journal article·2019-03

Interfacial reactions in In/Bi2Se3, In/Bi2Te3 and In/Bi2(Se0.2Te0.8)3 couples

Sinn-wen Chen, Yohanes Hutabalian, Shi-ting Lu, Ying-shuo Peng, Yi-cheng Lin

Publisher page

Abstract

Abstract Bi2(Se,Te)3 is the most commonly used N-type thermoelectric materials. The interfacial reactions in In/Bi2Se3 and In/Bi2Te3 couples at 400 °C, 250 °C and 200 °C and In/Bi2(Se0.2Te0.8)3 couples at 250 °C are systematically determined for the first time. Significant interfacial reactions are observed in all the couples. The reaction rate decreases when the reaction temperature is reduced and the reaction is fastest in the In/Bi2Te3 couple and slowest in the In/Bi2Se3 couple. After reaction for 5 minutes, the thickness of the reaction layer in the In/Bi2Te3 couple is 439 μm, 44 μm and 14 μm at 400 °C, 250 °C and 200 °C, respectively. The reaction phases and reaction paths in these couples are determined. In the In/Bi2(Se0.2Te0.8)3 couple that is reacted at 250 °C, the reaction path is liquid(In)/In4(Se,Te)3/liquid/(Bi2)m(Bi2(Se,Te)3)n/Bi2(Se0.2Te0.8)3. At 400 °C and 250 °C, Se and Te are the species that diffuse fastest in the reaction couples and the reaction path is primarily controlled by the speed with which Se and Te diffuse. However, the diffusion rates for Se and Te decrease significantly when the reaction temperature is reduced and at 200 °C, Se and Te cease to be the dominating diffusion species in the couples.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Thermoelectric Materials and Devices · Thermal properties of materials · Thermal Radiation and Cooling Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. A review on bismuth telluride (Bi2Te3) nanostructure for thermoelectric applications10.1016/j.rser.2017.10.112 ↗
2. A review of the development and applications of thermoelectric microgenerators for energy harvesting10.1016/j.rser.2018.03.052 ↗
3. Thermoelectric devices: a review of devices, architectures, and contact optimization
4. Self-tuning n-type Bi2(Te,Se)3/SiC thermoelectric nanocomposites to realize high performances up to 300 °C
5. Interfacial reactions in the Ni/(Bi0.25Sb0.75)2Te3 and Ni/Bi2(Te0.9Se0.1)3 couples10.1016/j.jallcom.2016.06.207 ↗
6. Interfacial reactions in Sn/Bi2Te3, Sn/Bi2Se3 and Sn/Bi2(Te1-xSex)3 couples10.1016/j.jallcom.2014.05.127 ↗
7. Chen · 2018
8. Solid liquid interdiffusion bonding of Zn4Sb3 thermoelectric material with Cu electrode10.1007/s11664-016-4645-8 ↗
9. Improvement of bonding strength of a (Pb,Sn)Te-Cu contact manufactured in a low temperature SLID- bonding process10.1016/j.jallcom.2014.06.020 ↗
10. Effect of doping indium into a Bi2Te3 matrix on the microstructure and thermoelectric transport properties
11. Enhanced figure of merit in antimony telluride thermoelectric materials by In–Ag co-alloying for mid-temperature power generation10.1016/j.actamat.2014.11.023 ↗
12. Thermodynamic calculation of phase diagram in the Bi–In–Sb ternary system10.2320/matertrans.43.1879 ↗
13. Intermetallic compounds formed by electrodeposition of indium on bismuth10.1016/0925-8388(94)91057-X ↗
14. In-Se (Indium-Selenium)
15. Use of the effective heat of formation model to determine phase formation sequences of in-Se, Ga-Se, Cu-Se, and Ga-in multilayer thin films10.1007/s11664-998-0093-4 ↗
16. The kinetics of indium/amorphous-selenium multilayer thin film reactions10.1557/JMR.1999.0103 ↗
17. Phase diagram of the indium-tellurium system
18. Thickness dependent structural and optical properties of In/Te bilayer thin films10.1016/j.mssp.2012.03.006 ↗
19. Crystalline perfection and mechanical investigations on vertical Bridgman grown Bismuth telluride (Bi2Te3) single crystals for thermoelectric applications10.1016/j.msea.2016.01.033 ↗
20. Reduced thermal conductivity in Pb-alloyed AgSbTe2 thermoelectric materials10.1016/j.actamat.2012.07.057 ↗
21. Structure and bonding properties of (Bi2Se3)m(Bi2)n stacks by first-principles density functional theory10.1103/PhysRevB.72.184101 ↗
22. Liquidus projections of Bi-Se-Ga and Bi-Se-Te ternary systems
23. Hutabalian · 2018
24. Liquidus projections of Bi-Se-Ga and Bi-Se-Te ternary systems
25. Solid-State displacement reactions in the Fe-Ni-S and Cu-Ni-S systems between 400 and 500oC10.1007/BF00656902 ↗
26. On the layer sequence and morphology in solid-state displacement reactions10.1007/BF00656903 ↗
27. Morphological development during platinum/gallium arsenide interfacial reactions10.1007/BF02651282 ↗
28. Diffusion studies in the β (B2), β′ (Bcc), and γ (Fcc) Fe-Ni-Al alloys at 1000°C10.1007/s11661-002-0326-8 ↗
29. Interfacial reactions in In/Cu2Se couples10.1016/j.jtice.2012.12.008 ↗
30. Self-diffusion in indium10.1016/0001-6160(59)90201-9 ↗
31. Self-diffusion in tellurium. I. Anisotropy and impurity effect10.1103/PhysRev.155.598 ↗
32. Self-Diffusion in selenium10.1002/pssb.19700370239 ↗
33. Grain growth in bismuth coating10.1016/j.msea.2006.05.156 ↗
34. Estimate of the self-diffusion coefficients for selenium and tellurium using viscosity data
35. Solid state demixing in Bi2Se3-Bi2Te3 and Bi2Se3-In2Se3 phase diagrams10.1016/0025-5408(95)00185-9 ↗
36. Bi-In-Te phase diagrams10.1016/j.jallcom.2017.06.144 ↗
37. Lin · 2018