journal article·2023-06Open access

High-performance gradient Fe-Si alloy thin sheets fabricated by solid powder siliconizing and diffusion annealing

Jingqi Chen, Wei Zhao, Xiaofeng Zheng, Rihuan Lu, Cheng Guo, Shoudong Chen, Jinlong Du, Chao Yu, Xianghua Liu

Abstract

A gradient Fe-Si alloy was prepared by solid powder siliconizing and diffusion annealing using Fe-3.0 wt% Si alloy as raw material. Solid powder siliconizing was carried out at 800 °C for 10–20 min, and siliconized samples with Fe 3 Si phase and FeSi phase were obtained. Then, the siliconized sample was subjected to diffusion annealing at 1050 °C for 1–2 h, and the Fe 3 Si phase and FeSi phase were transformed into single α-Fe phase. The magnetic properties of gradient Fe-Si alloys are higher than those of Fe-Si alloys with uniform Si content distribution (even Fe-6.5 wt%Si alloy). When the surface Si content is 12.3 wt% and the core Si content is 5.0 wt%, the iron loss of the gradient Fe-Si alloy at high frequency is reduced by 97.3% compared with Fe-3.0 wt%Si alloy. Moreover, gradient Fe-Si alloys show excellent magnetic induction intensity and mechanical properties after solid powder siliconizing and diffusion annealing process . This work proposes a solid powder siliconizing and diffusion annealing method to prepare high-performance gradient Fe-Si alloys, which is simple, low-cost, and can control the distribution of Si content in the thickness direction, providing a new idea for the realization of large-scale industrial production of high-performance Fe-Si alloys.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Aluminum Alloys Composites Properties · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Core loss reduction for Fe-6.5wt%Si soft magnetic composites doped with Co element10.1016/j.jmmm.2020.166553 ↗
2. Effect of quench cooling rate on residual stress, microstructure and mechanical property of an Fe–6.5Si alloy10.1016/j.msea.2011.10.013 ↗
3. Review of Fe-6.5 wt%Si high silicon steel-a promising soft magnetic material for sub-kHz application10.1016/j.jmmm.2019.02.089 ↗
4. Innovative ferrite nanofibres reinforced soft magnetic composite with enhanced electrical resistivity10.1016/j.jallcom.2018.04.237 ↗
5. Soft magnetic properties of Fe-based amorphous/nanocrystalline hybrid materials10.1016/j.powtec.2018.08.037 ↗
6. Deformation twinning characteristics in hot-rolled Fe-6.5wt%Si alloy with different degree of order10.1016/j.msea.2019.138095 ↗
7. Microstructure and properties of cost-effective Fe–6.5 wt% Si ribbons fabricated by melt-spinning10.1016/j.scriptamat.2019.01.002 ↗
8. Deformation and fracture behavior of rapidly solidified and annealed iron-silicon alloys10.1007/s11661-007-9436-7 ↗
9. Magnetic properties of commercially produced Fe-6.5wt% Si sheet10.1007/BF02833761 ↗
10. Effects of solidification cooling rates on microstructures and physical properties of Fe-6.5%Si alloys10.1016/j.actamat.2020.116575 ↗
11. Near net shape fabrication of anisotropic Fe-6.5%Si soft magnetic materials10.1016/j.actamat.2020.09.084 ↗
12. Evolution of microstructure and texture in grain-oriented 6.5%Si steel processed by strip-casting10.1016/j.matchar.2017.02.022 ↗
13. Fabrication of Fe-6.5wt%Si ribbons by melt spinning method on large scale10.1155/2015/296197 ↗
14. Microstructure and properties of cost-effective Fe-6.5 wt% Si ribbons fabricated by melt-spinning10.1016/j.scriptamat.2019.01.002 ↗
15. Thermodynamic and kinetic analysis of the melt spinning process of Fe-6.5 wt% Si alloy10.1016/j.jallcom.2018.08.293 ↗
16. Magnetic properties of high silicon iron sheet fabricated by direct powder rolling10.1016/j.jmmm.2004.04.098 ↗
17. Stress-induced magnetic anisotropy in Fe-based nanocrystalline alloy with addition of 1-5 at% Cr10.1016/j.jallcom.2011.12.088 ↗
18. Effect of Y addition on crystallization behavior and soft-magnetic properties of Fe78Si9B13 ribbons10.1016/j.jmmm.2017.04.023 ↗
19. Electromagnetic wave absorption properties of flaky Fe-Ti-Si-Al nanocrystalline composites10.1016/j.jmmm.2009.11.028 ↗
20. Effect of annealing temperature on magnetic properties of cold rolled high silicon steel thin sheet10.1016/j.jallcom.2009.10.118 ↗
21. Development of λ-fiber recrystallization texture and magnetic property in Fe-6.5wt% Si thin sheet produced by strip casting and warm rolling method10.1016/j.matlet.2012.09.046 ↗
22. Characterization of microstructure, texture and magnetic properties in twin-roll casting high silicon non-oriented electrical steel10.1016/j.matchar.2013.11.014 ↗
23. Magnetic properties evaluation of spray formed and rolled Fe–6.5wt% Si–1.0wt% Al alloy10.1016/j.msea.2006.02.318 ↗
24. Magnetic properties of spray formed Fe-6.wt%Si alloy10.4028/www.scientific.net/KEM.189-191.643 ↗
25. Magnetic properties and workability of 6.5% Si steel sheet10.1016/0304-8853(96)00128-X ↗
26. Influence of cooling rate on iron loss behavior in 6.5wt% grain-oriented silicon steel10.1016/j.jmmm.2013.10.004 ↗
27. Texture effect on magnetic properties by alloying specific elements in non-grain oriented silicon steels10.2355/isijinternational.45.918 ↗