Influence of B substitution for Ti and Ni on the electrochemical hydriding of TiNi
Source abstract
Abstract
Abstract Nanostructured TiNi0.8B0.2 and Ti0.8B0.2Ni were synthesized by mechanical alloying and by milling with subsequent annealing. X-ray analysis of the as-milled alloys shows a broad diffraction peak, which position corresponds to the cubic TiNi. Annealing for 1 h at 720 °C leads to microstructure coarsening and formation of TiNi and Ni3Ti. Boron doped titanium oxide (TiB0.024O2) was also detected in Ti0.8B0.2Ni. Electrochemical hydrogen charge/discharge measurements of the as-milled as well as of the annealed alloys were carried out at galvanostatic conditions. It was found that both alloys studied possessed low discharge capacities, as TiNi0.8B0.2 revealed a higher discharge capacity of 42 mAh/g in the as-milled state. Temperature increase from 23 to 45 °C did not result in capacity and cycle life changes. A capacity decrease for the two alloys was observed after annealing at 720 °C. Based on potentiostatic experiments the diffusion coefficients of hydrogen in the as-milled alloys were determined: 9.66 × 10−12 cm2/s for TiNi0.8B0.2 and 4.67 × 10−12 cm2/s for Ti0.8B0.2Ni.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen Storage and Materials · Electrocatalysts for Energy Conversion · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Justi · Energy Convers. · 1970 · 10 · 18310.1016/0013-7480(70)90031-8 ↗
2. M.A. Gutjahr, Ph.D. Thesis, Geneva University, 1974 (in French).
3. Machida · Electrochim. Acta · 1984 · 29 · 80710.1016/0013-4686(84)80018-3 ↗
4. Fruchart · Z. Phys. Chem. · 1993 · 179 · 22510.1524/zpch.1993.179.Part_1_2.225 ↗
5. Cuevas · J. Alloys Compd. · 2002 · 330–332 · 25010.1016/S0925-8388(01)01636-X ↗
6. Aoyagi · J. Alloys Compd. · 1995 · 231 · 80410.1016/0925-8388(95)01721-6 ↗
7. Mizuno · J. Less Common Met. · 1982 · 84 · 23710.1016/0022-5088(82)90148-5 ↗
8. Matsumoto · J. Less Common Met. · 1982 · 88 · 44310.1016/0022-5088(82)90255-7 ↗
9. Lee · J. Alloys Compd. · 1991 · 177 · 10710.1016/0925-8388(91)90061-Y ↗
10. Lee · J. Alloys Compd. · 1992 · 187 · 4910.1016/0925-8388(92)90519-F ↗
11. Lee · Int. J. Hydrogen Energy · 1994 · 19 · 25910.1016/0360-3199(94)90095-7 ↗
12. Suzuki · J. Less Common Met. · 1981 · 80 · 17910.1016/0022-5088(81)90091-6 ↗
13. Boulghallat · J. Less Common Met. · 1991 · 174 · 105210.1016/S0022-5088(06)80011-1 ↗
14. Bershadsky · J. Less Common Met. · 1991 · 174 · 103610.1016/S0022-5088(06)80009-3 ↗
15. Sandrock · J. Less Common Met. · 1980 · 73 · 16110.1016/0022-5088(80)90355-0 ↗
16. Jang · J. Less Common Met. · 1986 · 119 · 23710.1016/0022-5088(86)90684-3 ↗
17. Lee · J. Alloys Compd. · 1999 · 291 · 25410.1016/S0925-8388(99)00262-5 ↗
18. Szajek · J. Alloys Compd. · 2005 · 403 · 32310.1016/j.jallcom.2005.05.011 ↗
19. Drenchev · J. Alloys Compd. · 2007 · 441 · 19710.1016/j.jallcom.2006.09.071 ↗
20. Drenchev · J. Appl. Electrochem · 2008 · 38 · 43710.1007/s10800-007-9456-4 ↗
21. Xu · J. Alloys Compd. · 2002 · 335 · 26210.1016/S0925-8388(01)01838-2 ↗
22. Xu · J. Power Sources · 2002 · 112 · 10510.1016/S0378-7753(02)00348-8 ↗
23. Xu · Mater. Chem. Phys. · 2001 · 71 · 19010.1016/S0254-0584(01)00282-6 ↗
24. Xu · Int. J. Hydrogen Energy · 2001 · 26 · 117710.1016/S0360-3199(00)00111-7 ↗
25. Song · J. Alloys Compd. · 1993 · 199 · 16110.1016/0925-8388(93)90444-R ↗
26. Zheng · J. Electrochem. Soc. · 1995 · 8 · 269510.1149/1.2050076 ↗
27. Nishina · J. Electrochem. Soc. · 1996 · 143 · 128710.1149/1.1836631 ↗
28. Ura · J. Electroanal. Chem. · 1995 · 142 · 269510.1149/1.2050076 ↗
29. Mazzolai · J. Alloys Compd. · 2007 · 446/447 · 20410.1016/j.jallcom.2007.01.098 ↗