journal article·2021-03

Acicular microstructure formation and strengthening behavior of Ti-4%Fe alloys by Zr addition

Takuma Teramae, Takayuki Tanaka, Mizuki Fukuo, Kazuki Shitara, Junko Umeda, Shufeng Li, Abdulaziz Alhazaa, Katsuyoshi Kondoh

Publisher page

Abstract

Abstract Commercial pure Ti alloys are favorable for biomedical applications; however, they need to be strengthened by the addition of alloying elements. Herein, Ti-Fe alloys modified with Zr were explored to produce alloys that exhibit high strength and ductility and are biocompatible. Ti-Fe extruded materials with Zr solutes were prepared by combining solid sintering and hot extrusion. X-ray diffraction results revealed that the lattice constant of α-Ti and β-Ti increased proportionally with the Zr content, indicating the Zr solid solution behavior. In situ and ex situ observations of the microstructure formation revealed the element Zr, a weak β-stabilizer, and a decreased phase transformation temperature. However, during the cooling process after hot extrusion, the grain growth stagnated at the same temperature, irrespective of the Zr content, resulting in both α-Ti grain refinement and increased β-phase area fraction. The tensile test results demonstrated that 1010 MPa 0.2% yield strength of the Ti-4Fe-13Zr extruded material increased to 156%, compared with that of the base Ti-4Fe material. Furthermore, Labusch model and the Hall-Petch equation were used to quantitatively evaluate the strengthening mechanism derived from the Zr solid solution and the changes in the grain size.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Advanced materials and composites · Orthopaedic implants and arthroplasty

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. A review on biomedical titanium alloys: recent progress and prospect10.1002/adem.201801215 ↗
2. Mechanical properties of biomedical titanium alloys10.1016/S0921-5093(97)00806-X ↗
3. Development and application of physical vapor deposited coatings for medical devices: a review10.1016/j.procir.2020.05.149 ↗
4. Dissimilar transient liquid phase bonding of Ti–6Al–4V and Co–Cr–Mo biomaterials using a Cu interlayer: microstructure and mechanical properties10.1016/j.jallcom.2020.154510 ↗
5. Ti based biomaterials, the ultimate choice for orthopaedic implants - a review10.1016/j.pmatsci.2008.06.004 ↗
6. Froes · 2018
7. Microstructure and mechanical behavior of as-built and heat-treated Ti–6Al–7Nb produced by laser powder bed fusion10.1016/j.msea.2020.139978 ↗
8. Sintering properties of mechanically alloyed Ti-5Al-2.5Fe
9. Microstructure and mechanical behaviour of Ti-6Al-7Nb alloy produced by selective laser melting10.1016/j.matchar.2011.03.006 ↗
10. The Ti-Zr (Titanium-Zirconium) system10.1007/BF02881478 ↗
11. The effect of the solute on the structure, selected mechanical properties, and biocompatibility of Ti-Zr system alloys for dental applications10.1016/j.msec.2013.09.032 ↗
12. Development of a Ti-based alloy: design and experiment10.1007/s11837-009-0073-z ↗
13. Injection molding of mechanical alloyed Ti-Fe-Zr powder10.2320/matertrans.M2012031 ↗
14. Strengthening mechanisms of powder metallurgy extruded CP titanium materials with zirconium and oxygen solid solution via decomposition of ZrO 2 additives in sintering10.2320/matertrans.Y-M2019833 ↗
15. Microstructure and strengthening mechanism of ultrastrong and ductile Ti-xSn alloy processed by powder metallurgy10.1016/j.jallcom.2017.03.171 ↗
16. Fabrication of powder metallurgy pure ti material by using thermal decomposition of TiH210.7791/jhts.37.326 ↗
17. The PANDAT software package and its applications
18. Phase transformations during cooling in α + β titanium alloys10.1016/S0921-5093(97)00802-2 ↗
19. In situ SEM-EBSD observations of the hcp to bcc phase transformation in commercially pure titanium10.1016/j.actamat.2003.10.049 ↗
20. The Fe-Ti (Iron-Titanium) system10.1007/BF02868286 ↗
21. Ultrafine microstructures in eutectoid element bearing low-cost Ti-Fe alloys enabled by slow bainite formation10.1016/j.jallcom.2018.07.347 ↗
22. Grain boundary wetting by a second solid phase in Ti-Fe alloys10.1007/s11665-018-3300-3 ↗
23. The physical metallurgy of titanium alloys10.1016/0502-8205(58)90004-2 ↗
24. Influence of Zr content on microstructure and mechanical properties of implant Ti-35Nb-4Sn-6Mo-xZr alloys10.1016/S1003-6326(13)62597-2 ↗
25. A Review on High-Strength Titanium Alloys: Microstructure, Strengthening, and Properties10.1002/adem.201801359 ↗
26. Quantitative strengthening evaluation of powder metallurgy Ti-Zr binary alloys with high strength and ductility
27. Mechanical properties of the binary titanium‐zirconium alloys and their potential for biomedical materials10.1002/jbm.820290805 ↗
28. Open porous dealloying-based biomaterials as a novel biomaterial platform10.1016/j.msec.2018.03.008 ↗
29. The effects of Zr contents on microstructure and properties of laser additive manufactured Ti-6.5Al-3.5Mo-0.3Si-xZr alloys10.1016/j.jallcom.2018.02.079 ↗
30. Effect of Zr on the Stability of a Ti-15Mo Base Beta Alloy10.2320/jinstmet1952.35.2_97 ↗
31. β-Ti alloys with low young’s moduli interpreted by cluster-plus-glue-atom model10.1007/s11661-012-1523-8 ↗
32. Phase Transformation of α" Martensite Structure by Aging in Ti-8 mass%Mo Alloy10.2320/matertrans.45.1629 ↗
33. Verlinden · 2007
34. Study on the formation mechanism of α lamellae in a near β titanium alloy10.1016/j.pnsc.2016.06.009 ↗
35. Influence of transformation temperature on microtexture formation associated with α precipitation at β grain boundaries in a β metastable titanium alloy10.1016/j.actamat.2013.03.007 ↗
36. Ductility improvement mechanism of Ti6Al4V+O sintered material10.2320/matertrans.Y-M2019869 ↗
37. W.C.P. ASTM, Standard Specification for Titanium and Titanium Alloy Bars and Billets, (2005) 1–9. doi:10.1520/B0348–13.2.
38. Theory of Solid Solution Hardening10.1002/pssb.19700410221 ↗
39. Strength-ductility improvement of extruded Ti-(N) materials using pure Ti powder with high nitrogen solution10.1016/j.msea.2020.139136 ↗
40. Quantitative analysis on light elements solution strengthening in pure titanium sintered materials by labusch model using experimental data10.2320/matertrans.Y-M2018849 ↗
41. Ueber die Beziehung zwischen den beiden Elasticitätsconstanten isotroper Körper10.1002/andp.18892741206 ↗
42. Ultrafine composite microstructure in a bulk Ti alloy for high strength, strain hardening and tensile ductility10.1016/j.actamat.2005.11.011 ↗
43. Strengthening mechanism of two-phase titanium alloys with basketweave microstructure10.1016/j.jallcom.2014.03.057 ↗
44. The effect of volume per cent of phase on the high temperature tensile deformation of two-phase TiMn alloys10.1016/0921-5093(89)90197-4 ↗
45. The deformation and ageing of mild steel III Discussion of results10.1088/0370-1301/64/9/303 ↗
46. The cleavage strength of polycrystals
47. Extension of the Hall-Petch relation to two-ductile-phase alloys10.1080/01418619308207175 ↗
48. Improvement of tensile and fatigue properties of β-titanium alloy while maintaining low young’s modulus through grain refinement and oxygen addition10.2320/matertrans.M2013151 ↗
49. Microstructural effect on strength-ductility balance and deformation mode of Ti-4.5Al-2Mo-1.6V-0.5Fe-0.3Si alloy10.2464/jilm.66.531 ↗
50. An EBSD investigation of ultrafine-grain titanium for biomedical applications10.1016/j.msea.2015.09.080 ↗
51. Microstructural effects on the mechanical behavior of B-modified Ti-6Al-4V alloys10.1016/j.actamat.2007.05.009 ↗
52. Yielding nature and Hall-Petch relationships in Ti-6Al-4V alloy with fully equiaxed and bimodal microstructures10.1016/j.scriptamat.2019.07.015 ↗
53. On the validity of Hall-Petch equation for single-phase β Ti-Al-Nb alloys undergoing stress-induced martensitic transformation10.1016/j.msea.2009.05.041 ↗
54. Evolution of the structural phase state, deformation behavior, and fracture of ultrafine-grained near-β titanium alloy after annealing10.1007/s10853-020-04468-y ↗
55. Effect of zirconium content on the microstructure, physical properties and corrosion behavior of Ti alloys10.1016/j.msea.2014.08.010 ↗