Suppression of the critical temperature in binary vanadium hydrides
Source abstract
Abstract
Abstract The tendency of vanadium-based alloy membranes to embrittle is the biggest commercialisation barrier for this hydrogen separation technology. Excessive hydrogen absorption and the α → β hydride transition both contribute to brittle failure of these membranes. Alloying is known to reduce absorption, but the influence of alloying on hydride phase formation under conditions relevant to membrane operation has not been studied in great detail previously. Here, the effect of Cr, Ni, and Al alloying additions on V–H phase equilibrium has been studied using hydrogen absorption measurements and in situ X-ray diffraction studies. The addition of 10 mol% Ni increases the critical temperature for α + β hydride formation to greater than 400 °C, compared to 170 °C for V. Cr also increases the critical temperature, to between 200 and 300 °C. The addition of 10 mol% Al, however, suppresses the critical temperature to less than 30 °C, thereby enabling this material to be cycled thermally and hydrostatically while precluding formation of the β-hydride phase. This is despite Al also decreasing hydrogen absorption. The implication of this finding is that one of the mechanisms of brittle failure in vanadium-based hydrogen-selective membranes has been eliminated, thereby increasing the robustness of this material relative to V.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Dolan · Int. J. Hydrogen Energy · 2010 · 35 · 1099410.1016/j.ijhydene.2010.07.039 ↗
2. Hwang · Int. J. Hydrogen Energy · 2011 · 37 · 660110.1016/j.ijhydene.2012.01.022 ↗
3. HYSEP Hydrogen Separation Modules. Petten, Energy Research Centre of the Netherlands, 2013. (www.hysep.com)
4. Development of membrane reactor technology for power production with pre-combustion CO2 capture
5. 24 hour spot chart - Palladium - Kitco. 2013.
6. Alloy membranes for industrial hydrogen separation10.1016/j.memsci.2010.06.068 ↗
7. Miller · 2007
8. Buxbaum · J. Membr. Sci. · 1993 · 85 · 2910.1016/0376-7388(93)85004-G ↗
9. S.A. Steward, Review of Hydrogen Isotope Permeability through metals. US National Laboratory, Report 1983:UCRL-53441.10.2172/5277693 ↗
10. Amano · J. Less Common Met. · 1991 · 172–174 · 72710.1016/0022-5088(91)90196-B ↗
11. Dolan · J. Phys. Chem. C · 2012 · 116 · 151210.1021/jp208691x ↗
12. Nishimura · J. Alloys Comp. · 2002 · 330–332 · 90210.1016/S0925-8388(01)01648-6 ↗
13. Song · J. Membr. Sci. · 2010 · 363 · 30910.1016/j.memsci.2010.07.051 ↗
14. Dolan · Int. J. Hydrogen Energy · 2013 · 38 · 979410.1016/j.ijhydene.2013.05.073 ↗
15. Nishimura · J. Alloys Comp. · 2003 · 356–357 · 29510.1016/S0925-8388(02)01273-2 ↗
16. Kim · Scr. Mater. · 2013 · 68 · 90510.1016/j.scriptamat.2013.02.028 ↗
17. Adams · Mater. Lett. · 2007 · 61 · 81710.1016/j.matlet.2006.05.078 ↗
18. Dolan · J. Membr. Sci. · 2012 · 415–416 · 32010.1016/j.memsci.2012.05.012 ↗
19. Hashi · J. Alloys Comp. · 2005 · 404–406 · 27310.1016/j.jallcom.2005.02.085 ↗
20. Dolan · J. Alloys Comp. · 2013 · 446 · 405
21. Buxbaum · J. Nucl. Mater. · 1996 · 233–237 · 51010.1016/S0022-3115(96)00239-5 ↗
22. H. Yukawa ,C. Tsukada,T. Nambu,Y. Matsumoto, J. Alloys. Comp., in press 2013 (doi:10.1016/j,allcom.2013.03.144).
23. Rashid · J. Less Common Met. · 1973 · 31 · 37710.1016/0022-5088(73)90031-3 ↗
24. Takano · Acta Metall. · 1974 · 22 · 26510.1016/0001-6160(74)90166-7 ↗
25. Esayed · Int. J. Hydrogen Energy · 1992 · 17 · 4110.1016/0360-3199(92)90220-Q ↗
26. Yukawa · J. Alloys Comp. · 2002 · 337 · 26410.1016/S0925-8388(01)01936-3 ↗
27. Noda · Acta Crystallogr. · 1986 · B42 · 52910.1107/S0108768186097756 ↗
28. Marsh · Acta Crystallogr. · 1987 · B43 · 41510.1107/S010876818709757X ↗
29. Griffiths · J. Chem. Soc.: Faraday Trans. 1 · 1972 · 68 · 2344
30. Pesch · Scr. Metall. · 1982 · 16 · 30710.1016/0036-9748(82)90358-1 ↗
31. Westlake · Metall. Mater. Trans. · 1970 · 1 · 136110.1007/BF02900255 ↗
32. Ko · Int. J. Hydrogen Energy · 2012 · 37 · 1358310.1016/j.ijhydene.2012.06.075 ↗
33. Yukawa · J. Alloys Comp. · 2002 · 330–332 · 10510.1016/S0925-8388(01)01526-2 ↗
34. Knapton · Platinum Met. Rev. · 1977 · 21 · 4410.1595/003214077X2124450 ↗
35. Kim · Int. J. Hydrogen Energy · 2011 · 37 · 783610.1016/j.ijhydene.2012.01.117 ↗
36. Lynch · J. Phys. Chem. Solids · 1978 · 39 · 88310.1016/0022-3697(78)90150-6 ↗
37. Watanabe · J. Less-Common Met. · 1982 · 88 · 4310.1016/0022-5088(82)90010-8 ↗