Microstructure evolution of SiC-ZrB2-ZrC coating on C/C composites at 1773 K under different oxygen partial pressures
Source abstract
Abstract
Abstract The oxidation behavior of SiC-ZrB 2 -ZrC coating on C/C composites was investigated, basing on the microstructure evolution of oxide scale under different oxygen partial pressures at 1773 K. Similar experiments were conducted in SiC coatings, ZrB 2 and ZrC ceramic sheets for comparison. The multiphase coating showed the better oxidation resistance at a higher oxygen partial pressure, and its mass change was 1.34% after isothermal oxidation for 6 h at an oxygen partial pressure of 80,000 Pa. With the increase of the oxygen partial pressure, ZrO 2 particles with fibrous denticles were replaced by the aggregations of ZrO 2 particles and more SiO 2 glass was formed in a short time. The formed SiO 2 glass could effectively heal the microcracks of oxide scale. Moreover, the ZrB 2 and ZrC phases played an important role in deflecting cracks and restraining the propagation of cracks during oxidation. As the oxygen partial pressure increased, the oxide scale of SiC-ZrB 2 -ZrC coating became denser, presenting a two-layered structure composed of a SiO 2 layer and a Si-O-Zr layer at the elevated oxygen partial pressure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Carbon-carbon composites10.1146/annurev.ms.24.080194.000315 ↗
2. Oxidation protection of carbon/carbon composites with a plasma-sprayed ZrB2-SiC-Si/Yb2SiO5/LaMgAl11O19 coating during thermal cycling10.1016/j.jeurceramsoc.2015.01.015 ↗
3. Review oxidation protection for carbon fibre composites10.1007/BF00357844 ↗
4. Ultra-high-temperature ceramic coatings for oxidation protection of carbon-carbon composites10.1111/j.1551-2916.2008.02331.x ↗
5. A double layer nanostructure SiC coating for anti-oxidation protection of carbon/carbon composites prepared by chemical vapor reaction and chemical vapor deposition10.1016/j.ceramint.2012.11.104 ↗
6. A mullite/SiC oxidation protective coating for carbon/carbon composites10.1016/j.jeurceramsoc.2012.08.009 ↗
7. Oxidation protection of ultra-high temperature ceramic ZrxTa1-xB2-SiC/SiC coating prepared by in-situ reaction method for carbon/carbon composites10.1016/j.jeurceramsoc.2014.09.038 ↗
8. Preparation of ZrC by self-propagating high-temperature synthesis10.1016/j.ceramint.2010.03.013 ↗
9. C/SiC-ZrB2-ZrC composites fabricated by reactive melt infiltration with ZrSi2 alloy10.1016/j.ceramint.2012.05.035 ↗
10. ZrB2-SiC oxidation protective coating on C/C composites prepared by vapor silicon infiltration process10.1111/j.1551-2916.2009.03481.x ↗
11. Ablation resistance of SiC-ZrC coating prepared by a simple two-step method on carbon fiber reinforced composites10.1016/j.corsci.2014.07.014 ↗
12. Influence of infiltration temperature on the microstructure and oxidation behavior of SiC-ZrC ceramic coating on C/C composites prepared by reactive melt infiltration10.1016/j.ceramint.2014.08.138 ↗
13. In-situ fabrication of ZrB2-SiC/SiC gradient coating on C/C composites10.1016/j.jallcom.2015.05.205 ↗
14. A SiC-ZrB2-ZrC coating toughened by electrophoretically-deposited SiC nanowires to protect C/C composites against thermal shock and oxidation10.1016/j.apsusc.2015.05.028 ↗
15. A model for the oxidation of ZrB2, HfB2 and TiB210.1016/j.actamat.2007.07.027 ↗
16. In situ studies of oxidation of ZrB2 and ZrB2-SiC composites at high temperatures10.1016/j.jeurceramsoc.2010.03.009 ↗
17. Modeling oxidation kinetics of SiC-containing refractory diborides10.1111/j.1551-2916.2011.04927.x ↗
18. Oxidation behavior of ZrC-based composites in static laboratory air up to 1300 °C10.1016/j.ijrmhm.2014.05.013 ↗
19. SiC depletion in ZrB2-30 vol% SiC at ultrahigh temperatures10.1111/jace.13519 ↗
20. The oxidation behaviors of a ZrB2-SiC-ZrC ceramic10.1016/j.solidstatesciences.2010.12.022 ↗
21. Oxidation mechanism of a ZrB2-SiC-ZrC ceramic heated through high frequency induction at 1600 °C10.1016/j.corsci.2011.03.024 ↗
22. Changed oxidation behavior of ZrB2-SiC ceramics with the addition of ZrC10.1016/j.ceramint.2015.02.150 ↗
23. Oxidation of zirconium diboride-silicon carbide ceramics under an oxygen partial pressure of 200 Pa: formation of zircon10.1016/j.corsci.2010.06.004 ↗
24. Effects of oxygen partial pressure and atomic oxygen on the microstructure of oxide scale of ZrB2-SiC composites at 1500 °C10.1016/j.corsci.2013.03.023 ↗
25. Oxidation behavior of ZrB2-xSiC composites at 1500 °C under different oxygen partial pressures10.1016/j.ceramint.2014.07.036 ↗
26. Oxidation transitions for SiC part I. Active-to-passive transitions10.1111/jace.12108 ↗
27. Oxidation transitions for SiC part II. Passive-to-active transitions10.1111/jace.12104 ↗
28. Preparation of oxidation protective Hf0.2Ta0.8B2-x-SiC coating by in-situ reaction method on SiC-coated carbon/carbon composites10.1016/j.jallcom.2014.08.185 ↗
29. A SiC/ZrB2-SiC/SiC oxidation resistance multilayer coating for carbon/carbon composites10.1016/j.corsci.2011.12.023 ↗
30. In situ microscopy observation of liquid flow, zirconia growth, and CO bubble formation during high temperature oxidation of zirconium diboride-silicon carbide10.1016/j.jeurceramsoc.2010.01.034 ↗