journal article·2017-07

Microstructure and mechanical properties of the as-cast and warm rolled Mg-9Li-x(Al-Si)-yTi alloys with x = 1, 3, 5 and y = 0.05 wt.%

JeongTae Kim, Hae Joon Jeong, Yeabin Moon, Ki Buem Kim, Hyeon Taech Son, Changwoo Jeon, Jae Won Sim, Sudong Moon, Jin Man Park

Publisher page

Abstract

Abstract The as-cast Mg-9Li alloys with difference Al-Si addition were fabricated using induction casting method under the argon atmosphere and then warm rolling process was performed at 473 K. The Al-Si addition to Mg-9Li alloy leads to the formation of Mg2Si intermetallic compounds and microstructural evolutions such as increased volume fraction of α-Mg phases and changed morphology of α-Mg primary phase on the as-cast specimens. Moreover, the addition of 0.05 wt.% Ti elements on Mg-9Li-3(Al-Si) alloy raised the further microstructural evolutions, e.g. volume fraction of α-Mg phases, which bring about change in the microstructure after warm rolling process. The effects of this micro alloying influences the formation of fine microstructure after warm rolling process, which is the main factor in determining the mechanical properties. With these microstructural evolutions, tensile strength was increased from 101.71 MPa to 247.41 MPa by the minor alloying and warm rolling process. Moreover, the remarkably enhanced strength of Mg-9Li-3(Al-Si) alloy was the results of the addition of 0.05 wt.% Ti from 247 MPa to 412 MPa. Furthermore, the warm press-forming tests were carried out at 523 K to evaluate the applicability of this novel alloy for commercial products.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Low temperature superplasticity of ECAE processed Mg-10%Li-1%Zn alloy10.2320/matertrans.43.2419 ↗
2. Mechanical and anisotropic behaviors of Mg–Li–Zn alloy thin sheets10.1016/j.matdes.2008.04.001 ↗
3. Yamamoto · Mater. Trans. · 2003 · 44 · 61910.2320/matertrans.44.619 ↗
4. Precipitation in Mg-(4-13)% Li-(4-5)% Zn ternary alloys10.1023/A:1013133521947 ↗
5. Okamoto · 2000
6. Mechanical properties and microstructure of new magnesium—lithium base alloys10.1016/S0921-5093(96)10460-3 ↗
7. Characterization of cast Mg–Li–Ca alloys10.1016/j.matchar.2004.12.001 ↗
8. Mechanical properties of Mg–Li–Cu–Y metallic glass composites10.1016/j.jallcom.2010.02.141 ↗
9. The influences of alloying additions and processing parameters on the rolling microstructures and textures of magnesium alloys10.1016/j.msea.2007.07.003 ↗
10. Development of lightweigh MgLiAl alloys with high specific strength10.1016/j.jallcom.2016.04.109 ↗
11. Microstructure and mechanical properties of Mg–xLi–3Al–1Sn–0.4 Mn alloys (x= 5, 8 and 11wt.%)10.1016/j.jallcom.2013.08.154 ↗
12. Microstructure evolution of Mg–14% Li–1% Al alloy during the process of equal channel angular pressing10.1016/j.msea.2007.01.108 ↗
13. Microstructure and mechanical properties of Mg-Li alloy with Ca addition10.1016/S1006-7191(06)62073-5 ↗
14. Influence of the combined addition of Y and Nd on the microstructure and mechanical properties of Mg–Li alloy10.1016/j.matdes.2013.12.057 ↗
15. Effects of adding Al–Si eutectic alloy and hot rolling on microstructures and mechanical behavior of Mg–8Li alloys10.1016/j.jallcom.2015.01.094 ↗
16. Microstructure and mechanical properties of the as-cast and extruded Mg-(6-11) Li-3Al-Ce-Ca alloys10.2320/matertrans.M2010156 ↗
17. Effect of cooling rates on as-cast microstructures of Mg-9Al-xSi (x= 1, 3) alloys10.1016/S1003-6326(10)60504-3 ↗
18. Effects of titanium addition on mechanical and corrosion behaviours of AZ91 magnesium alloy10.1016/j.jallcom.2010.10.100 ↗
19. Grain refinement of AZ31 magnesium alloy by titanium and low-frequency electromagnetic casting10.1007/s11661-007-9215-5 ↗
20. Microstructures and properties of superlight Mg–Li–Al–Zn wrought alloys10.1016/j.jallcom.2009.07.047 ↗
21. Structure and decomposition behaviour of Mg-Li-Al alloys10.1016/0956-716X(94)90485-5 ↗