High-impact polystyrene (HIPS) is widely used in household appliances, electronic equipment casings, packaging materials, and automotive parts due to its excellent dimensional stability, fluidity, electrical insulation, and rigidity. However, its high flammability and significant smoke emission during combustion limit its application in fire-sensitive environments. In this study, a synergistic intumescent flame retardant system composed of hollow cubic zinc hydroxystannate (H-ZHS), piperazine pyrophosphate (PAPP), and melamine polyphosphate (MPP) was developed to improve the fire safety of HIPS composites. Thermogravimetric analysis (TGA), limiting oxygen index (LOI), UL-94 vertical combustion, and cone calorimetry (CCT) were employed to evaluate the thermal stability, flame retardancy, and smoke suppression properties. The optimised composite (30 wt% total flame retardant loading with a PAPP/MPP mass ratio of 7:3 and 2 wt% H-ZHS) achieved a UL94-V0 rating (1.6 mm thickness) and an LOI of 34.3%. Compared to pure HIPS, the peak heat release rate (pHRR), total heat release (THR), and total smoke production (TSP) decreased by 74.1 ± 3.2%, 20.6 ± 1.8%, and 65.3%, respectively. The synergistic mechanism involved condensed-phase char formation catalysed by H-ZHS and gas-phase flame inhibition by non-flammable gases (e.g. NH 3 ) from PAPP/MPP decomposition. This work provides a practical strategy for developing halogen-free flame-retardant HIPS composites with balanced fire safety and mechanical properties.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Flame retardant materials and properties · Fire dynamics and safety research · Polymer composites and self-healing

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Faculty of Chemical Engineering, Kunming University of Science and Technology

The International Joint Laboratory for Sustainable Polymers of Yunnan Province, Faculty of Chemical Engineering, Kunming University of Science and Technology, Kunming, China

The Higher Educational Key Laboratory for Phosphorus Chemical Engineering of Yunnan Province, Faculty of Chemical Engineering, Kunming University of Science and Technology, Kunming, China

Yunnan Tin & Indium Laboratory, Kunming, China

Yunnan Tin New Material Company Limited, Kunming, China

Funding

The Major Science and Technology Special Project of Yunnan Province · The Science and Technology Plan Project of Yunnan Tin Industry New Materials Company

References (39)

Show source-provided references
1. 10.1016/j.compscitech.2012.03.00610.1016/j.compscitech.2012.03.006 ↗
2. 10.1002/app.1130210.1002/app.11302 ↗
3. Juan L. Effect of multiwalled carbon nanotubes (MWNT) on the properties of high impact polystyrene (HIPS). J Nanomater 2018; 2018: 1–5.
4. 10.3390/polym1104061510.3390/polym11040615 ↗
5. Liu J, Zhang Y, Peng S, et al. Fire property and charring behavior of high impact polystyrene containing expandable graphite and microencapsulated red phosphorus. Polym Degrad Stab 2015; 121: 261–270.
6. 10.1007/s13726-015-0394-410.1007/s13726-015-0394-4 ↗
7. 10.1002/macp.20040025510.1002/macp.200400255 ↗
8. 10.1016/j.polymdegradstab.2006.10.00610.1016/j.polymdegradstab.2006.10.006 ↗
9. 10.1002/fam.265010.1002/fam.2650 ↗
10. Liu J, Guo Y, Zhang Y, et al. Thermal conduction and fire property of glass fiber-reinforced high impact polystyrene/magnesium hydroxide/microencapsulated red phosphorus composite. Polym Degrad Stab 2016; 129: 180–191.
11. Hoffendahl C, Duquesne S, Fontaine G, et al. Decomposition mechanism of fire retarded ethylene vinyl acetate elastomer (EVA) containing aluminum trihydroxide and melamine. Polym Degrad Stab 2015; 113: 168–179.
12. Guo J, Xu F, Guo Y, et al. Synergistic flame-retardant effect of nano al(OH)3 phosphorus hybrid polymer/polystyrene composite. Mater Rev 2018; 32: 2497–2502. 2512.
13. 10.1002/fam.275810.1002/fam.2758 ↗
14. Liu J, Yu Z, Shi Y, et al. A preliminary study on the thermal degradation behavior and flame retardancy of high impact polystyrene/magnesium hydroxide/microencapsulated red phosphorus composite with a gradient structure. Polym Degrad Stab 2014; 105: 21–30.
15. 10.1016/j.polymdegradstab.2010.08.02210.1016/j.polymdegradstab.2010.08.022 ↗
16. 10.1002/pc.2399810.1002/pc.23998 ↗
17. 10.1007/s10973-016-6070-x10.1007/s10973-016-6070-x ↗
18. 10.1007/s10973-016-5484-910.1007/s10973-016-5484-9 ↗
19. 10.1007/s13726-016-0453-510.1007/s13726-016-0453-5 ↗
20. 10.3390/polym1104061510.3390/polym11040615 ↗
21. Juan L. Multiwalled carbon nanotubes reinforced polypropylene composite material. J Nanomater 2017; 2017: 1–5.
22. 10.1016/j.matpr.2015.08.02910.1016/j.matpr.2015.08.029 ↗
23. 10.1007/s10118-018-2036-810.1007/s10118-018-2036-8 ↗
24. 10.1007/s10973-016-5391-010.1007/s10973-016-5391-0 ↗
25. 10.3390/polym1418372210.3390/polym14183722 ↗
26. 10.1016/j.polymdegradstab.2007.05.00710.1016/j.polymdegradstab.2007.05.007 ↗
27. 10.1016/j.polymdegradstab.2020.10947710.1016/j.polymdegradstab.2020.109477 ↗
28. 10.1002/pat.499610.1002/pat.4996 ↗
29. 10.1080/14658011.2019.158220010.1080/14658011.2019.1582200 ↗
30. 10.1016/j.tca.2015.06.00410.1016/j.tca.2015.06.004 ↗
31. 10.1002/app.5248810.1002/app.52488 ↗
32. 10.3390/polym1211244210.3390/polym12112442 ↗
33. 10.1016/j.polymdegradstab.2012.08.01710.1016/j.polymdegradstab.2012.08.017 ↗
34. 10.1016/j.porgcoat.2023.10804110.1016/j.porgcoat.2023.108041 ↗
35. 10.1016/j.inoche.2022.10950710.1016/j.inoche.2022.109507 ↗
36. 10.1016/j.cej.2021.13033810.1016/j.cej.2021.130338 ↗
37. 10.1016/j.polymdegradstab.2022.10992710.1016/j.polymdegradstab.2022.109927 ↗
38. 10.1016/j.compositesa.2022.10741710.1016/j.compositesa.2022.107417 ↗
39. 10.1007/s42823-023-00663-410.1007/s42823-023-00663-4 ↗