Indentation plastic work and large compression plasticity in in situ nanocrystallized Zr62Cu18Ni10Al10 bulk metallic glass
Source abstract
Abstract
Large plasticity is observed during uniaxial macroscopic compression of Zr62Cu18Ni10Al10 bulk metallic glass. Nanoindentation experiments, performed on the as-cast and compressed specimens, confirm the enhanced plasticity after compression. Indeed, the ratio between the plastic and the total indentation energies, Upl/Utot, is larger in the compressed sample than in the as-cast alloy. Furthermore, in both samples, Upl/Utot tends to progressively increase with the maximum indentation applied load, thus confirming the tendency towards enhanced plasticity as deformation proceeds. Transmission electron microscopy reveals that deformation (induced either by macroscopic compression tests or nanoindentation) causes partial nanocrystallization of the glass. This effect is likely to play a crucial role in the observed plasticity and also results in mechanical hardening.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Schuh · Acta Mater. · 2007 · 55 · 406710.1016/j.actamat.2007.01.052 ↗
2. Telford · Mater. Today · 2004 · 7 · 3610.1016/S1369-7021(04)00124-5 ↗
3. Liu · Science · 2007 · 315 · 138510.1126/science.1136726 ↗
4. Schroers · Phys. Rev. Lett. · 2004 · 93 · 25550610.1103/PhysRevLett.93.255506 ↗
5. Zhang · Nat. Mater. · 2006 · 5 · 85710.1038/nmat1758 ↗
6. Das · Phys. Rev. Lett. · 2005 · 94 · 20550110.1103/PhysRevLett.94.205501 ↗
7. Lewandowsky · Philos. Mag. Lett. · 2005 · 85 · 7710.1080/09500830500080474 ↗
8. Van Steenberge · Mater. Sci. Eng. A · 2008 · 491 · 12410.1016/j.msea.2008.01.083 ↗
9. Lee · Mater. Sci. Eng. A · 2007 · 449 · 17210.1016/j.msea.2006.02.306 ↗
10. Yim · Acta Mater. · 1999 · 47 · 245510.1016/S1359-6454(99)00103-2 ↗
11. Spaepen · Acta Metall. · 1977 · 25 · 40710.1016/0001-6160(77)90232-2 ↗
12. Argon · Acta Metall. · 1979 · 27 · 4710.1016/0001-6160(79)90055-5 ↗
13. Slipenyuk · Scripta Mater. · 2004 · 50 · 3910.1016/j.scriptamat.2003.09.038 ↗
14. Flores · Acta Mater. · 2007 · 55 · 340310.1016/j.actamat.2007.01.040 ↗
15. Kanungo · Intermetallics · 2004 · 12 · 107310.1016/j.intermet.2004.04.033 ↗
16. Van Steenberge · Scripta Mater. · 2007 · 56 · 60510.1016/j.scriptamat.2006.12.014 ↗
17. Fornell · Int. J. Plast. · 2009 · 25 · 154010.1016/j.ijplas.2008.11.002 ↗
18. Fornell · Scripta Mater. · 2010 · 62 · 1310.1016/j.scriptamat.2009.09.014 ↗
19. Correlation between structural changes and enhanced mechanical properties during thermally-induced devitrification of Fe–Co–B–Si–Nb bulk metallic glass10.1016/j.actamat.2010.07.047 ↗
20. Oliver · J. Mater. Res. · 1992 · 7 · 156410.1557/JMR.1992.1564 ↗
21. Song · Intermetallics · 2008 · 16 · 81310.1016/j.intermet.2008.03.007 ↗
22. Chen · Intermetallics · 2009 · 17 · 33010.1016/j.intermet.2008.11.004 ↗
23. Dalla Torre · Acta Mater. · 2008 · 56 · 463510.1016/j.actamat.2008.05.021 ↗
24. Schuh · Acta Mater. · 2003 · 51 · 8710.1016/S1359-6454(02)00303-8 ↗
25. 1998
26. Zander · Mater. Sci. Eng. A · 2001 · 304–306 · 29210.1016/S0921-5093(00)01456-8 ↗
27. Tekaya · J. Mater. Sci. · 2009 · 44 · 493010.1007/s10853-009-3752-9 ↗
28. Yang · J. Phys. D: Appl. Phys. · 2009 · 42 · 06540110.1088/0022-3727/42/6/065401 ↗
29. Milman · J. Phys. D: Appl. Phys. · 2008 · 41 · 07401310.1088/0022-3727/41/7/074013 ↗