Impact of NH3 plasma treatment for solution-processed indium oxide thin-film transistors with low thermal budget

Xuyang Li, Jin Cheng, Yanfei Gao, Meng Li, Dan Kuang, Yan Li, Jianshe Xue, Ting Zhang, Zhinong Yu

Publisher page

Abstract

Abstract The challenges associated with low-temperature solution-processed metal oxide thin-film transistors (TFTs) have hindered the realization of flexible oxide electronics at temperatures lower than 200 °C. NH3 plasma treatment is embarked upon as a route to effectively transform the chemical precursors to semiconducting metal oxides with high electrical quality. NH3 plasma-activated indium oxide (InOx) TFTs with saturated mobility 2.48 cm2V−1s−1 have been obtained at temperature as low as 150 °C. The low-temperature activation mechanism of NH3 plasma treatment for InOx films and the role of post-annealing in the fabrication process of InOx TFTs have been explored. Research shows that NH3 plasma treatment activates InOx films based on plasma bombardment, radicals doping and radical reactions; then, unreacted radicals and interstitial radicals were effectively removed by extra thermal energy from post-annealing. In comparison to thermal annealing, NH3 plasma treatment with moderate post-annealing is capable of achieving high degrees of condensation and densification reactions for InOx film and modulating the carrier concentration in a manner suitable for high-performance semiconducting behavior with low thermal budget. However, The InOx film after NH3 plasma treatment exhibited a non-uniform geometry due to the effect of plasma-induced damage in the local regions of InOx film, which restricts its commercial application. Some strategies were reported to eliminate the effect of plasma-induced damage by changing plasma conditions or pre-annealing temperature. The results demonstrated that changing plasma conditions by decreasing the plasma chamber temperature or the plasma power can eliminate plasma-induced damage, but attenuate the electrical performance of InOx TFT; nevertheless, changing pre-annealing temperature to 30 °C not only effectively eliminate plasma-induced damage, but also further improve the electrical performances of InOx TFT. These results provide a way for fabricating low-temperature oxide circuitry and supply an effective idea for avoiding plasma-induced damage.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Thin-Film Transistor Technologies · ZnO doping and properties · Ga2O3 and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Room-temperature fabrication of transparent flexible thin-film transistors using amorphous oxide semiconductors10.1038/nature03090 ↗
2. Water-based processed and alkoxide-based processed indium oxide thin-film transistors at different annealing temperatures
3. Recent advances of solution-processed metal oxide thin-film transistors10.1021/acsami.7b16010 ↗
4. Oxide semiconductor thin-film transistors: a review of recent advances10.1002/adma.201103228 ↗
5. 14-1: large-area processing of solution type metal-oxide in TFT backplanes and integration in highly stable OLED displays10.1002/sdtp.11612 ↗
6. Strong influence of humidity on low-temperature thin-film fabrication via metal aqua complex for high performance oxide semiconductor thin-film transistors10.1021/acsami.6b11867 ↗
7. Solution-grown homojunction oxide thin-film transistors10.1021/acsami.8b18422 ↗
8. Interface engineering of metal oxide semiconductors for biosensing applications10.1002/admi.201700020 ↗
9. Solution processed metal oxide high-k dielectrics for emerging transistors and circuits
10. Low-temperature, high-performance solution-processed metal oxide thin-film transistors formed by a ’sol-gel on chip’ process10.1038/nmat2914 ↗
11. Flexible metal-oxide devices made by room-temperature photochemical activation of sol-gel films10.1038/nature11434 ↗
12. Low-temperature fabrication of high-performance metal oxide thin-film electronics via combustion processing10.1038/nmat3011 ↗
13. Low-temperature, high-performance, solution-processed indium oxide thin-film transistors10.1021/ja104864j ↗
14. Simultaneous modification of pyrolysis and densification for low-temperature solution-processed flexible oxide thin-film transistors10.1039/c2jm16846d ↗
15. High-performance low-temperature solution-processable ZnO thin film transistors by microwave-assisted annealing10.1039/C0JM02178D ↗
16. An ‘aqueous route’ for the fabrication of low-temperature-processable oxide flexible transparent thin-film transistors on plastic substrates10.1038/am.2013.11 ↗
17. Significant performance improvement of solution-processed metal oxide transistors by ligand dissociation through coupled temperature–time treatment of aqueous precursors10.1021/acsaelm.8b00117 ↗
18. Ultralow-temperature sol-gel route to metal oxide semiconductors for soft platforms10.1002/admi.201600664 ↗
19. Low-temperature aqueous route processed indium oxide thin-film transistors by NH3 plasma-assisted treatment10.1109/TED.2018.2889597 ↗
20. Low-temperature, nontoxic water-induced metal-oxide thin films and their application in thin-film transistors10.1002/adfm.201500056 ↗
21. Low-temperature chemical transformations for high-performance solution-processed oxide transistors10.1021/acs.chemmater.6b03499 ↗
22. Comparative studies on the physical and electronic properties of reactively sputtered ZnO and ZnON semiconductors10.1016/j.ceramint.2015.07.110 ↗
23. Optical and electrical properties of p-type ZnO fabricated by NH3 plasma post-treated ZnO thin films10.1016/j.apsusc.2007.10.056 ↗
24. Ammonia plasma modification towards a rapid and low temperature approach for tuning electrical conductivity of ZnO nanowires on flexible substrates10.1039/c1nr10527b ↗
25. Highly stable thin-film transistors based on indium oxynitride semiconductor10.1021/acsami.8b02678 ↗
26. Controllable graphene N-doping with ammonia plasma10.1063/1.3368697 ↗
27. Numerical analysis of a mixture of Ar/NH3 microwave plasma chemical vapor deposition reactor10.1063/1.4728210 ↗
28. Effect of NH 3 plasma treatment on the transient characteristics of ZnO nanorod-gated AlGaN/GaN high electron mobility transistor-based UV sensors10.1016/j.tsf.2017.09.022 ↗
29. Self-aligned indium gallium zinc oxide thin-film transistor with source/drain regions treated by NH3Plasma10.1002/sdtp.11871 ↗
30. Source/drain formation of self-aligned top-gate amorphous GaInZnO thin-film transistors by NH3 plasma treatment10.1109/LED.2009.2014181 ↗
31. Effective atmospheric-pressure plasma treatment toward high-performance solution-processed oxide thin-film transistors10.1021/acsami.8b11111 ↗
32. Optimization of a solution-processed SiO2 gate insulator by plasma treatment for zinc oxide thin film transistors10.1021/acsami.5b10520 ↗
33. Plasma nitridation of atomic layer deposition (ALD) Al2O3 by NH3 in plasma-enhanced chemical vapor deposition (PECVD) for silicon solar cell10.1016/j.surfcoat.2016.05.057 ↗
34. Influence of NH3 plasma pretreatment on the properties of plasma-enhanced chemical-vapor-deposited SiON on GaAs interface10.1063/1.337208 ↗
35. Damage to amorphous indium-gallium-zinc-oxide thin film transistors under Cl2 and BCl3 plasma10.1007/s11814-018-0034-8 ↗
36. Rational solvent selection strategies to combat striation formation during spin coating of thin films10.1557/JMR.2001.0158 ↗
37. Inkjet-Printed in-Ga-Zn oxide thin-film transistors with laser spike annealing10.1007/s11664-017-5440-x ↗
38. High performance inkjet-printed metal oxide thin film transistors via addition of insulating polymer with proper molecular weight10.1063/1.5000313 ↗
39. Low-temperature-processed printed metal oxide transistors based on pure aqueous inks10.1002/adfm.201606062 ↗
40. Effects of nitrogen and hydrogen codoping on the electrical performance and reliability of InGaZnO thin-film transistors10.1021/acsami.6b15275 ↗
41. Plasma-enhanced flexible metal-insulator-metal capacitor using high-k ZrO2 film as gate dielectric with improved reliability10.1016/j.microrel.2010.05.004 ↗