Abstract As-milled composite metal hydrides composed of Mg2Ni and TiNi phases were cold-pressed under a pressure of 490 MPa and sintered for 1 h at 5×10−6 Torr and 300 °C. Electrochemical characteristics of the sintered composite metal hydride electrode were investigated. The maximum discharge capacity of the sintered composite alloy electrode was 125 mAh/g at a discharge current density of 100 mA/g. This value was similar to that of the as-milled one before sintering. However, the sintered electrode retained 80% of the maximum discharge capacity after 150 cycles, while the as-milled electrode retained only 55%. This is because after the sintering process an interface between Mg2Ni and TiNi plays a role similar to a diffusion layer of hydrogen. In the sintered composite electrode, when a discharging step proceeds, hydrogen absorbed in a Mg2Ni particle can move into a TiNi phase through the bonded-interface between Mg2Ni and TiNi, then discharges at the interface between TiNi and the electrolyte. Also, the electrochemical impedance spectroscopy (EIS) tests showed that the composite alloy electrodes had a lower charge-transfer resistance and a higher hydrogen diffusion coefficient than those in single-phase Mg2Ni. This indicates that TiNi particles in the composite are the active sites for redox reaction of hydrogen and the pathway for the diffusion of hydrogen
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen Storage and Materials · Ammonia Synthesis and Nitrogen Reduction · Magnesium Alloys: Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. Goo · J. Alloys Comp. · 1999 · 288 · 28610.1016/S0925-8388(99)00100-0 ↗
2. Han · J. Power Sources · 2001 · 92 · 15710.1016/S0378-7753(00)00516-4 ↗
3. Zaluska · J. Alloys Comp. · 1999 · 289 · 19710.1016/S0166-0462(99)00013-7 ↗
4. Zhang · J. Alloys Comp. · 1998 · 269 · 27810.1016/S0925-8388(98)00222-9 ↗
5. Tsushio · J. Alloys Comp. · 1998 · 281 · 30110.1016/S0925-8388(98)00779-8 ↗
6. Terzieva · J. Alloys Comp. · 1998 · 267 · 23510.1016/S0925-8388(97)00556-2 ↗
7. Cracco · J. Alloys Comp. · 1998 · 268 · 24810.1016/S0925-8388(97)00552-5 ↗
8. Davidson · J. Alloys Comp. · 1999 · 292 · 19410.1016/S0925-8388(99)00190-5 ↗
9. Lee · J. Alloys Comp. · 1999 · 292 · 25810.1016/S0925-8388(99)00435-1 ↗
10. Liu · J. Alloys Comp. · 1997 · 252 · 23410.1016/S0925-8388(96)02735-1 ↗
11. Fujii · J. Alloys Comp. · 1996 · 232 · L1610.1016/0925-8388(95)02079-9 ↗
12. Woo · J. Electrochemical Soc. · 1999 · 146 · 81910.1149/1.1391687 ↗
13. Goo · J. Power Sources · 2000 · 87 · 11810.1016/S0378-7753(99)00432-2 ↗
14. Macdonald · 1987 · 22
15. Cui · J. Power Sources · 1996 · 63 · 20910.1016/S0378-7753(96)02473-1 ↗
16. Cui · Int. J. Hydrogen Energy · 1999 · 24 · 3710.1016/S0360-3199(98)00026-3 ↗
17. Cabanel · J. Appl. Electrochem. · 1993 · 23 · 9310.1007/BF00246943 ↗
18. Barral · Electrochim. Acta · 1995 · 40 · 281510.1016/0013-4686(95)00274-I ↗