Microwave dielectric properties of low-fired Mg 1.9 Cu 0.1 SiO 4 –(La 0.5 Na 0.5 )TiO 3 composite ceramics
Source abstract
Abstract
Abstract Mg 2− x Cu x SiO 4 (0 ≤ x ≤ 0.2) ceramics were fabricated by the traditional solid-state process. The results revealed that solid solution was formed at x ≤ 0.2 by substitution Cu 2+ for Mg 2+ and the sintering temperature was lowered from 1500 to 1200 °C. LiF-doped (1 − y )Mg 1.9 Cu 0.1 SiO 4 – y (La 0.5 Na 0.5 )TiO 3 (0.1 ≤ y ≤ 0.4) composite ceramics were obtained at a temperature range from 890 to 1000 °C. As increasing (La 0.5 Na 0.5 )TiO 3 content y , the τ f values showed a continuous positive increase. The 0.8Mg 1.9 Cu 0.1 SiO 4 –0.2(La 0.5 Na 0.5 )TiO 3 composite ceramics with 4.0 wt% LiF sintered at 950 °C possess excellent microwave dielectric properties of e r = 13.3, Q × f = 14,400 GHz, and τ f = 6 ppm/°C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microwave Dielectric Ceramics Synthesis · Ferroelectric and Piezoelectric Materials · Dielectric properties of ceramics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Dielectric materials for applications in microwave communication10.1039/b003681l ↗
2. Novel series of low-firing microwave dielectric ceramics: Ca5A4(VO4)6 (A2+= Mg, Zn)10.1111/jace.12359 ↗
3. Constrained sintering of dielectric and ferrite LTCC tape composites10.1016/j.jeurceramsoc.2005.03.011 ↗
4. Forsterite ceramics for millimeterwave dielectrics10.1007/s10832-006-0452-6 ↗
5. Fabrication of nanopowders by high energy ball milling and low temperature sintering of Mg2SiO4 microwave dielectrics10.1016/j.jallcom.2011.10.051 ↗
6. Microwave dielectric properties of forsterite-based solid solutions10.1016/j.jeurceramsoc.2005.09.102 ↗
7. Structure-dependent microwave dielectric properties and middle temperature sintering of forsterite (Mg1–xNix)2SiO4 ceramics10.1111/jace.13347 ↗
8. Phase evolution and microwave dielectric characteristics of Ti-substituted Mg2SiO4 forsterite ceramics10.1016/j.matlet.2007.05.078 ↗
9. Effect of lithium magnesium zinc borosilicate glass addition on densification temperature and dielectric properties of Mg2SiO4 ceramics10.1007/s10854-009-9882-7 ↗
10. Low-temperature sintered Mg2SiO4-CaTiO3 ceramics with near-zero temperature coefficient of resonant frequency10.1007/s10854-012-0945-9 ↗
11. Mg2SiO4-TiO2 composite ceramics prepare using a liquid phase deposition process10.1007/s10832-007-9388-8 ↗
12. Microwave dielectric properties of Ba3(VO4)2–Mg2SiO4 composite ceramics10.1111/j.1551-2916.2009.03429.x ↗
13. Microwave dielectric properties of Li2TiO3 ceramics doped with LiF for LTCC applications10.1016/j.jallcom.2012.10.110 ↗
14. Low temperature firing of BiSbO4 microwave dielectric ceramic with B2O3–CuO addition10.1016/j.jeurceramsoc.2008.08.024 ↗
15. Low-temperature sintering and microwave dielectric properties of MgO ceramic with LiF addition10.1143/JJAP.50.09NF02 ↗
16. Microwave dielectric properties in the (1-x)(Na1/2La1/2)TiO3–x(Li1/2Sm1/2)TiO3 ceramic system10.1016/S0955-2219(03)00342-X ↗
17. Microwave dielectric properties of (1-x)(Mg0.95Zn0.05)TiO3–x(Na0.5La0.5)TiO3 ceramic system10.1016/j.jallcom.2008.05.007 ↗
18. The intercept method-2. Determination of spatial grain size10.1016/S1359-6454(96)00198-X ↗
19. Significant enhancement in quality factor of Zn2TiO4with Cu-substitution10.1016/j.mseb.2011.01.013 ↗
20. Effect of porosity and grain size on the microwave dielectric properties of sintered alumina10.1111/j.1151-2916.1997.tb03066.x ↗
21. Microwave dielectric losses caused by lattice defects10.1016/j.jeurceramsoc.2005.09.080 ↗
22. Structural, optical and microwave dielectric properties of Sr1-xCaxWO4 ceramics prepared by the solid state reaction route10.1016/j.ceramint.2013.05.084 ↗