Synthesis of nano TiB2 particles in copper matrix by in situ reaction of double-beam melts
Source abstract
Abstract
Abstract Bulk copper alloys with nano TiB2 particles were prepared by a new technology that combining in situ reaction with rapid solidification. Appropriate reactor shape and procedure parameters are as follows: S0/(S1 + S2) = 0.8–1.2, L0/D0 = 10–15, θ = 60–90°, melt temperature 1350–1450 °C, air pressure 0.2–0.3 MPa. A special water-cooled copper mold can satisfy the need of rapid solidifying Cu–TiB2 alloy melt. The average size of TiB2 particle in the copper matrix synthesized by using optimal parameters is about 20 nm.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced materials and composites · Metallic Glasses and Amorphous Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. Weertman · 2002 · 397
2. Choy · Prog. Mater. Sci. · 2003 · 48 · 5710.1016/S0079-6425(01)00009-3 ↗
3. Popov · J. Alloys .Compd. · 2007 · 434–435 · 68910.1016/j.jallcom.2006.08.337 ↗
4. Hibbard · U. Erb. Scripta Mater. · 2002 · 47 · 8310.1016/S1359-6462(02)00098-2 ↗
5. Ju · J. Alloys Compd. · 2006 · 425 · 41110.1016/j.jallcom.2006.01.064 ↗
6. Vasiliev · Scripta Mater. · 2005 · 53 · 46910.1016/j.scriptamat.2005.04.041 ↗
7. Lee · Scripta Mater. · 2001 · 44 · 213710.1016/S1359-6462(01)00764-3 ↗
8. Shi · Appl. Surf. Sci. · 1998 · 134 · 10310.1016/S0169-4332(98)00223-2 ↗
9. Tjong · Mater. Sci. Eng. · 2000 · 29 · 4910.1016/S0927-796X(00)00024-3 ↗
10. Weber · ZAMM · 1936 · 16 · 35510.1002/zamm.19360160611 ↗
11. Nakae · Key Eng. Mater. · 1997 · 127–131 · 50310.4028/www.scientific.net/KEM.127-131.503 ↗
12. Shangguan · Metall. Trans. · 1992 · 23 · 66910.1007/BF02801184 ↗