Sintering behaviors, magnetic and electric properties of Bi–Zn co-doped Co2Y ferrites
Source abstract
Abstract
Abstract The Bi and Zn substitution effects on the sintering behaviors, magnetic and electric properties of hexagonal ferrites with a composition of 2(Ba 1− x Bi x O)·2(Zn y Co 0.8− y Cu 0.2 O)·6(Fe 2− x /3 Zn x /3 O 3 ) were investigated. The results showed that the addition of Bi and Zn can significantly promote Co 2 Y densification. The Y phase may be triggered to decompose into M and spinel phases at high sintering temperatures (above 1050 °C) for samples with excess Bi ( x = 0.2) substitution, which resulted in densification and magnetic properties degradation. Co 2 Y ferrites with x = 0.1 and y = 0.4 sintered at 1050 °C show a relative density of 94%, a high initial permeability of 4.5, a quality factor ( Q ) of 50.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties and Synthesis of Ferrites · Multiferroics and related materials · Magneto-Optical Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Nakamura · J. Magn. Magn. Mater. · 1997 · 168 · 28510.1016/S0304-8853(96)00709-3 ↗
2. Hsu · IEEE Trans. Magn. · 1997 · 33 · 332510.1109/20.617932 ↗
3. Smith · 1959
4. Jonker · Philips Tech. Rev. · 1956 · 18 · 145
5. Hsiang · J. Alloys Compd. · 2011 · 509 · 334310.1016/j.jallcom.2010.12.060 ↗
6. Hsiang · Mater. Chem. Phys. · 2007 · 104 · 110.1016/j.matchemphys.2007.02.030 ↗
7. Hsiang · J. Magn. Magn. Mater. · 2011 · 323 · 101110.1016/j.jmmm.2010.12.006 ↗
8. Hsiang · Jpn. J. Appl. Phys. · 2002 · 41 · 513710.1143/JJAP.41.5137 ↗
9. Xu · J. Alloys Compd. · 2011 · 509 · 429010.1016/j.jallcom.2011.01.027 ↗
10. Jia · J. Alloys Compd. · 2010 · 489 · 16210.1016/j.jallcom.2009.09.043 ↗
11. Xu · J. Alloys Compd. · 2010 · 490 · 55210.1016/j.jallcom.2009.10.079 ↗
12. Chen · J. Alloys Compd. · 2010 · 490 · 60910.1016/j.jallcom.2009.10.116 ↗
13. Snoek · Physica · 1948 · 14 · 20710.1016/0031-8914(48)90038-X ↗
14. Li · J. Am. Ceram. · 2006 · 89 · 145010.1111/j.1551-2916.2006.00873.x ↗
15. Bai · J. Alloys Compd. · 2008 · 450 · 41210.1016/j.jallcom.2006.10.122 ↗
16. Bai · J. Magn. Magn. Mater. · 2004 · 278 · 20810.1016/j.jmmm.2003.12.1389 ↗
17. Bai · Mater. Sci. Eng. · 2003 · B99 · 26610.1016/S0921-5107(02)00545-7 ↗
18. Li · J. Am. Ceram. Soc. · 2006 · 89 · 145010.1111/j.1551-2916.2006.00873.x ↗
19. Pires Júnior · J. Alloys Compd. · 2010 · 493 · 32610.1016/j.jallcom.2009.12.094 ↗
20. Costa · Mater. Chem. Phys. · 2010 · 123 · 3510.1016/j.matchemphys.2010.03.026 ↗
21. Macdonald · 2005 · 1
22. Kingery · 1976