Abstract
Abstract This study assesses the reliability of eutectic Sn–Pb, Sn–1.0Ag–0.5Cu, Sn–3.0Ag–0.5Cu and Sn–4.0Ag–0.5Cu solder bumps on three different pad surface finishes (ENIG, electrolytic Ni/Au and Cu-OSP) with and without an aging treatment at 150 °C for 100 h. This study focused primarily on how the pad surface finish and solder alloy composition affects the reliability of solder joints using a high-speed ball pull test method. The fracture forces and failure mechanisms were also examined. The results showed that the electrolytic Ni/Au surface finish had the highest fracture forces for all four different solder alloys with and without the aging process.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced Welding Techniques Analysis · Powder Metallurgy Techniques and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Lai · Microelectron. Reliab. · 2006 · 46 · 64510.1016/j.microrel.2005.07.005 ↗
2. Xia · J. Alloys Compd. · 2008 · 454 · 17410.1016/j.jallcom.2006.12.098 ↗
3. Lee · 2002 · 82
4. Amagai · 2003 · 317
5. Chin · Microelectron. Reliab. · 2008 · 48 · 107910.1016/j.microrel.2008.04.003 ↗
6. You · J. Electron. Mater. · 2009 · 38 · 41010.1007/s11664-008-0633-y ↗
7. Song · 2007 · 364
8. Jeon · Microelectron. Eng. · 2008 · 85 · 196710.1016/j.mee.2008.06.003 ↗
9. Song · 2007 · 1504
10. Liu · JOM · 2007 · 59 · 2610.1007/s11837-007-0085-5 ↗
11. Chen · Microelectron. Reliab. · 2006 · 46 · 89610.1016/j.microrel.2005.06.006 ↗
12. Wong · Microelectron. Reliab. · 2008 · 48 · 106910.1016/j.microrel.2008.04.008 ↗
13. Alam · Microelectron. Reliab. · 2002 · 42 · 106510.1016/S0026-2714(02)00068-9 ↗
14. Arra · 2002 · 1256
15. Huang · Solder. SMT · 2005 · 17 · 310.1108/09540910510613501 ↗
16. Goyal · 2002 · 732
17. Yoon · Mater. Sci. Eng. A · 2008 · 483–4 · 73110.1016/j.msea.2006.09.162 ↗
18. Yoon · Microelectron. Reliab. · 2008 · 48 · 186410.1016/j.microrel.2008.07.065 ↗
19. Seo · Microelectron. Reliab. · 2009 · 49 · 28810.1016/j.microrel.2008.11.014 ↗
20. Yao · J. Alloys Compd. · 2008 · 462 · 7310.1016/j.jallcom.2007.08.041 ↗
21. Kim · Microelectron. Reliab. · 2003 · 43 · 75710.1016/S0026-2714(03)00060-X ↗
22. Koo · Microelectron. Reliab. · 2007 · 47 · 216910.1016/j.microrel.2006.09.043 ↗