journal article·2014Open access

Microwave sintering of biogenic hydroxyapatite ceramics for reconstructive surgery

Hanna Tovstonoh, Olena Sych, Valery Skorokhod

Abstract

Ceramics based on biogenic hydroxyapatite have been produced via a microwave sintering at 1000?C for 5, 10, 15, 20 and 30 min. It was shown that all of the ceramics studied exhibit volumetric shrinkage (2.3- 4.6 %), which increases with increasing sintering time at maximum temperature. It was established that the total porosity did not depend on sintering time at 1000?C and was equal to 38-40 %. Moreover, in all of the materials an open porosity dominated. The ultimate compression strength was in the range 35-40 MPa.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Bone Tissue Engineering Materials · Titanium Alloys Microstructure and Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

National Technical University of Ukraine “Kyiv Politechnical Institute”, Kyiv, Ukraine + Frantsevich Institute for Problems of Materials Science of NAS of Ukraine, Kyiv, Ukraine

Frantsevich Institute for Problems of Materials Science of NAS of Ukraine, Kyiv, Ukraine

References