Enhanced thermoelectric performance of highly dense and fine-grained (Sr1−xGdx)TiO3−δ ceramics synthesized by sol–gel process and spark plasma sintering
Source abstract
Abstract
Abstract Highly dense and fine-grained (Sr1−xGdx)TiO3−δ ceramics (x = 0.05–0.12) were fabricated by a sol–gel process plus spark plasma sintering, and their thermoelectric properties were investigated from ∼300 K to 1100 K. The results show that the electrical resistivity of the (Sr1−xGdx)TiO3−δ ceramics decreases greatly while maintaining large absolute value of the Seebeck coefficient |S| upon Gd doping. As a result, a large power factor (PF) greater than 10 μW cm−1 K−2 is obtained in (Sr0.9Gd0.1)TiO3−δ in the temperature range from 400 K to 1000 K, and peak PF reaches 16 μW cm−1 K−2 at ∼570 K. Simultaneously, the lattice thermal conductivity κL reduces remarkably (e.g. κL decreases from 2.7 to 2.13 W m−1 K−1 at ∼1000 K). Owing to the large PF and low κL, a record value of figure of merit ZT = 0.37 is achieved at 1006 K for (Sr0.9Gd0.1)TiO3−δ, indicating that appropriate combinations of fine-grained microstructure with both high densities and proper doping as well as oxygen deficiency are essential to the effective enhancement of thermoelectric performance of STO-based ceramics.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Thermoelectric Materials and Devices · Phase Change Materials Research · Magnetic and transport properties of perovskites and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Zebarjadi · Adv. Mater. · 2013 · 25 · 157710.1002/adma.201204802 ↗
2. Li · J. Alloys Comp. · 2013 · 576 · 36910.1016/j.jallcom.2013.05.228 ↗
3. Li · J. Alloys Comp. · 2013 · 547 · 8610.1016/j.jallcom.2012.08.041 ↗
4. Koumoto · J. Am. Ceram. Soc. · 2013 · 96 · 110.1111/jace.12076 ↗
5. Wang · J. Alloys Comp. · 2013 · 554 · 25410.1016/j.jallcom.2012.11.107 ↗
6. Wang · J. Alloys Comp. · 2009 · 477 · 81710.1016/j.jallcom.2008.10.162 ↗
7. Li · Energy Environ. Sci. · 2012 · 5 · 854310.1039/c2ee22622g ↗
8. Han · J. Alloys Comp. · 2013 · 555 · 29110.1016/j.jallcom.2012.12.091 ↗
9. Ohta · Appl. Phys. Lett. · 2005 · 87 · 09210810.1063/1.2035889 ↗
10. Muta · J. Alloys Comp. · 2003 · 350 · 29210.1016/S0925-8388(02)00972-6 ↗
11. Liu · Appl. Phys. Lett. · 2009 · 95 · 16211010.1063/1.3254219 ↗
12. Liu · J. Alloys Comp. · 2010 · 492 · L5410.1016/j.jallcom.2009.11.165 ↗
13. Wang · J. Am. Ceram. Soc. · 2011 · 94 · 83810.1111/j.1551-2916.2010.04185.x ↗
14. Kovalevsky · J. Appl. Phys. · 2013 · 113 · 05370410.1063/1.4790307 ↗
15. Wang · Scr. Mater. · 2011 · 65 · 19010.1016/j.scriptamat.2011.03.037 ↗
16. Kikuchi · Scr. Mater. · 2010 · 63 · 40710.1016/j.scriptamat.2010.04.041 ↗
17. Shang · Solid State Sci. · 2010 · 12 · 134110.1016/j.solidstatesciences.2010.05.005 ↗
18. Abeles · Phys. Rev. · 1963 · 131 · 190610.1103/PhysRev.131.1906 ↗
19. Irvine · Ionics · 1996 · 2 · 21310.1007/BF02376024 ↗
20. Fang · J. Appl. Phys. · 2012 · 112 · 03411410.1063/1.4745876 ↗
21. Lee · J. Appl. Phys. · 2010 · 107 · 09430810.1063/1.3388076 ↗
22. Payne · J. Am. Ceram. Soc. · 1967 · 50 · 49110.1111/j.1151-2916.1967.tb15171.x ↗
23. Moos · J. Appl. Phys. · 1996 · 80 · 39310.1063/1.362796 ↗
24. Li · J. Power Sour. · 2007 · 166 · 4710.1016/j.jpowsour.2007.01.008 ↗
25. Capizzi · Phys. Rev. Lett. · 1970 · 25 · 129810.1103/PhysRevLett.25.1298 ↗
26. Onoda · J. Phys.: Condens. Matter · 2009 · 21 · 435603
27. Lee · Phys. Rev. B · 2009 · 79 · 13411010.1103/PhysRevB.79.134110 ↗
28. Fisher · Phys. Rev. B · 2000 · 61 · 47010.1103/PhysRevB.61.470 ↗
29. Kumar · J. Appl. Phys. · 2012 · 112 · 11410410.1063/1.4767840 ↗
30. Wang · Appl. Phys. Express · 2010 · 3 · 03110110.1143/APEX.3.031101 ↗
31. Yang · Acta Mater. · 2002 · 50 · 230910.1016/S1359-6454(02)00057-5 ↗
32. Ohta · J. Ceram. Soc. Jpn. · 2006 · 114 · 10210.2109/jcersj.114.102 ↗