Cu gettering by phosphorus-doped emitters in p-type silicon: Effect on light-induced degradation
Source abstract
Abstract
The presence of copper (Cu) contamination is known to cause relevant light-induced degradation (Cu-LID) effects in p-type silicon. Due to its high diffusivity, Cu is generally regarded as a relatively benign impurity, which can be readily relocated during device fabrication from the wafer bulk, i.e. the region affected by Cu-LID, to the surface phosphorus-doped emitter. This contribution examines in detail the impact of gettering by industrially relevant phosphorus layers on the strength of Cu-LID effects. We find that phosphorus gettering does not always prevent the occurrence of Cu-LID. Specifically, air-cooling after an isothermal anneal at 800°C results in only weak impurity segregation to the phosphorus-doped layer, which turns out to be insufficient for effectively mitigating Cu-LID effects. Furthermore, we show that the gettering efficiency can be enhanced through the addition of a slow cooling ramp (-4°C/min) between 800°C and 600°C, resulting in the nearly complete disappearance of Cu-LID effects.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and devices · Thin-Film Transistor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Electronics and Nanoengineering, Aalto University , Tietotie 3, 02150 Espoo, Finland
Funding
Tiina and Antti Herlinin Foundation · Suomen Kulttuurirahasto · Sähkötekniikan Korkeakoulu, Aalto-yliopisto · Alfred Kordelinin Säätiö · EC | FP7 | FP7 Ideas: European Research Council
References (29)
Show source-provided references
1. Appl. Phys. Lett. · 2016 · 108 · 20210410.1063/1.4950765 ↗
2. J. Appl. Phys. · 2003 · 94 · 655210.1063/1.1618912 ↗
3. ECS Trans. · 2008 · 179
4. Energy Procedia · 2013 · 38 · 53110.1016/j.egypro.2013.07.313 ↗
5. Sol. Energy · 2016 · 125 · 19810.1016/j.solener.2015.12.004 ↗
6. Sol. Energy Mater. Sol. Cells · 2016 · 147 · 11510.1016/j.solmat.2015.11.047 ↗
7. J. Appl. Phys. · 2017 · 121 · 19570310.1063/1.4983454 ↗
8. J. Appl. Phys. · 2017 · 121 · 19570410.1063/1.4983455 ↗
9. Phys. Status Solidi · 2017 · 14 · 170010310.1002/pssc.201700103 ↗
10. Appl. Phys. Lett. · 2014 · 105 · 18210810.1063/1.4901533 ↗
11. J. Electrochem. Soc. · 2002 · 149 · G2110.1149/1.1421348 ↗
12. Solid State Phenom · 2008 · 131–133 · 39910.4028/www.scientific.net/ssp.131-133.399 ↗
13. SEMI PV Group · 2016
14. Sol. Cells · 1984 · 11 · 110.1016/0379-6787(84)90114-5 ↗
15. Sol. Energy Mater. Sol. Cells · 2012 · 105 · 13710.1016/j.solmat.2012.06.007 ↗
16. J. Appl. Phys. · 2002 · 91 · 247310.1063/1.1432476 ↗
17. IEEE Trans. Electron Devices · 1990 · 37 · 36510.1109/16.46368 ↗
18. Phys. Status Solidi · 2017 · 214
19. Phys. Status Solidi · 2014 · 11 · 169710.1002/pssc.201400036 ↗
20. 2016 · 0678
21. Meas. Sci. Technol · 2001 · 12 · R1610.1088/0957-0233/12/3/202 ↗
22. Appl. Phys. Lett. · 2015 · 107 · 5210110.1063/1.4927838 ↗
23. J. Electrochem. Soc. · 2003 · 150 · G79010.1149/1.1624845 ↗
24. Appl. Phys. Lett. · 2005 · 87 · 3210910.1063/1.1999008 ↗
25. AIP Adv. · 2016 · 6 · 3511910.1063/1.4944839 ↗
26. Energy Procedia · 2016 · 92 · 80810.1016/j.egypro.2016.07.073 ↗
27. Phys. Rev. B · 1990 · 41 · 577010.1103/physrevb.41.5770 ↗
28. Phys. Rev. Lett. · 1998 · 81 · 124310.1103/physrevlett.81.1243 ↗
29. Appl. Phys. A Mater. Sci. Process · 2002 · 75 · 52510.1007/s003390101021 ↗