrosion while retaining suitable mechanical properties. Overall, the bimodal Fe–30Mn–1Ag alloy demonstrated an attractive combination of accelerated biodegradation, high strength, and substantial ductility, highlighting bimodal microstructural design as a promising strategy for the development of next-generation Fe-based biodegradable metallic implants. KEYWORDS Biodegradable Metals • Bimodal Structure • Corrosion • Fe–Mn–Ag • Spark Plasma Sintering • Mechanical Alloying • Nanostructured Alloy • Biodegradable Implants HOW TO CITE Sotoudeh Bagha, P., Khakbiz, M., Sheibani, S., & Hermawan, H. (2018). Design and characterization of nano and bimodal structured biodegradable Fe-Mn-Ag alloy with accelerated corrosion rate. Journal of Alloys and Compounds, 767, 955–965. DOI: 10.1016/j.jallcom.2018.07.206 Publisher: Elsevier Article Website: ScienceDirect – Journal of Alloys and Compounds
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Corrosion Behavior and Inhibition · Magnesium Alloys: Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Updates on the research and development of absorbable metals for biomedical applications10.1007/s40204-018-0091-4 ↗
2. Long-term in vivo corrosion behavior, biocompatibility and bioresorption mechanism of a bioresorbable nitrided iron scaffold10.1016/j.actbio.2017.03.020 ↗
3. Biodegradable Fe-based alloys for use in osteosynthesis: outcome of an in vivo study after 52 weeks10.1016/j.actbio.2014.04.007 ↗
4. In vitro and in vivo corrosion properties of new iron-manganese alloys designed for cardiovascular applications10.1002/jbm.b.33234 ↗
5. Microstructure, mechanical and corrosion properties of biodegradable powder metallurgical Fe-2 wt% X (X = Pd, Ag and C) alloys10.1016/j.matchemphys.2016.06.087 ↗
6. Novel biodegradable Fe-Mn-C-S alloy with superior mechanical and corrosion properties10.1016/j.matlet.2016.10.037 ↗
7. Fe-Au and Fe-Ag composites as candidates for biodegradable stent materials10.1002/jbm.b.33389 ↗
8. In vitro degradation and biocompatibility of Fe-Pd and Fe-Pt composites fabricated by spark plasma sintering10.1016/j.msec.2013.10.023 ↗
9. Characterization and in vivo evaluation of a bio-corrodible nitrided iron stent10.1007/s10856-012-4823-z ↗
10. In vitro studies on silver implanted pure iron by metal vapor vacuum arc technique10.1016/j.colsurfb.2016.01.065 ↗
11. Magnetron sputtering a new fabrication method of iron based biodegradable implant materials10.1155/2015/294686 ↗
12. Controlling the degradation kinetics of porous iron by poly(lactic-co-glycolic acid) infiltration for use as temporary medical implants10.1038/srep11194 ↗
13. Tailoring the electrochemical degradation of iron protected with polypyrrole films for biodegradable cardiovascular stents10.1016/j.electacta.2017.05.172 ↗
14. Strategy of metal–polymer composite stent to accelerate biodegradation of iron-based biomaterials10.1021/acsami.7b15206 ↗
15. Design of Fe–Mn–Ag alloys as potential candidates for biodegradable metals10.1007/s40195-018-0702-z ↗
16. Corrosion properties of bioresorbable FeMn-Ag alloys prepared by selective laser melting10.1002/maco.201709478 ↗
17. Grain size distribution effects on the corrosion behaviour of materials10.1016/j.corsci.2012.04.040 ↗
18. Effect of grain size on corrosion: a review
19. Influence of cross-rolling on the micro-texture and biodegradation of pure iron as biodegradable material for medical implants10.1016/j.actbio.2015.01.024 ↗
20. Study on microstructure and properties of bimodal structured ultrafine-grained ferrite steel10.3390/met7080316 ↗
21. Effects of Strain energy and grain size on corrosion resistance of ultrafine grained Fe-20%Cr Steels with extremely low C and N fabricated by ECAP10.1155/2015/386865 ↗
22. Synthesizing of nanostructured Fe-Mn alloys by mechanical alloying process10.1016/j.mspro.2015.11.134 ↗
23. Characterization of nanostructured biodegradable Zn-Mn alloy synthesized by mechanical alloying10.1016/j.jallcom.2017.11.155 ↗
24. Bimodally grained high-strength Fe fabricated by mechanical alloying and spark plasma sintering10.1016/j.actamat.2009.03.034 ↗
25. Novel antibacterial biodegradable Fe-Mn-Ag alloys produced by mechanical alloying10.1016/j.msec.2018.03.005 ↗
26. ASTM G59-97(2014), Standard Test Method for Conducting Potentiodynamic Polarization Resistance Measurements, ASTM International, West Conshohocken, n.d.
27. ASTM G31-72(2004) · 2004
28. Superplasticity of a nano-grained Mg–Gd–Y–Zr alloy processed by high-pressure torsion10.1016/j.msea.2015.10.094 ↗
29. Effect of impurities in iron on corrosion in acids10.1149/1.2423393 ↗
30. Coarsening in sintering: grain shape distribution, grain size distribution, and grain growth kinetics in solid-pore systems10.1080/10408436.2010.525197 ↗
31. Transient liquid-phase sintering using silver and tin powder mixture for die bonding10.7567/JJAP.55.04EC14 ↗
32. Review: liquid phase sintering10.1007/s10853-008-3008-0 ↗
33. X-ray line broadening from filed aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
34. Sintering, consolidation, reaction and crystal growth by the spark plasma system (SPS)10.1016/S0921-5093(00)00773-5 ↗
35. The Ag−Fe (Silver-Iron) system10.1007/BF02868316 ↗
36. The Ag-Mn (Silver-Manganese) system10.1007/BF02898263 ↗
37. Materials selection and design
38. Tensile property and microstructure of Fe-22Mn-0.5C TWIP steel10.1016/j.msea.2017.09.061 ↗
39. Effect of two-step intercritical annealing on microstructure and mechanical properties of hot-rolled medium manganese TRIP steel containing δ-ferrite10.1016/j.msea.2017.01.063 ↗
40. Microstructural, mechanical, corrosion and cytotoxicity characterization of the hot forged FeMn30(wt.%) alloy10.1016/j.msec.2015.09.049 ↗
41. Corrosion behaviour of ferrite and austenite phases on super duplex stainless steel in a modified green-death solution10.1016/j.corsci.2014.08.014 ↗
42. Preparation of bimodal grain size 7075 aviation aluminum alloys and their corrosion properties10.1016/j.cja.2017.06.001 ↗
43. Effects of microstructure and heat treatment on mechanical properties and corrosion behavior of powder metallurgy derived Fe–30Mn alloy10.1016/j.msea.2017.07.054 ↗
44. Electrochemical impedance spectroscopy study on silver coated metallic implants10.1016/j.electacta.2011.01.072 ↗
45. Orazem · 2017
46. Thickness and clearance effects in shear punch testing10.1002/adem.200600255 ↗
47. A novel high-strength and highly corrosive biodegradable Fe-Pd alloy: structural, mechanical and in vitro corrosion and cytotoxicity study10.1016/j.msec.2017.05.100 ↗
48. Fe-Cr-Ni-Zr alloys with bi-modal grain size distribution: synthesis, mechanical properties and oxidation resistance10.1016/j.msea.2013.02.049 ↗
49. Three strategies to achieve uniform tensile deformation in a nanostructured metal10.1016/j.actamat.2003.12.022 ↗
50. Superplasticity of a fine-grained Mg–9Gd–4Y–0.4Zr alloy evaluated using shear punch testing10.1016/j.jmrt.2014.04.004 ↗
51. Guduru · 2005 · vol. 395 · 307
52. Correlation between shear punch and tensile strength for low-carbon steel and stainless steel sheets10.1007/s11665-012-0256-6 ↗
53. Coronary stents: a materials perspective10.1016/j.biomaterials.2006.11.042 ↗
54. Effect of immersion in simulated body fluid on the mechanical properties and biocompatibility of sintered Fe–Mn-based alloys10.3390/met6120309 ↗
55. Iron – manganese : new class of metallic degradable biomaterials prepared by powder metallurgy10.1179/174329008X284868 ↗