Effect of a high magnetic field on solidification structure in directionally solidified NiAl-Cr(Mo)-Hf eutectic alloy
Source abstract
Abstract
Abstract The effect of a high magnetic field on the microstructure in directionally solidified NiAl-Cr(Mo)-Hf eutectic alloy was investigated experimentally. The obtained results indicated that the application of the magnetic field caused the degeneration of the regular lamellar eutectic structure and induced the columnar-to-equiaxed transition (CET) of eutectic dendrites. In addition, the magnetic field modified the macroscopic solid-liquid interface shape and decreased the volume fraction of the Heusler phase. Furthermore, the amplitude and distribution of the thermoelectric magnetic force (TEMF) and thermoelectric magnetic convection (TEMC) in NiAl-Cr(Mo) eutectic alloy during directional solidification under a high magnetic field were studied by numerical simulation at different scales. It was found that the abovementioned results should be attributed to the coupling effects between the TEMC and TEMF. Besides, present work may provide a new method for modification of eutectic morphology during directional solidification under a high magnetic field.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Solidification and crystal growth phenomena · Intermetallics and Advanced Alloy Properties · Metallic Glasses and Amorphous Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Physical and mechanical properties of the B2 compound NiAl10.1179/imr.1993.38.4.193 ↗
2. NiAl alloys for high-temperature structural applications10.1007/BF03220163 ↗
3. The physical and mechanical properties of NiAl10.1016/0956-7151(93)90001-9 ↗
4. Brittle fracture and grain boundary chemistry of microalloyed NiAl10.1557/JMR.1990.0754 ↗
5. The effect of alloy additions on the rod-plate transition in the eutectic NiAl-Cr10.1007/BF03037830 ↗
6. Processing and mechanical properties of in-situ composites from the NiAl-Cr and the NiAl-(Cr,Mo) eutectic systems10.1016/0966-9795(95)92674-O ↗
7. Phase-specific deformation behavior of a relatively tough NiAl-Cr(Mo) lamellar composite10.1016/j.scriptamat.2014.04.025 ↗
8. Microstructures and mechanical properties of a directionally solidified NiAl-Mo eutectic alloy10.1016/j.actamat.2004.09.003 ↗
9. Microstructure and mechanical behavior of in-situ directional solidified NiAl/Cr(Mo) eutectic composite10.1016/S1359-6454(96)00124-3 ↗
10. Microstructure, creep and fracture toughness of directionally solidified NiAl/(Cr,Mo) alloys modified with Hf, Si, Ta, Ti additions
11. Effects of Hf additions on high-temperature mechanical properties of a directionally solidified NiAl/Cr(Mo) eutectic alloy10.1016/j.jallcom.2007.08.065 ↗
12. Effect of heat treatment on the microstructure and elevated temperature tensile property of Fe-doped NiAl-Cr(Mo)-(Hf,Dy) eutectic alloy10.1016/j.msea.2015.12.043 ↗
13. Modification of interdendritic convection in directional solidification by a uniform magnetic field10.1016/S1359-6454(98)00064-0 ↗
14. Alignment of BiMn crystal orientation in Bi-20at%Mn alloys by laser melting under a magnetic field10.2320/matertrans.44.2550 ↗
15. Dendrite fragmentation and columnar-to-equiaxed transition during directional solidification at lower growth speed under a strong magnetic field10.1016/j.actamat.2012.02.019 ↗
16. Influence of thermoelectric effects on the morphology of Al-Si eutectic during directional solidification under an axial strong magnetic field10.1016/j.jcrysgro.2012.12.032 ↗
17. Effect of a high axial magnetic field on the microstructure in a directionally solidified Al-Al2Cu eutectic alloy10.1016/j.actamat.2006.06.051 ↗
18. Electrical properties of β-phase NiAl10.1016/0022-3697(69)90384-9 ↗
19. Lide · 2010
20. The thermoelectric power of liquid Fe, Co and Ni10.1080/14786437708236005 ↗
21. Thermophysical properties of solid and liquid Inconel 71810.1016/S0040-6031(01)00751-1 ↗
22. Viscosity of superalloy 718 by the oscillating vessel technique10.1007/BF02915672 ↗
23. Effect of an axial high magnetic field on Sn dendrite morphology of Pb-Sn alloys during directional solidification10.1016/j.jallcom.2013.11.011 ↗
24. Effect of strong magnetic field on solid solubility and microsegregation during directional solidification of Al-Cu alloy10.1557/jmr.2013.271 ↗
25. The spiral growth of lamellar eutectics in a high magnetic field during the directional solidification process10.1016/j.scriptamat.2006.11.019 ↗
26. Strong magnetic field effect on surface tension associated with an interfacial magnetic pressure10.1021/jp305542q ↗
27. Influence of thermoelectric effects on the solid-liquid interface shape and cellular morphology in the mushy zone during the directional solidification of Al-Cu alloys under a magnetic field10.1016/j.actamat.2007.02.031 ↗
28. Influence of forced/natural convection on segregation during the directional solidification of Al-based binary alloys10.1007/s11663-009-9311-6 ↗
29. Thermoelectric effects on electrical conducting particles in liquid metal10.22364/mhd.51.1.6 ↗
30. Effect of a high magnetic field on the morphological instability and irregularity of the interface of a binary alloy during directional solidification10.1016/j.actamat.2008.12.005 ↗
31. Assessment of substitutional self-diffusion along short-circuit paths in Al, Fe and Ni10.1016/j.calphad.2014.06.008 ↗