Effect of Ni addition on the contact resistance of Ag-WC electrical contacts

Nachiketa Ray, Bernd Kempf, Timo Mützel, Frank Heringhaus, Ludo Froyen, Kim Vanmeensel, Jef Vleugels

Publisher page

Abstract

Abstract In this work, Ni was used as an additive in Ag-WC (60–40 wt.%) metal matrix composites employed as electrical contacts. Increasing the Ni content from 1 to 3 wt.% resulted in an increase in the mean electrical contact resistance ( R c ) from ∼2 to ∼3 mΩ. However, further addition of Ni up to 10 wt.% resulted in the formation of a silver layer on the contact surface after switching, which strongly reduced the R c from ∼3 to ∼1.5 mΩ. The influence of Ni addition on the microstructural changes in the contact material was investigated and the mechanism for the transfer of silver from the bulk composite material to the surface as a consequence of thermal cycling during switching was elucidated.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Electrical Contact Performance and Analysis · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Electro-mechanical properties of composite materials for high-current contact applications10.1088/0022-3727/47/12/125501 ↗
2. Microstructure, hardness and electrical properties of silver-based refractory contact materials10.1016/S0261-3069(03)00125-0 ↗
3. Development of Contact Material Solutions for Low-Voltage Circuit Breaker Applications (2)
4. Silver tungsten carbide contacts for circuit breaker applications
5. A Comparison of Ag/W,Ag/WC, and Ag/Mo Electrical Contacts10.1109/TCHMT.1984.1136333 ↗
6. The development of silver-based cadmium-free contact materials10.1109/33.19007 ↗
7. Arc erosion tests and study of surface of Ag-WC contacts after arc switching operations
8. Erosion and resistance characteristics of AgW and AgC contacts at high current arcing in air
9. Effective erosion rates for selected contact materials in low-voltage contactors, IEEE Transactions on Components10.1109/95.390312 ↗
10. Surface Degradation of Ag/W Circuit Breaker Contacts During Standardized UL Testing
11. Microstructure effects on dynamic welding of Ag/W contacts, IEEE Transactions on Components10.1109/33.2963 ↗
12. On the application of W/Cu materials in the fields of power engineering and plasma technology, IEEE Transactions on Components10.1109/33.76502 ↗
13. The effects of nickel on the switching performance of silver-tungsten-based contacts
14. The effect of nickel additions on the performance of tungsten-silver materials
15. Effects of nickel addition on properties of Ag–W electrical contact materials10.1179/003258901666202 ↗
16. The effect of cobalt addition on sintering and microstructural behaviour of silver–tungsten (Ag–W) composite10.1007/s10973-009-0152-y ↗
17. Effect of WC particle size and Ag volume fraction on electrical contact resistance and thermal conductivity of Ag–WC contact materials10.1016/j.matdes.2015.07.006 ↗
18. The effect of microstructure on the electrical performance of Ag-WC-C contact materials
19. Activated sintering of nickel-doped tungsten: approach by grain boundary structural transition10.1016/S1359-6462(99)00344-9 ↗
20. Diffusion parameters of grain-growth inhibitors in WC based hardmetals with Co, Fe/Ni and Fe/Co/Ni binder alloys10.1016/j.ijrmhm.2014.06.002 ↗
21. Cemented carbide phase diagrams: A review, Int10.1016/j.ijrmhm.2011.02.004 ↗
22. Materials science of cemented carbides—an overview10.1016/S0261-3069(01)00007-3 ↗
23. The wetting behaviour of silver on carbon, pure and carburized nickel, cobalt and molybdenum substrates10.1016/j.apsusc.2010.02.075 ↗
24. Witter · 1979
25. 1996
26. P.C. Wingert, Testing of the thermal-stress-cracking characteristics of silver-refractory contacts, 41st IEEE Holm Conference on Electrical Contacts, Montreal, Canada, 1995, pp. 338–345. doi:10.1109/HOLM.1995.482889.10.1109/HOLM.1995.482889 ↗
27. A Correlation of Material Toughness, Thermal Shock Resistance, and Microstructure of High Tungsten, Silver-Tungsten Composite Materials10.1109/TPHP.1975.1135028 ↗
28. An Electrical Arc Erosion Model Valid for High Current: Vaporization and Splash Erosion
29. Thermodynamic Assessments of the Ag-Ni Binary and Ag-Cu-Ni Ternary Systems10.1007/s11664-007-0315-1 ↗
30. Arc erosion behavior of Ag/Ni electrical contact materials10.1016/j.matdes.2015.06.142 ↗
31. Thin intergranular films and solid-state activated sintering in nickel-doped tungsten10.1016/j.actamat.2007.01.017 ↗
32. Experimental and First Principles Study of the Ni-Ti-W System10.4028/www.scientific.net/MSF.730-732.775 ↗
33. In situ formation of tungsten oxycarbide, tungsten carbide and tungsten nitride nanoparticles in micro- and mesoporous polymer-derived ceramics10.1039/c4ta01509f ↗
34. Ni-w (nickel-tungsten)
35. S.G.T.E. (sgte), Ni-W
36. Gustafson · 1985 · 1986