journal article·2016-06

Effect of massive spalling on mechanical strength of solder joints in Pb-free solder reflowed on Co-based surface finishes

Hao Chen, Yi-Ling Tsai, Yu-Ting Chang, Albert T. Wu

Publisher page

Abstract

Abstract This study investigated the effect of massive spalling of intermetallic compounds (IMCs) on the microstructural evolution and mechanical properties of solder joints after multiple reflows. SAC305 solder was reflowed on substrates with four Co-based surface finishes: electroless Co (EC), electroless Co/immersion Au (ECIG), electroless Co/electroless Pd (ECEP), and electroless Co/electroless Pd/immersion Au (ECEPIG). CoSn 3 was the main intermetallic compound (IMC) that formed in the systems, and it massively spalled in the systems with Pd and high P content. Systems with massive spalling have a high shear strength and low shear height owing to solid solution strengthening. Due to strain hardening, high shear velocity caused high strength in all systems. Massive spalling of CoSn 3 transformed the failure mode from brittle to ductile and enhanced the shear strength of the joints.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Intermetallics and Advanced Alloy Properties · 3D IC and TSV technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Tin–lead (SnPb) solder reaction in flip chip technology10.1016/S0927-796X(01)00029-8 ↗
2. Solder reaction-assisted crystallization of electroless Ni–P under bump metallization in low cost flip chip technology10.1063/1.370627 ↗
3. Influence of phosphorus content on the interfacial microstructure between Sn–3.5Ag solder and electroless Ni–P metallization on Cu substrate10.1109/TADVP.2006.879420 ↗
4. Interconnecting to aluminum- and copper-based semiconductors (electroless-nickel/gold for solder bumping and wire bonding10.1016/S0026-2714(01)00236-0 ↗
5. The root causes of the “black pad” phenomenon and avoidance tactics10.1007/s11837-008-0074-3 ↗
6. The root cause of black pad failure of solder joints with electroless Ni/immersion gold plating10.1007/s11837-006-0187-5 ↗
7. Interfacial reaction and elemental redistribution in Sn3.0Ag.05Cu-xPd/immersion Au/electroless Ni solder joints after aging10.1016/j.mseb.2011.12.011 ↗
8. The influence of Pd on growth behavior of a quaternary (Cu,Ni,Pd)6Sn5 compound in Sn–3.0Ag–.05Cu/Au/Pd/Ni–P solder joint during a liquid state reaction10.1007/s10853-012-6807-2 ↗
9. Evaluation of mechanical properties of low-Ag ball grid array solder joints using a high-speed ball shear test10.1016/j.jallcom.2013.11.199 ↗
10. Micro void growth in NiSnP layer between (Cu,Ni)6Sn5 intermetallic compound and Ni3P by higher reflow temperature and multiple reflow10.1007/s10854-010-0072-4 ↗
11. Sn/Co solid/solid interfacial reactions10.1016/j.intermet.2007.12.017 ↗
12. The interfacial reaction between Sn–Ag alloys and Co substrate10.1016/j.msea.2006.11.117 ↗
13. Phase equilibria of the ternary Sn–Pb–Co system at 250 °C and interfacial reactions of Co with Sn–Pb alloys10.1007/s11664-015-3950-y ↗
14. Strong effects of minor Ga addition on liquid-state Sn–Ga/Co interfacial reactions10.1016/j.jallcom.2015.07.228 ↗
15. Electroless Co–P for diffusion barrier in Pb-free soldering10.1016/j.electacta.2004.10.098 ↗
16. The nanoindentation characteristics of Cu6Sn5, Cu3Sn, and Ni3Sn4 intermetallic compounds in the solder bump10.1007/s11664-004-0111-0 ↗
17. Nanohardness study of CoSn2 intermetallic layers formed between Co UBM and Sn flip-chip solder joints
18. Mechanical properties of intermetallic compounds in electrodeposited multilayered thin film at small scale by nanoindentation10.1016/j.matlet.2015.01.127 ↗
19. Comparative study of ENIG and ENEPIG as surface finishes for a Sn–Ag–Cu solder joint10.1007/s11664-011-1686-x ↗
20. Interfacial reaction and intermetallic compound formation of Sn–1Ag/ENIG and Sn–1Ag/ENEPIG solder joints10.1016/j.jallcom.2014.11.208 ↗
21. Massive spalling and morphological change of intermetallic compound affected by adding Pd in Co-based surface finishes10.1016/j.jallcom.2013.05.109 ↗
22. Spalling of Cu3Sn intermetallics in high-lead 95Pb5Sn solder bumps on Cu under bump metallization during solid-state annealing10.1063/1.1739530 ↗
23. Massive spalling of intermetallic compounds in solder-substrate reactions due to limited supply of the active element10.1063/1.2717564 ↗
24. Spalling of Cu6Sn5 spheroids in the soldering reaction of eutectic SnPb on Cr/Cu/Au thin films10.1063/1.363728 ↗
25. Abnormal spalling phenomena in the Sn–0.7Cu/Au/Ni/SUS304 interfacial reactions10.1557/jmr.2010.0305 ↗
26. Correlation between chemical reaction and brittle fracture found in electroless Ni(P)/immersion gold–solder interconnection10.1557/JMR.2005.0246 ↗
27. Direct correlation between mechanical failure and metallurgical reaction in flip chip solder joints10.1063/1.369779 ↗
28. Prevention of spalling by the self-formed reaction barrier layer on controlled collapse chip connections under bump metallization10.1007/s11664-003-0251-7 ↗
29. Effects of microstructural evolution and intermetallic layer growth on shear strength of ball-grid-array Sn–Cu solder joints10.1007/s11664-001-0119-7 ↗
30. High-speed shear test for low alpha Sn–1.0%Ag–0.5%Cu (SAC–105) solder ball of sub-100-μm dimension for wafer level packaging10.1109/TCPMT.2012.2230688 ↗
31. Failure behavior of BGA solder joints under various loading conditions of high-speed shear test10.1007/s10854-008-9588-2 ↗
32. Reliability of Sn–Pb solder joints with Cu and Co–P surface finishes under thermal cycling
33. IMC growth and shear strength of Sn–Ag–Cu/Co–P ball grid array solder joints under thermal cycling10.1007/s10854-014-2489-7 ↗
34. Dewetting of molten Sn on Au/Cu/Cr thin-film metallization10.1063/1.117855 ↗
35. The local nominal composition-useful concept for microjoining and interconnection applications10.1016/S1359-6462(97)00290-X ↗
36. Advances in lead-free electronics soldering10.1016/S1359-0286(00)00036-X ↗
37. Phase transformation of the phosphorus-rich layer in SnAgCu/Ni–P solder joints10.1016/j.scriptamat.2006.01.006 ↗
38. Diffusion barrier characteristics of electroless Co(W,P) thin films to lead-free SnAgCu solder10.1149/2.004111jes ↗
39. An investigation of diffusion barrier characteristics of an electroless Co(W,P) layer to lead-free SnBi solder10.1007/s11664-010-1488-6 ↗
40. Composition microstructure and magnetic properties of electroless-plated thin Co–P films10.1016/S0257-8972(99)00161-9 ↗
41. Interfacial reaction between Sn–Ag–Cu solder and Co–P films with various microstructures
42. Influence of the P content on phase formation in the interfacial reactions between Sn and electroless Co(P) metallization on Cu substrate10.1016/j.jallcom.2014.09.017 ↗
43. Reactions of Sn–4.0Ag–0.5Cu on Cu and electroless Ni substrate in premelting soldering process10.1007/s11664-013-2582-3 ↗
44. Interfacial reactions in the Sb–Sn/(Cu, Ni) systems: wetting experiments10.1016/j.matchemphys.2012.09.028 ↗
45. Effect of displacement rate on ball shear properties for Sn–37Pb and Sn–3.5Ag BGA solder joints during isothermal aging10.1016/j.microrel.2006.09.043 ↗
46. Influence of palladium thickness on the soldering reactions between Sn–3Ag–0.5Cu and Au/Pd(P)/Ni(P) surface finish10.1007/s11664-010-1351-9 ↗