Effect of WS2/Al co-doping on microstructural and magnetic properties of Nd−Fe−B sintered magnets

Kyoung-Hoon Bae, Seong-Rae Lee, Hyo-Jun Kim, Min-Woo Lee, Tae-Suk Jang

Publisher page

Abstract

Abstract The effect of WS2 (0–1.2 wt.%) and Al (0.3 wt.%) doping on microstructural and magnetic properties of Nd2Fe14B sintered magnets was investigated. Grain growth in WS2-doped magnets was inhibited by the grain boundary (GB) pinning resulting in increased magnet coercivity. Al co-doping (0.3 wt.%) produced continuous Nd-rich grain boundary phases (GBPs), in which fine WFeB precipitates were distributed selectively at the grain boundaries due to the higher fluidity of the liquid phases. 0.6 wt.% WS2/Al co-doped magnets are characterized by the optimum magnetic properties because of the smaller grain sizes and formation of continuous Nd-rich GB phases. When the WS2 content exceeds 0.6 wt.%, magnetic properties of the resulting magnets deteriorate due to the reduction in magnet density and relatively large WFeB precipitates formed inside the main phase and at the GBs.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties of Alloys · Magnetic properties of thin films · Magnetic Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Sepehri-Amin · Acta Mater. · 2012 · 60 · 81910.1016/j.actamat.2011.10.043 ↗
2. Li · Acta Mater. · 2009 · 57 · 133710.1016/j.actamat.2008.11.019 ↗
3. Kim · J. Alloy. Comp. · 2012 · 537 · 26110.1016/j.jallcom.2012.05.075 ↗
4. Li · J. Magn. Magn. Mater. · 2012 · 324 · 139110.1016/j.jmmm.2011.11.049 ↗
5. Kim · J. Appl. Phys. · 2015 · 117 · 17B52310.1063/1.4916496 ↗
6. Zhang · J. Alloy. Comp. · 2014 · 593 · 13710.1016/j.jallcom.2014.01.055 ↗
7. Cheng · J. Alloy. Comp. · 2001 · 319 · 28010.1016/S0925-8388(01)00900-8 ↗
8. Chu · J. Appl. Phys. · 1994 · 76 · 683410.1063/1.358146 ↗
9. Gabay · J. Appl. Phys. · 2011 · 109 · 08391610.1063/1.3574444 ↗
10. Sasaki · Scr. Mater. · 2016 · 113 · 21810.1016/j.scriptamat.2015.10.042 ↗
11. Knoch · IEEE Trans. Magn. · 1989 · 25 · 342610.1109/20.42323 ↗
12. Knoch · IEEE Trans. Magn. · 1990 · 26 · 195110.1109/20.104918 ↗
13. Gabay · J. Magn. Magn. Mater · 2002 · 238 · 22610.1016/S0304-8853(01)00917-9 ↗
14. Ni · J. Alloy. Comp. · 2010 · 502 · 34610.1016/j.jallcom.2010.04.021 ↗
15. Ni · J. Magn. Magn. Mater. · 2011 · 323 · 254910.1016/j.jmmm.2011.05.029 ↗
16. Xianglian · J. Rare Earth · 2007 · 25 · 32910.1016/S1002-0721(07)60431-1 ↗
17. Park · Appl. Phys. Lett. · 2006 · 89 · 06290610.1063/1.2335816 ↗
18. Li · J. Appl. Phys. · 2009 · 105 · 07A70610.1063/1.3058671 ↗
19. Kittel · Rev. Mod. Phys. · 1949 · 21 · 54110.1103/RevModPhys.21.541 ↗
20. Niedra · 1999 · vol. 85 · 5923