Effect of sintering temperature on microstructures and tribological characteristics of dense α-Si3N4-based ceramic coating on porous Si3N4 ceramics
Source abstract
Abstract
Abstract A dense α-Si3N4-based ceramic protective coating was successfully prepared on porous Si3N4 ceramics by a liquid infiltration and filling method using α-Si3N4 and B-Si-A-O glass raw powders. SEM and XRD analysis showed that the coating surface prepared at 1500 °C was covered by a dense B-Si-A-O glass layer. As the sintering temperature increased, the top glass layer disappeared completely, and a dense and rough α-Si3N4-based ceramic coating, including primary α-Si3N4 and secondly O′-Sialon and B-Si-Al-O amorphous phase, was exposed on the surface. An intermediate layer was produced in the interface of coating and substrate, which indicated a strong interfacial bonding between them. The coatings displayed an excellent waterproof ability, and water absorption of the coated porous Si3N4 ceramics was only in the range of 3.5–8.6%. Among all the coatings, the coating prepared at sintering temperature of 1600 °C had a higher hardness and elastic modulus than the other two kinds of coatings, which made it have a better wear resistance, and its wear rate was only 0.21 × 10−3 mm3/Nm after friction for 20 min.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Effect of Si3N4 solid contents on mechanical and dielectric properties of porous Si3N4 ceramics through freeze-drying10.1016/j.jallcom.2017.10.172 ↗
2. Development of silicon nitride-based ceramic radomes-a review10.1111/ijac.12305 ↗
3. High temperature mechanical properties of porous Si3N4 prepared via SRBSN10.1016/j.ceramint.2018.03.044 ↗
4. Gas pressure sintering of arbitrary porous silicon nitride ceramics with high mechanical strength10.1111/j.1551-2916.2010.03603.x ↗
5. Oxidation bonding of porous silicon nitride ceramics with high strength and low dielectric constant10.1016/j.matlet.2006.08.067 ↗
6. A novel aerogels/porous Si3N4 ceramics composite with high strength and improved thermal insulation property10.1016/j.ceramint.2017.12.132 ↗
7. A tough silicon nitride ceramic with high thermal conductivity10.1002/adma.201102462 ↗
8. Novel porous Si3N4 ceramics prepared by aqueous gelcasting using Si3N4 poly-hollow microspheres as pore-forming agent10.1016/j.jeurceramsoc.2013.11.025 ↗
9. Fabrication and properties of supersonic plasma sprayed Al2O3 coating on porous Si3N4 substrate10.1016/j.msea.2012.09.015 ↗
10. Effect of Si3N4 content on the microstructure and properties of Y-Al-Si-O-N ceramic coating
11. Study on damp-proof and enhanced coating of porous Si3N4 surface10.3724/SP.J.1077.2008.00769 ↗
12. Study on inorganic coating of porous nitride radome10.4028/www.scientific.net/KEM.537.16 ↗
13. Effect of holding time on microstructure and properties of dense α-Si3N4/Sialon composite coating on porous Si3N4 ceramic10.1016/j.ceramint.2016.08.060 ↗
14. Fabrication of dense β-Si3N4-based ceramic coating on porous Si3N4 ceramic10.1016/j.jeurceramsoc.2014.10.015 ↗
15. Fabrication and erosion resistance of dense α-Si3N4/Sialon coating on porous Si3N4 ceramic10.1039/C6RA13310J ↗
16. Gelcasting preparation of porous silicon nitride ceramics by adjusting the content of monomers10.1007/s10971-009-2125-9 ↗
17. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
18. Sialon ceramics10.1111/j.1151-2916.1992.tb08175.x ↗
19. Progress in sialon ceramics10.1016/S0955-2219(00)00039-X ↗
20. Chemical reactions in the system Si3N4-SiO2-B2O310.1016/S0955-2219(97)00188-X ↗
21. A novel structure for carbon nanotube reinforced alumina composites with improved mechanical properties10.1088/0957-4484/19/31/315708 ↗
22. Nanotube fracture during the failure of carbon nanotube/alumina composites10.1016/j.carbon.2011.04.022 ↗
23. Toughening by SiC nanowires in a dense SiC-Si ceramic coating for oxidation protection of C/C composites10.1111/j.1551-2916.2012.05412.x ↗
24. Influences of current density on tribological characteristics of ceramic coatings on ZK60 Mg alloy by plasma electrolytic oxidation10.1021/am900802x ↗
25. Microstructure-mechanical properties-wear resistance relationship of SiAlON ceramics10.1007/s11661-009-9930-1 ↗
26. Interaction of tribochemistry and microfracture in the friction and wear of silicon nitride10.1016/0043-1648(85)90004-3 ↗
27. Friction and wear properties of the co-deposited Ni-SiC nanocomposite coating10.1016/j.apsusc.2007.04.047 ↗