Hydrogen storage properties of LiBH4 destabilized by SrH2
Source abstract
Abstract
Abstract In this work, we have succeeded in destabilizing LiBH4 by the addition of SrH2, via the reaction 6LiBH4 + SrH2 → SrB6 + 6LiH + 10H2 with a theoretical hydrogen capacity of 9.1 wt.%. According to the van’t Hoff and Arrhenius equations, the dehydrogenation enthalpy change and activation energy for the LiBH4/SrH2 system were experimentally determined to be 48 kJ/mol H2 and 64 kJ/mol, respectively. Both are remarkably reduced in comparison with the pristine LiBH4, which is responsible for the improved dehydrogenation property of the LiBH4/SrH2 system. The dehydrogenated products SrB6 + 6LiH can be rehydrogenated to form LiBH4 and LiSrH3 at 723 K under an initial hydrogen pressure of 8.0 MPa.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen Storage and Materials · Hybrid Renewable Energy Systems · Superconductivity in MgB2 and Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Li · Energy · 2011 · 4 · 18510.3390/en4010185 ↗
2. Li · Int. J. Hydrogen Energy · 2011 · 36 · 1451210.1016/j.ijhydene.2011.08.030 ↗
3. Bouhadda · J. Alloys Compd. · 2012 · 534 · 2010.1016/j.jallcom.2012.04.060 ↗
4. Mauron · J. Phys. Chem. B · 2008 · 112 · 90610.1021/jp077572r ↗
5. Züttel · J. Alloys Compd. · 2003 · 356–357 · 51510.1016/S0925-8388(02)01253-7 ↗
6. Vajo · J. Phys. Chem. B · 2005 · 109 · 371910.1021/jp040769o ↗
7. Pinkerton · J. Alloys Compd. · 2008 · 464 · L110.1016/j.jallcom.2007.09.125 ↗
8. Mao · J. Alloys Compd. · 2011 · 509 · 501210.1016/j.jallcom.2011.02.004 ↗
9. Jiang · J. Alloys Compd. · 2011 · 509 · 905510.1016/j.jallcom.2011.05.087 ↗
10. Zhang · Int. J. Hydrogen Energy · 2011 · 36 · 973310.1016/j.ijhydene.2011.05.035 ↗
11. Meggouh · J. Phys. Chem. C · 2011 · 115 · 2205410.1021/jp208009v ↗
12. Liu · Chem. Commun. · 2011 · 47 · 574110.1039/c1cc11238d ↗
13. Gennari · Int. J. Hydrogen Energy · 2011 · 36 · 1523110.1016/j.ijhydene.2011.08.059 ↗
14. Shim · J. Alloys Compd. · 2012 · 510 · L910.1016/j.jallcom.2011.09.005 ↗
15. Wu · J. Alloys Compd. · 2012 · 517 · 12710.1016/j.jallcom.2011.12.054 ↗
16. Zhou · J. Phys. Chem. C · 2012 · 116 · 158810.1021/jp2101573 ↗
17. Shao · J. Mater. Chem. · 2012 · 22 · 2076410.1039/c2jm33374k ↗
18. Luo · Int. J. Hydrogen Energy · 2012 · 37 · 1344610.1016/j.ijhydene.2012.06.114 ↗
19. Deng · Int. J. Hydrogen Energy · 2012 · 37 · 673310.1016/j.ijhydene.2012.01.094 ↗
20. Chen · Int. J. Hydrogen Energy · 2012 · 37 · 1242510.1016/j.ijhydene.2012.06.057 ↗
21. Lim · Scripta Mater. · 2008 · 59 · 125110.1016/j.scriptamat.2008.08.037 ↗
22. Zhou · Dalton Trans. · 2012 · 41 · 1098010.1039/c2dt30945a ↗
23. Jiang · J. Alloys Compd. · 2012 · 539 · 10310.1016/j.jallcom.2012.06.039 ↗
24. Liu · J. Alloys Compd. · 2012 · 514 · 10310.1016/j.jallcom.2011.11.009 ↗
25. Bösenberg · Acta Mater. · 2007 · 55 · 395110.1016/j.actamat.2007.03.010 ↗
26. Yuan · J. Phys. Chem. C · 2011 · 115 · 706710.1021/jp200057v ↗
27. Walker · 2008
28. Zhang · J. Phys. Chem. C · 2009 · 113 · 1842410.1021/jp903967y ↗
29. Li · Acta Mater. · 2011 · 59 · 182910.1016/j.actamat.2010.11.049 ↗
30. Gross · J. Phys. Chem. C · 2008 · 112 · 565110.1021/jp711066t ↗
31. Kato · Phys. Chem. Chem. Phys. · 2010 · 12 · 1095010.1039/c000299b ↗
32. Chen · J. Alloys Compd. · 2004 · 366 · L610.1016/S0925-8388(03)00735-7 ↗