journal article·2018-05

Fabrication of alumina-titanium composites by spark plasma sintering and their mechanical properties

Tomoyuki Fujii, Keiichiro Tohgo, Masahiro Iwao, Yoshinobu Shimamura

Publisher page

Abstract

Abstract Alumina (Al2O3) - titanium (Ti) composites were fabricated by the spark plasma sintering (SPS) technique to produce biocompatible materials with superior mechanical properties. To fabricate the composites, powders of Al2O3 and Ti hydride (TiH2) were used as raw materials because it was reported that the use of TiH2 powder enhances the sinterability of Ti phase in composites, compared with the use of Ti powder. The composites made of Al2O3 and Ti powders were also fabricated, and the effects of raw materials on their sintering state and mechanical properties were discussed. Phase constituents were identified by the X-ray diffraction analysis, and it revealed that the Al2O3-Ti composites without any reaction phases were fabricated, irrespective of raw materials. Then, three-point bending tests and hardness tests were conducted, and the bending strength and hardness of the composites made of Al2O3 and TiH2 improved, compared with the composites made of Al2O3 and Ti. Therefore, the use of TiH2 as a raw material was effective to fabricate Al2O3-Ti composites with high strength and hardness.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Bone Tissue Engineering Materials · Titanium Alloys Microstructure and Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Metallic implant biomaterials10.1016/j.mser.2014.10.001 ↗
2. Implant biomaterials: a comprehensive review10.12998/wjcc.v3.i1.52 ↗
3. Sintering effect on mechanical properties of composites of bovine derived hydroxyapatite (BHA) with titanium10.4028/www.scientific.net/KEM.309-311.359 ↗
4. In vitro bioactivity of a biocomposite fabricated from HA and Ti powders by powder metallurgy method10.1016/S0142-9612(01)00419-7 ↗
5. Toughening mechanisms in iron-containing hydroxyapatite/titanium composites10.1016/j.biomaterials.2009.11.046 ↗
6. Fabrication and strength evaluation of biocompatible ceramic-metal composite materials10.1299/jmmp.4.1699 ↗
7. Processing and spark plasma sintering of zirconia/titanium cermets10.1016/j.ceramint.2013.02.029 ↗
8. Fabrication of PSZ-Ti composites by spark plasma sintering and their mechanical properties10.1016/j.msea.2014.10.062 ↗
9. Mechanical properties of zirconia-titanium composites
10. Effect of yttria-titanium shell-core structured powder on strength and ageing of zirconia/titanium composites10.1016/j.msea.2015.08.048 ↗
11. The formation of ZrO2-Ti composites by spark plasma sintering10.1007/s11106-017-9851-2 ↗
12. Reaction between titanium and zirconia powders during sintering at 1500 °C10.1111/j.1551-2916.2007.01708.x ↗
13. Processing, spark plasma sintering, and mechanical behavior of alumina/titanium composites10.1007/s10853-014-8095-5 ↗
14. Mechanical properties of Al2O3/Ti composites fabricated by spark plasma sintering10.1016/j.ceramint.2014.12.008 ↗
15. In vitro and in vivo evaluation of a new zirconia/niobium biocermet for hard tissue replacement10.1016/j.biomaterials.2015.10.058 ↗
16. Al2O3-Ti functionally graded material prepared by spark plasma sintering for orthopedic applications10.1016/j.jmbbm.2017.04.024 ↗
17. Hydroxyapatite-Ti functionally graded biomaterial fabricated by powder metallurgy
18. Experimental and numerical analysis of titanium/HA FGM for dental implantation
19. Fabrication of PSZ-Ti functionally graded materials by spark plasma sintering and its fracture toughness10.1016/j.msea.2016.11.091 ↗
20. Nano- and micro- indentation characterization of ZrO2/Ti functionally graded materials fabricated by spark plasma sintering
21. Consolidation behavior and mechanical properties of SiC with Al2O3 and Yb2O3 consolidated by SPS10.2497/jjspm.56.788 ↗
22. Intense atomic oxygen emission from incandescent zirconia10.1021/jp902159p ↗
23. Oxygen solid solution hardening in titanium by heat treatment
24. Densification and microstructure of Al2O3-cBN composites prepared by spark plasma sintering10.2109/jcersj2.116.744 ↗
25. Alumina-based nanocomposites consolidated by spark plasma sintering10.1016/S1359-6462(02)00191-4 ↗
26. Effect of TiO2 addition on the properties of Al2O3-ZrO2 composites prepared by spark plasma sintering10.4303/bda/D110147 ↗
27. Fabrication of powder metallurgy pure Ti material by using thermal decomposition of TiH2
28. Role of hydrogen in the process of sintering of titanium powders10.1007/s11003-012-9440-y ↗
29. Bulk titanium for structural and biomedical applications obtaining by spark plasma sintering (SPS) from titanium hydride powder10.1007/s10973-012-2824-2 ↗
30. Comparison of sintering of titanium and titanium hydride powders10.1179/003258909X12450768327063 ↗
31. Preparation of strong and ductile pure titanium via two-step rapid sintering of TiH2 powder10.1016/j.jallcom.2016.05.020 ↗
32. NIH Image to Image J: 25 years of image analysis10.1038/nmeth.2089 ↗
33. PC-PDF, Powder Diffraction File: International Centre for Diffraction Data (JCPDS/ICDD), Newton Square, (1999, 2000).
34. Fabrication of high strength pure titanium by mechanical milling and spark plasma sintering and its properties10.2464/jilm.59.659 ↗
35. Hydrogen embrittlement in titanium and its alloys10.3323/jcorr.60.248 ↗
36. Jewett · 1973