Wetting kinetics and spreading phenomena of the precursor film and bulk liquid in the AgCuTi/TC4 system
Source abstract
Abstract
Abstract The reactive wetting of AgCuTi filler metal over a TC4 substrate was conducted using real-time in situ hot stage microscopy. In addition to the commonly observed bulk liquid, a rapidly spreading precursor film was observed. Both the precursor film and bulk liquid were studied and characterized. The wetting kinetics of the bulk liquid within the main spreading stage was predominantly controlled by chemical reactions, in which Ag-based solid solutions (Ag(s,s)), Ti-based solid solutions (Ti(s,s)) and intermetallic compounds (Ti2Cu) were formed within the central domain. The high temperature phase transition of α-Ti to β-Ti induced by the diffusion of Ag into the TC4 substrate was also observed at the edge domain. In the mid-to late-stage spreading process, a thin precursor film, with an extremely rapid spreading speed, appeared at the front of the triple line. According to compositional analysis, the precursor film was predominantly composed of Ag and exhibited similar spreading characteristics to pure Ag on TC4. The formation mechanism of the precursor film can be explained by the mechanism of rapid adsorption followed by the film overflow; based on this mechanism, a physical model was proposed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · nanoparticles nucleation surface interactions · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. Vacuum brazing TC4 titanium alloy to 304 stainless steel with Cu-Ti-Ni-Zr-V amorphous alloy foil10.1007/s11665-014-1145-y ↗
2. Effect of brazing conditions on microstructure and mechanical properties of Al2O3/Ti–6Al–4V alloy joints reinforced by TiB whiskers10.1016/j.jmst.2013.05.009 ↗
3. Liquid metal/ceramic interactions in the (Cu, Ag, Au)/ZrB2 systems10.1016/j.jeurceramsoc.2006.12.008 ↗
4. Wetting of AgCu-Ti filler on porous Si3N4 ceramic and brazing of the ceramic to TiAl alloy10.1016/j.ceramint.2017.11.212 ↗
5. Microstructure evolution and mechanical properties of ZrO2/TiAl joints vacuum brazed by Ag–Cu filler metal10.1016/j.msea.2015.05.059 ↗
6. Brazing TC4 alloy to Si3N4 ceramic using nano-Si3N4 reinforced AgCu composite filler10.1016/j.matdes.2015.03.046 ↗
7. Wetting and spreading of Sn on molten ZnCl2 treated amorphous Zr55Cu30Al10Ni5 surface10.1016/j.jallcom.2016.03.282 ↗
8. Critical issues for producing UHTC-brazed joints: wetting and reactivity10.1007/s11665-016-1990-y ↗
9. Kinetics of wetting and spreading of AgCu filler metal over Ti-6Al-4V substrates10.1007/s10853-016-0308-7 ↗
10. Precursor film of tin-based active solder wetting on ceramics10.1007/BF00400889 ↗
11. Characteristics of precursor film in the wetting of Zr-based alloys on ZrC substrate at 1253 K10.1016/j.tsf.2014.02.074 ↗
12. Reactive wetting of low carbon steel by al 4043 and 6061 alloys at 600-750 oC10.1016/j.surfcoat.2016.06.005 ↗
13. The spreading kinetics and precursor film characteristics of Zr-based alloy melt on W substrate10.1016/j.matlet.2013.02.005 ↗
14. High-efficiency perovskite solar cells prepared by using a sandwich structure MAI–PbI 2–MAI precursor film10.1039/C6NR07689K ↗
15. Preparation of CuIn (S, Se) 2 films by PLD of precursor layers and post-annealing and their application to solar cells10.1002/pssc.201600183 ↗
16. The preparation and corrosion behaviors of MAO coating on AZ91D with rare earth conversion precursor film10.1016/j.apsusc.2010.11.153 ↗
17. Precursor film in dynamic wetting, electro wetting, and electro-elasto-capillarity10.1103/PhysRevLett.104.246101 ↗
18. Growth of void free Cu2ZnSnS4 (CZTS) thin films by sulfurization of stacked metallic precursor films10.1016/j.vacuum.2014.01.007 ↗
19. Wetting: statics and dynamics10.1103/RevModPhys.57.827 ↗
20. Reactive wetting of tin/steel and tin/aluminum at 350-450oC10.1016/j.jallcom.2017.05.036 ↗
21. Effect of processing parameters on the formation of Cf/LAS composites/AgCuTi/TC4 brazed joint10.1016/j.matchar.2016.09.014 ↗
22. Interfacial microstructure and performance of nano-diamond film/Ti-6Al-4V joint brazed with AgCuTi alloy10.1016/j.diamond.2016.05.011 ↗
23. Microstructure and interfacial reactions of vacuum brazing titanium alloy to stainless steel using an AgCuTi filler metal10.1016/j.matchar.2008.03.014 ↗
24. Dissolution of TiAl alloy during high temperature brazing10.1007/s10853-013-7315-8 ↗
25. Wettability of SnCuNi-xEu solders and mechanical properties of solder joints10.1016/S1002-0721(14)60201-5 ↗
26. Wetting mechanism of AgCuTi on heterogeneous surface of Diamond/Cu composites10.1016/j.surfcoat.2017.05.012 ↗
27. Spreading kinetics of liquid solders over an intermetallic solid surface. Part 2: lead-free solders10.1007/s11664-009-0870-8 ↗
28. The Ag-Ti (Silver-Titanium) system10.1007/BF02884876 ↗
29. On the existence of the β→α m transformation in the alloy systems Ti-Ag, Ti-Au, and Ti-Si10.1007/BF02646561 ↗
30. Mechanical properties and microstructures of dental cast Ti-Ag and Ti-Cu alloys10.4012/dmj.21.270 ↗
31. Fabrication of Ti–Nb–Ag alloy via powder metallurgy for biomedical applications10.1016/j.matdes.2013.11.066 ↗
32. Wetting kinetics of eutectic lead and lead-free solders: spreading over the Cu surface10.1007/s11664-008-0590-5 ↗
33. Non-reactive versus dissolutive wetting of Ag-Cu alloys on Cu substrates10.1007/s10853-009-3924-7 ↗
34. Wetting behaviour of Zn-Al filler metal on a stainless steel substrate10.1080/13621718.2017.1314657 ↗
35. The initial stages of oxidation of γ-TiAl: an X-ray photoelectron study10.1016/S0040-6090(02)00551-5 ↗
36. Anisotropic spreading of liquid metal on a rough intermetallic surface10.2298/TAM1104365L ↗
37. The spreading of silicone oil drops on horizontal surfaces10.1088/0022-3727/12/9/009 ↗
38. Reactive wetting of AgCuTi filler metal on the TiAl-based alloy substrate10.1016/j.apsusc.2012.07.047 ↗
39. Effects of roughness on the wettability of high temperature wetting system10.1016/j.surfcoat.2015.12.092 ↗
40. Segregation to interfaces10.1179/imr.1977.22.1.262 ↗
41. Silver segregation to θ′(Al2Cu)-Al interfaces in Al-Cu-Ag alloys10.1016/j.actamat.2012.07.039 ↗
42. Structure determination of multilayer silicene grown on Ag (111) films by electron diffraction: evidence for Ag segregation at the surface10.1103/PhysRevB.89.241403 ↗
43. Segregation effects in Ag-Si composites10.1016/0167-577X(94)00268-1 ↗
44. Irregular phenomenon induced by Ag atomic segregation during the heating process of Ag-Pd cluster10.1088/1674-1056/19/11/113604 ↗
45. Bulk and surface properties of liquid Ag–X (X= Ti, Hf) compound forming alloys10.1016/j.susc.2005.06.022 ↗
46. Surface and transport properties of Ag–Cu liquid alloys10.1016/j.susc.2004.12.009 ↗
47. Elastic moduli of cast Ti–Au, Ti–Ag, and Ti–Cu alloys10.1016/j.dental.2005.05.015 ↗
48. Wear and corrosion behaviors of Ti6Al4V alloy biomedical materials by silver plasma immersion ion implantation process10.1016/j.tsf.2012.02.046 ↗
49. Motions of droplets on solid surfaces induced by chemical or thermal gradients10.1021/la00086a025 ↗
50. Analysis of the effects of Marangoni stresses on the microflow in an evaporating sessile droplet10.1021/la0475270 ↗
51. Controlled uniform coating from the interplay of Marangoni flows and surface-adsorbed macromolecules10.1103/PhysRevLett.116.124501 ↗
52. The marangoni effects10.1038/187186a0 ↗
53. On the effect of Marangoni flow on evaporation rates of heated water drops10.1021/la801294x ↗
54. Self-propulsion of pure water droplets by spontaneous marangoni-stress-driven motion10.1103/PhysRevLett.113.248302 ↗
55. Self-propelled motion of a droplet induced by Marangoni-driven spreading10.1103/PhysRevE.80.016303 ↗
56. Anomalous wetting of Ti-48 at.% Al-2 at.% Cr-2at.% Nb substrates by liquid copper10.1557/JMR.1999.0526 ↗
57. Wettability of preoxidised TiAl substrates by liquid aluminum, copper, and silver10.1179/026708301101509223 ↗
58. Oxidation protection of γ-TiAl-based alloys–A review10.1016/j.intermet.2014.08.002 ↗
59. Al2O3–ZrO2–Pt composite coatings prepared by cathode plasma electrolytic deposition on the TiAl alloy10.1016/j.surfcoat.2015.10.050 ↗
60. Effects of Nb addition on oxidation behavior of TiAl10.1016/0966-9795(95)94254-C ↗
61. The initial stages of oxidation of γ-TiAl: an X-ray photoelectron study10.1016/S0040-6090(02)00551-5 ↗
62. The role of intermetallics in wetting in metallic systems10.1016/S1359-6462(01)01181-2 ↗
63. Reactive wetting of tin/steel and tin/aluminum at 350-450oC10.1016/j.jallcom.2017.05.036 ↗