journal article·2014-08

Thermoelectric properties of WSi2–SixGe1−x composites

F.W. Dynys, A. Sayir, J. Mackey, A. Sehirlioglu

Publisher page

Abstract

Abstract Thermoelectric properties of the W/Si/Ge alloy system have been investigated with varying concentration levels of germanium and tungsten. The alloys were fabricated by directional solidification with the Bridgman method using boron nitride and fused silica crucibles. The effect of crucible contamination was investigated and found to result in doping the system to suitable levels for thermoelectric applications. The system has been demonstrated as a suitable high temperature p-type thermoelectric material exhibiting high power factors, >3000 μW/m K 2 . Seebeck coefficients of the system are on the order of +300 μV/K and electrical conductivities of 2.8 × 10 4 S/m at the optimum operating temperature. The best composition, 0.9 at% W/9.3 at% Ge, achieved a figure of merit comparable to RTG values over the temperature range of interest. The results suggest that W addition can reduce the use of expensive Ge component of the alloy. Reported are the details of processing conditions, microstructure development, and temperature dependent thermoelectric properties. The material system was stable at the temperatures required for NASA’s radioisotope thermoelectric generators.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Thermoelectric Materials and Devices · Intermetallics and Advanced Alloy Properties · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Review of recent advances of radioisotope power systems10.1016/j.enconman.2007.10.028 ↗
2. High efficiency semimetal/semiconductor nanocomposite thermoelectric materials10.1063/1.3514145 ↗
3. Nanoparticle-in-alloy approach to efficient thermoelectrics: silicides in SiGe10.1021/nl8031982 ↗
4. Effect of embedding nanoparticles on the lattice thermal conductivity of bulk semiconductor crystals10.1063/1.4789808 ↗
5. Comparison of properties of p-type nanostructured bulk Si0.8Ge0.2 alloy with Si0.8Ge0.2 composites embedded with CrSi2 nano-inclusions10.1063/1.4764919 ↗
6. Enhanced electrical conductivity in Si80Ge20B0.6 alloys with Er addition prepared by spark plasma sintering10.1557/jmr.2011.127 ↗
7. Enhancement in thermoelectric power factor of polycrystalline Bi0.5Sb1.5Te3 by crystallite alignment10.1002/pssa.201228147 ↗
8. Self-assembled nanometer lamellae of thermoelectric PbTe and Sb2Te3 with epitaxy-like interfaces10.1021/cm062121p ↗
9. Microstructure and thermoelectric properties of mechanically robust PbTe–Si eutectic composites10.1021/cm9016672 ↗
10. Spinodal decomposition and nucleation and growth as a means to bulk nanostructured thermoelectrics: enhanced performance in Pb1−xSnxTe–PbS10.1021/ja071875h ↗
11. Nanostructuring, compositional fluctuations, and atomic ordering in the thermoelectric materials AgPbmSbTe2+m: the myth of solid solutions10.1021/ja051653o ↗
12. Ternary eutectic growth of nanostructured thermoelectric Ag–Pb–Te materials10.1063/1.4733661 ↗
13. Silicon germanium thermoelectric materials and module development program (U), RCA Topical Report, Contract AT (29–2)-2510, 1969.
14. Thermal and electrical properties of heavily doped Ge–Si alloys up to 1300K10.1063/1.1713126 ↗
15. Enhanced thermoelectric figure-of-merit in nanostructured p-type silicon germanium bulk alloys10.1021/nl8026795 ↗
16. Thermal conductivity of silicon, germanium III–V compounds and III–V alloys10.1016/0038-1101(67)90069-X ↗
17. Thermal conductivity of Ge–Si alloys at high temperatures10.1103/PhysRev.125.44 ↗
18. The maximum possible conversion efficiency of silicon–germanium thermoelectric generators10.1063/1.349385 ↗
19. Lattice thermal conductivity of disordered semiconductor alloys at high temperatures10.1103/PhysRev.131.1906 ↗
20. C.B. Vining, Thermoelectric properties of silicides 277, CRC Handbook of Thermoelectrics (Ed.) D.M. Rowe, CRC Press, London, 1995.10.1201/9781420049718.ch23 ↗
21. Mechanochemical synthesis and thermoelectric properties of high quality magnesium silicide10.1039/c1jm10827a ↗
22. Self assemble silicide architectures by directional solidification10.1016/j.jeurceramsoc.2005.01.033 ↗
23. Liquid encapsulated bridgman (LEB) method for directional solidification of silicon using calcium chloride10.1016/0022-0248(89)90603-9 ↗
24. J. Schilz, V.N. Romanenko, Bulk growth of silicon-germanium solid solutions, J. Mater. Sci. Mater. Electron. 6 (1995) 265–279.10.1007/BF00125881 ↗
25. Radiation loss in the flash method for thermal diffusivity10.1063/1.321635 ↗
26. PDF 01–072-6182 (ICDD, 2008).10.1088/1126-6708/2008/05/072 ↗
27. PDF 04–006-2527 (ICDD, 2005).10.1088/1475-7516/2005/04/006 ↗
28. Anisotropic microstrain broadening due to compositional inhomogeneities and its parameterisation10.1524/zksu.2006.suppl_23.117 ↗
29. Lamellar and Rod Eutectic Growth
30. Correlations between surface and interface energies with respect to crystal nucleation10.1006/jcis.2002.8627 ↗
31. Standard enthalpies of formation of some 3d transition metal silicides by high temperature direct synthesis calorimetry10.1016/S0925-8388(97)00528-8 ↗
32. Highly anisotropic columnar structures in silicon10.1063/1.1654382 ↗
33. The reversal of precipitation in heavily doped silicon-germanium alloys10.1088/0022-3727/12/9/024 ↗
34. Comparison of boron precipitation in p-type bulk nanostructured and polycrystalline silicon germanium alloy10.1063/1.4801388 ↗
35. Thermoelectric properties of group VI metal silicide semiconductors10.1016/j.phpro.2011.01.039 ↗
36. Theory of enhancement of thermoelectric properties of materials with nanoinclusions10.1103/PhysRevB.77.214304 ↗
37. Flash method of determining thermal diffusivity, heat capacity, and thermal conductivity10.1063/1.1728417 ↗
38. Microsegregation effects on the thermal conductivity of silicon-germanium alloys10.1063/1.4828884 ↗
39. The thermal conductivity of the silicides of transition metals
40. Arpaci · 1966